Nonaqueous electrolyte secondary battery
    5.
    发明申请
    Nonaqueous electrolyte secondary battery 失效
    非水电解质二次电池

    公开(公告)号:US20060216607A1

    公开(公告)日:2006-09-28

    申请号:US11385656

    申请日:2006-03-22

    IPC分类号: H01M4/62 H01M4/50 H01M4/52

    摘要: A non-aqueous electrolyte secondary battery includes a positive electrode (1) containing lithium cobalt oxide as a positive electrode active material, a negative electrode (2) containing molybdenum dioxide as a negative electrode active material, and a non-aqueous electrolyte. The mass ratio of the negative electrode active material to the positive electrode active material is within the range of from 0.725 to 0.480. The conductive agent of the negative electrode consists of a carbon material having a lattice constant C0 along a stacking direction of from 6.7 Å to 6.8 Å, as determined by X-ray diffraction, or the negative electrode contains no conductive agent made of carbon material.

    摘要翻译: 非水电解质二次电池包括含有作为正极活性物质的钴酸锂的正极(1),含有二氧化钼作为负极活性物质的负极(2)和非水电解质。 负极活性物质与正极活性物质的质量比在0.725〜0.480的范围内。 负极的导电剂由通过X射线衍射确定的沿着层叠方向的晶格常数C 0的碳材料构成,或者负极含有 没有由碳材料制成的导电剂。

    Nonaqueous electrolyte secondary battery
    10.
    发明授权
    Nonaqueous electrolyte secondary battery 失效
    非水电解质二次电池

    公开(公告)号:US07655356B2

    公开(公告)日:2010-02-02

    申请号:US11385656

    申请日:2006-03-22

    IPC分类号: H01M4/58 H01M10/40

    摘要: A non-aqueous electrolyte secondary battery includes a positive electrode (1) containing lithium cobalt oxide as a positive electrode active material, a negative electrode (2) containing molybdenum dioxide as a negative electrode active material, and a non-aqueous electrolyte. The mass ratio of the negative electrode active material to the positive electrode active material is within the range of from 0.725 to 0.480. The conductive agent of the negative electrode consists of a carbon material having a lattice constant C0 along a stacking direction of from 6.7 Å to 6.8 Å, as determined by X-ray diffraction, or the negative electrode contains no conductive agent made of carbon material.

    摘要翻译: 非水电解质二次电池包括含有作为正极活性物质的钴酸锂的正极(1),含有二氧化钼作为负极活性物质的负极(2)和非水电解质。 负极活性物质与正极活性物质的质量比在0.725〜0.480的范围内。 负极的导电剂由通过X射线衍射测定的沿着层叠方向的晶格常数C0的碳材料构成,或者负极不含有由碳材料制成的导电剂。