摘要:
According to one embodiment, an electrode includes a current collector, an active material-containing layer, a first peak, a second peak and a pore volume. The active material-containing layer contains an active material having a lithium absorption potential of 0.4 V (vs. Li/Li+) or more. The first peak has a mode diameter of 0.01 to 0.1 μm in a diameter distribution of pores detected by mercury porosimetry. The second peak has a mode diameter of 0.2 μm (exclusive) to 1 μm (inclusive) in the diameter distribution of pores. The pore volume detected by the mercury porosimetry is within a range of 0.1 to 0.3 mL per gram of a weight of the electrode excluding a weight of the current collector.
摘要翻译:根据一个实施例,电极包括集电器,含活性材料的层,第一峰,第二峰和孔体积。 含活性物质的层含有锂吸收电位为0.4V(相对于Li / Li +)以上的活性物质。 在通过水银孔率法检测的孔的直径分布中,第一峰的模式直径为0.01〜0.1μm。 第二峰在孔的直径分布中的模式直径为0.2μm(不包括)至1μm。 通过水银孔率法检测的孔体积在0.1至0.3mL /克重量的电极之外,不包括集电体的重量。
摘要:
According to one embodiment, a battery electrode includes an active material layer and a current collector is provided. The active material layer contains particles of a monoclinic β-type titanium complex oxide and particles of a lithium titanate having a spinel structure. When a particle size frequency distribution of particles contained in the active material layer is measured by the laser diffraction and scattering method, a first peak P1 appears in a range of 0.3 μm to 3 μm and a second peak P2 appears in a range of 5 μm to 20 μm in the frequency distribution diagram. The ratio FP1/FP2 of the frequency FP1 of the first peak P1 to the frequency FP2 of the second peak P2 is 0.4 to 2.3.
摘要:
According to one embodiment, a battery electrode includes an active material layer and a current collector is provided. The active material layer contains particles of a monoclinic β-type titanium complex oxide and particles of a lithium titanate having a spinel structure. When a particle size frequency distribution of particles contained in the active material layer is measured by the laser diffraction and scattering method, a first peak P1 appears in a range of 0.3 μm to 3 μm and a second peak P2 appears in a range of 5 μm to 20 μm in the frequency distribution diagram. The ratio FP1/FP2 of the frequency FP1 of the first peak P1 to the frequency FP2 of the second peak P2 is 0.4 to 2.3.
摘要:
According to one embodiment, there is provided an electrode for a nonaqueous electrolyte battery. The electrode includes an active material layer. The active material layer includes a monoclinic β-type titanium composite oxide. When the electrode is subjected to an X-ray diffraction measurement using a Cu-Kα ray source, a ratio of a reflection intensity I(020) of a peak derived from a plane (020) of a crystal of the monoclinic β-type titanium composite oxide to a reflection intensity I(001) of a peak derived from a plane (001) of the crystal of the monoclinic β-type titanium composite oxide being in the range from 0.6 to 1.2.
摘要:
According to one embodiment, there is provided an electrode for a nonaqueous electrolyte battery. The electrode includes an active material layer. The active material layer includes a monoclinic β-type titanium composite oxide. When the electrode is subjected to an X-ray diffraction measurement using a Cu-Kα ray source, a ratio of a reflection intensity I(020) of a peak derived from a plane (020) of a crystal of the monoclinic β-type titanium composite oxide to a reflection intensity I(001) of a peak derived from a plane (001) of the crystal of the monoclinic β-type titanium composite oxide being in the range from 0.6 to 1.2.
摘要:
According to one embodiment, there is provided an active material. The active material includes a titanate oxide compound. The active material has a peak appearing in a range of 1580 cm−1 to 1610 cm−1 in the infrared diffusion reflective spectrum when pyridine is absorbed onto the active material and released from it, after that, the active material is subjected to measurement of the infrared diffusion reflective spectrum. Further, a relationship represented by the following formula (I) is satisfied: S1/S2≧2.4 (I). Wherein S1 indicates an area of a peak appearing in a range of 1430 cm−1 to 1460 cm−1 in the spectrum, and S2 indicates an area of a peak appearing in a range of 1520 cm−1 to 1560 cm−1 in the spectrum.
摘要:
According to one embodiment, there is provided an electrode. The electrode includes a current collector and an active material layer provided on the current collector. The active material layer contains an active material and an acrylic based polymer.
摘要:
According to one embodiment, a non-aqueous electrolyte battery includes an electrode group. The electrode group includes a positive electrode and a negative electrode. At least one of the positive electrode or the negative electrode has a first electrode part and a second electrode part. The first electrode part includes a first metal substrate and an active material-containing part. The second electrode part includes a second metal substrate and an active material-containing part. The first metal substrate has a tensile strength larger than a tensile strength of the second metal substrate. A part of the first electrode part is provided more outside of the electrode group than a part of the second electrode group.
摘要:
According to one embodiment, a nonaqueous electrolyte secondary battery includes a nonaqueous electrolytic solution, a positive electrode and a negative electrode is provided. The nonaqueous electrolytic solution comprises a nonaqueous solvent. The nonaqueous solvent comprises from 50 to 95% by volume of a sulfone-based compound represented by the following formula 1: wherein R1 and R2 are each an alkyl group having 1 to 6 carbon atoms and satisfy R1≠R2. The positive electrode comprises a composite oxide represented by Li1-xMn1.5-yNi0.5-zMy+zO4. The negative electrode comprises a negative electrode active material being capable of absorbing and releasing lithium at 1 V or more based on a metallic lithium potential.
摘要:
According to one embodiment, a non-aqueous electrolyte battery includes an electrode group. The electrode group includes a positive electrode and a negative electrode. At least one of the positive electrode or the negative electrode has a first electrode part and a second electrode part. The first electrode part includes a first metal substrate and an active material-containing part. The second electrode part includes a second metal substrate and an active material-containing part. The first metal substrate has a tensile strength larger than a tensile strength of the second metal substrate. A part of the first electrode part is provided more outside of the electrode group than a part of the second electrode group.