Polylactic Acid Resin Composition, Moldings, and Process for Production Thereof
    5.
    发明申请
    Polylactic Acid Resin Composition, Moldings, and Process for Production Thereof 有权
    聚乳酸树脂组合物,成型品及其制造方法

    公开(公告)号:US20100174017A1

    公开(公告)日:2010-07-08

    申请号:US11661671

    申请日:2005-09-02

    IPC分类号: C08K5/24

    CPC分类号: C08K5/25 C08K3/34 C08L67/04

    摘要: A polylactic acid resin composition in which polylactic acid is blended with dibasic acid bis(benzoylhydrazide) represented by general formula (I) below; and a process for producing heat-resistant polylactic acid resin moldings, wherein after the polylactic acid resin composition is melted, the polylactic acid resin composition melted is filled in a die of a molding machine and molded accompanied with crystallization, in which the temperature of the die has been set in a range not higher than the initiation temperature of crystallization and not lower than the glass transition temperature determined with a differential scanning calorimeter (DSC). (In the formula, R represents a alkylene, alkenylene, cycloalkylene, alkylene having an ether bond, or alkylene interrupted with a cycloalkylene, the groups each having 1 to 12 carbon atoms; and R1, R2, R3, and R4 each represent a hydrogen atom, halogen atom, alkyl, cycloalkyl, aryl, aralkyl, or alkylaryl, the groups each having 1 to 12 carbon atoms, or R1 and R2 and/or R3 and R4 bond to each other to form a five- to eight-membered ring.)

    摘要翻译: 将聚乳酸与下述通式(I)表示的二元酸二(苯甲酰基酰肼)配合的聚乳酸树脂组合物; 以及制造耐热性聚乳酸树脂成形体的方法,其中在聚乳酸树脂组合物熔融之后,熔融的聚乳酸树脂组合物被填充在模塑机的模具中,并且随着结晶而成型,其中, 晶粒已经设定在不高于结晶的起始温度的范围内,并且不低于用差示扫描量热计(DSC)测定的玻璃化转变温度。 (式中,R表示亚烷基,亚烯基,亚环烷基,具有醚键的亚烷基,或亚环烷基间隔的亚烷基,各自具有1〜12个碳原子的基团,R1,R2,R3,R4分别表示氢原子 原子,卤素原子,烷基,环烷基,芳基,芳烷基或烷基芳基,各自具有1至12个碳原子,或R 1和R 2和/或R 3和R 4彼此键合以形成五至八元环 。)

    Polylactic acid resin composition, moldings, and process for production thereof
    6.
    发明授权
    Polylactic acid resin composition, moldings, and process for production thereof 有权
    聚乳酸树脂组合物,成型品及其制造方法

    公开(公告)号:US07910643B2

    公开(公告)日:2011-03-22

    申请号:US11661671

    申请日:2005-09-02

    IPC分类号: C08K5/24 C08G63/08

    CPC分类号: C08K5/25 C08K3/34 C08L67/04

    摘要: A polylactic acid resin composition in which polylactic acid is blended with dibasic acid bis(benzoylhydrazide) represented by general formula (I) below; and a process for producing heat-resistant polylactic acid resin moldings, wherein after the polylactic acid resin composition is melted, the polylactic acid resin composition melted is filled in a die of a molding machine and molded accompanied with crystallization, in which the temperature of the die has been set in a range not higher than the initiation temperature of crystallization and not lower than the glass transition temperature determined with a differential scanning calorimeter (DSC). (In the formula, R represents a alkylene, alkenylene, cycloalkylene, alkylene having an ether bond, or alkylene interrupted with a cycloalkylene, the groups each having 1 to 12 carbon atoms; and R1, R2, R3, and R4 each represent a hydrogen atom, halogen atom, alkyl, cycloalkyl, aryl, aralkyl, or alkylaryl, the groups each having 1 to 12 carbon atoms, or R1 and R2 and/or R3 and R4 bond to each other to form a five- to eight-membered ring.)

    摘要翻译: 将聚乳酸与下述通式(I)表示的二元酸二(苯甲酰基酰肼)配合的聚乳酸树脂组合物; 以及制造耐热性聚乳酸树脂成形体的方法,其中在聚乳酸树脂组合物熔融之后,熔融的聚乳酸树脂组合物被填充在模塑机的模具中,并且随着结晶而成型,其中, 晶粒已经设定在不高于结晶的起始温度的范围内,并且不低于用差示扫描量热计(DSC)测定的玻璃化转变温度。 (式中,R表示亚烷基,亚烯基,亚环烷基,具有醚键的亚烷基,或亚环烷基间隔的亚烷基,各自具有1〜12个碳原子的基团,R1,R2,R3,R4分别表示氢原子 原子,卤素原子,烷基,环烷基,芳基,芳烷基或烷基芳基,各自具有1至12个碳原子,或R 1和R 2和/或R 3和R 4彼此键合以形成五至八元环 。)

    Polylactic acid composition
    8.
    发明授权
    Polylactic acid composition 失效
    聚乳酸组成

    公开(公告)号:US07585910B2

    公开(公告)日:2009-09-08

    申请号:US11387964

    申请日:2006-03-24

    IPC分类号: B60C1/00

    CPC分类号: C08K5/10 C08L67/04

    摘要: A polylactic acid composition containing polylactic acid and ester-based plasticizer, wherein a content of the ester-based plasticizer is 16 to 33 wt %, and when the composition is highly deformed by stress loading as the relation between the stress and the deformation deviates from linear viscoelastic behavior and thereafter the stress is released, residual deformation measured after the stress is released is not less than 66.0% after 0.2 minute of the stress release, and is not more than 34.0% after 240 hours of the stress release.

    摘要翻译: 含有聚乳酸和酯系增塑剂的聚乳酸组合物,其中酯类增塑剂的含量为16〜33重量%,当应力负荷与组合物的应力与变形之间的关系偏离时,组合物高度变形 线性粘弹性行为,然后释放应力,应力释放后测得的残余变形在应力释放0.2分钟后不低于66.0%,应力释放240小时后不大于34.0%。