1.
公开(公告)号:US20190017549A1
公开(公告)日:2019-01-17
申请号:US16070554
申请日:2016-08-25
Applicant: NATIONAL INSTITUTE FOR MATERIALS SCIENCE
Inventor: Masahiro GOTO , Michiko SASAKI , Akira KASAHARA , Masahiro TOSA
Abstract: ZnO sputtering is performed while a rolling body is housed in a basket made of a metal wire and is rotated. By setting a ratio of a mesh size of the basket to a diameter of the rolling body in a range of 40 to 95%, fine and uniform ZnO coating can be formed on a surface of the rolling body. By using the rolling body with ZnO coating prepared in this manner in a bearing which is rotated at high speed in a high-load state, a friction coefficient can significantly be lowered in comparison with a case of no coating.
-
公开(公告)号:US20180155183A1
公开(公告)日:2018-06-07
申请号:US15576376
申请日:2016-05-25
Applicant: NATIONAL INSTITUTE FOR MATERIALS SCIENCE
Inventor: Michiko SASAKI , Masahiro GOTO , Akira KASAHARA , Masahiro TOSA
IPC: B81B3/00 , C23C14/35 , C10M103/06 , C23C14/08
CPC classification number: B81B3/0005 , B81B3/0078 , B81B7/02 , B81B2201/035 , B81C2201/0119 , B81C2201/0181 , C10M103/06 , C10M2201/0623 , C23C14/08 , C23C14/086 , C23C14/35
Abstract: Low friction coating of the present invention includes a boron-doped zinc oxide thin film, wherein piezoelectric polarization in a vertical direction perpendicular to a film surface and a lateral direction horizontal to the film surface occurs and a magnitude of the piezoelectric polarization in the vertical direction is within 150 pm and a magnitude of the piezoelectric polarization in the lateral direction is within 100 pm at 90% or more of measurement points. This makes it possible to greatly decrease the friction in a nanometer order.
-