Method for hot dip coating a flat steel product
    1.
    发明授权
    Method for hot dip coating a flat steel product 有权
    热轧镀锌钢板产品的方法

    公开(公告)号:US09279175B2

    公开(公告)日:2016-03-08

    申请号:US13819481

    申请日:2011-08-18

    摘要: A method for hot dip coating a flat stainless steel product with more than 5 wt. % Cr with a protective metallic coating by: heating the flat steel product under an oxygen-free heating atmosphere to 100° C.-600° C. within 1-30 seconds; continuing heating to a holding temperature of 750° C.-950° C., by heating to 550° C.-800° C. under an inert or reducing atmosphere, holding within this temperature window for 1 to 15 seconds under an oxidizing atmosphere, and continuing heating under an inert or reducing atmosphere, until the holding temperature is reached; holding at the holding temperature for 10-120 seconds under a reducing atmosphere; and passing the flat steel product through a nozzle area under an inert or reducing atmosphere at 430°-780° C. and into a molten bath in which the flat steel product is coated with the metallic coating.

    摘要翻译: 一种用于热浸涂覆超过5重量%的扁平不锈钢产品的方法。 %Cr,具有保护性金属涂层:在无氧加热气氛下将扁钢产品在1-30秒内加热至100℃-600℃; 通过在惰性或还原气氛下加热至550℃-800℃,在氧化气氛下在该温度窗内保持1至15秒,继续加热至保持温度为750℃-950℃ ,并在惰性或还原气氛下继续加热,直到达到保持温度; 在还原气氛下保持10-120秒; 并在惰性或还原气氛中在430℃-780℃下将扁钢产品通过喷嘴区域并进入熔融浴,其中扁钢产品被金属涂层涂覆。

    Method for Hot Dip Coating of a Flat Steel Product
    2.
    发明申请
    Method for Hot Dip Coating of a Flat Steel Product 有权
    扁钢产品热浸镀方法

    公开(公告)号:US20140144550A1

    公开(公告)日:2014-05-29

    申请号:US13819481

    申请日:2011-08-18

    IPC分类号: C23C2/02

    摘要: A method for hot dip coating a flat stainless steel product with more than 5 wt. % Cr with a protective metallic coating by: heating the flat steel product under an oxygen-free heating atmosphere to 100° C.-600° C. within 1-30 seconds; continuing heating to a holding temperature of 750° C.-950° C., by heating to 550° C.-800° C. under an inert or reducing atmosphere, holding within this temperature window for 1 to 15 seconds under an oxidising atmosphere, and continuing heating under an inert or reducing atmosphere, until the holding temperature is reached; holding at the holding temperature for 10-120 seconds under a reducing atmosphere; and passing the flat steel product through a nozzle area under an inert or reducing atmosphere at 430°-780° C. and into a molten bath in which the flat steel product is coated with the metallic coating.

    摘要翻译: 一种用于热浸涂覆超过5重量%的扁平不锈钢产品的方法。 %Cr,具有保护性金属涂层:在无氧加热气氛下将扁钢产品在1-30秒内加热至100℃-600℃; 通过在惰性或还原气氛下加热至550℃-800℃,在氧化气氛下在该温度窗口内保持1至15秒,继续加热至保持温度为750℃-950℃ ,并在惰性或还原气氛下继续加热,直到达到保持温度; 在还原气氛下保持10-120秒; 并在惰性或还原气氛中在430℃-780℃下将扁钢产品通过喷嘴区域并进入熔融浴,其中扁钢产品被金属涂层涂覆。