摘要: A wet friction material comprises a fiber base material, a filler and a binder: wherein the filler contains a disc-shaped diatomaceous earth; wherein the filler contains at least one of a filler having Mohs hardness of 8 to 9.5 and a diatomaceous earth and the binder contains a specific silicone resin binder; or wherein the binder contains another specific silicone resin binder.
-
公开(公告)号:US20060223907A1
公开(公告)日:2006-10-05
申请号:US11388094
申请日:2006-03-24
申请人: Masahiro Mori , Hirokazu Yagi , Sousuke Kawai
发明人: Masahiro Mori , Hirokazu Yagi , Sousuke Kawai
IPC分类号: C08J5/14
CPC分类号: C08G8/28 , C08L61/06 , F16D69/026 , F16D2200/0095 , Y10T428/2962 , Y10T442/2738 , Y10T442/2803
摘要: The invention provides a wet friction material having high friction coefficient, excellent compression fatigue property and positive gradient of a μ-V property. The wet friction material contains a paper base material and a binder, in which the binder contains a cured material of a liquid resin composition obtained by mixing a hydrolyzed solution of a silane coupling agent represented by the following formula (1) and a resol-type phenol resin, and a weight ratio (S/R) between respective non-volatile components of the hydrolyzed solution (S) of the silane coupling agent and the resol-type phenol resin (R) is in the range of from 80/20 to 20/80: (X)(R1)nSi(OR2)3-n (1), in which X represents an alkylamino group having a primary amine at a terminal; R1 and R2 each independently represent an alkyl group having from 1 to 3 carbon atoms; and n represents an integer of 0 or 1.
摘要翻译: 本发明提供具有高摩擦系数,优异的压缩疲劳特性和μ-V特性的正梯度的湿摩擦材料。 湿摩擦材料包含纸基材料和粘合剂,其中粘合剂含有通过将下式(1)表示的硅烷偶联剂的水解溶液与甲阶酚醛树脂型 酚醛树脂,硅烷偶联剂和甲阶酚醛树脂型酚醛树脂(R)的水解溶液(S)的各非挥发成分的重量比(S / R)为80/20〜 20/80:(X)(R 1)N 2 Si(OR 2)3-n(1) ),其中X表示末端具有伯胺的烷基氨基; R 1和R 2各自独立地表示具有1至3个碳原子的烷基; n表示0或1的整数。
-
公开(公告)号:US07491664B2
公开(公告)日:2009-02-17
申请号:US11388094
申请日:2006-03-24
申请人: Masahiro Mori , Hirokazu Yagi , Sousuke Kawai
发明人: Masahiro Mori , Hirokazu Yagi , Sousuke Kawai
CPC分类号: C08G8/28 , C08L61/06 , F16D69/026 , F16D2200/0095 , Y10T428/2962 , Y10T442/2738 , Y10T442/2803
摘要: The invention provides a wet friction material having high friction coefficient, excellent compression fatigue property and positive gradient of a μ-V property. The wet friction material contains a paper base material and a binder, in which the binder contains a cured material of a liquid resin composition obtained by mixing a hydrolyzed solution of a silane coupling agent represented by the following formula (1) and a resol-type phenol resin, and a weight ratio (S/R) between respective non-volatile components of the hydrolyzed solution (S) of the silane coupling agent and the resol-type phenol resin (R) is in the range of from 80/20 to 20/80: (X)(R1)nSi(OR2)3−n (1), in which X represents an alkylamino group having a primary amine at a terminal; R1 and R2 each independently represent an alkyl group having from 1 to 3 carbon atoms; and n represents an integer of 0 or 1.