Abstract:
A touchscreen sensor includes a transparent base material, a first transparent electrode pattern, a first index-matching layer and a first adhesive layer disposed in this order at one side of the transparent base material, and a second transparent electrode pattern, a second index-matching layer and a second adhesive layer disposed in this order at another side of the transparent base material. The first index-matching layer has a refractive index greater than a refractive index of the first adhesive layer. The second index-matching layer has a refractive index greater than a refractive index of the second adhesive layer. Each of the first index-matching layer and the second index-matching layer has a thickness of 85 nm to 120 nm.
Abstract:
The present invention relates to a water-resistant organic thin film obtained by crosslinking, with organic nitrogen compounds, an organic thin film comprising an organic dye having an anionic group, wherein the organic nitrogen compounds are first, second, and third acyclic organic nitrogen compounds each having two or more nitrogen atoms per molecule, wherein the nitrogen atoms of each of the first, second, and third organic nitrogen compounds are each in a cationic group, and the relation A≤0.4 nm
Abstract:
In the case where a pressure-sensitive adhesive sheet comprising a pressure-sensitive adhesive layer having a refractive index adjustment zone is provided in such a manner that two PET separators are laminated to opposite surfaces of the pressure-sensitive adhesive layer, it is difficult to distinguish between obverse and reverse sides of the pressure-sensitive adhesive sheet itself. The present invention is directed to solving the above problems and, specifically, to offering a pressure-sensitive adhesive sheet having a refractive index adjustment zone capable of being easily produced at low cost, in a state in which it is preliminarily laminated with a substrate provided with an electroconductive layer, thereby making it possible to resolve complexity in handling (to easily distinguish between one surface defined by the refractive index adjustment zone and the other surface defined by the remaining zone).
Abstract:
Provided is a method for manufacturing a long laminate film having a uniform coating layer while suppressing wrinkling of the coating receiving surface of a long film used as a base film,the method including supporting the long film with first and second guide rolls while feeding the long film, nipping transverse both ends of the long film with a pair of nip rolls and the guide roll while feeding the long film, and applying a coating material to the long film to form a coating layer, wherein the guide roll has both end parts, which are arranged opposite to the pair of nip rolls, and a middle part other than both end parts, and both end parts have an outer diameter larger than that of the middle part.
Abstract:
The present invention provides a method for producing a waterproof organic thin film being capable of restraining the generation of defects such as a crack. The method for producing a waterproof organic thin film includes a waterproofing step of preparing a long laminate having an organic thin film and bringing at least the organic thin film into contact with a waterproofing-treatment liquid, a washing step of washing at least the organic thin film surface of the long laminate, and a conveying step to be performed between the waterproofing step and the washing step, the conveying step being a step of conveying the long laminate from the waterproofing step to the washing step, wherein in the conveying step, the long laminate is conveyed while the waterproofing-treatment liquid remaining on the organic thin film surface is caused to flow relatively to the organic thin film surface.
Abstract:
A laminate of optical elements comprises a transparent first optical element, a second optical element, and a transparent pressure-sensitive adhesive layer for bonding the first optical element to the second optical element. The pressure-sensitive adhesive layer comprises a base adhesive zone, a transparent refractive index-adjusting zone. The base adhesive zone is made essentially of a transparent base pressure-sensitive adhesive material and formed over a given range from a first principal surface of the pressure-sensitive adhesive layer facing the first optical element, in a thickness direction of the pressure-sensitive adhesive layer. The a transparent, adherent, refractive index-adjusting zone is formed over a given range from a second principal surface of the pressure-sensitive adhesive layer facing the second optical element.
Abstract:
As one sensor layer structure for a capacitive touch panel, a layer structure in which a transparent electroconductive layer is formed on each of opposite surfaces of a single film substrate, so-called GFD structure, is used. In the structure, for sufficiently suppressing internal reflection from the transparent electroconductive layer, it is necessary to employ a technique of forming one or more refractive index adjustment (IM) layers on each of the opposite surfaces of the single film substrate. This causes a problem that production yield is likely to deteriorate, and a production cost is increased. The present invention is directed to solving such a problem and, specifically, to laminating a refractive index adjustment zone-formed pressure-sensitive adhesive layer capable of being produced easily and at low cost, to each transparent electroconductive layer of a double-sided transparent electroconductive film, so as to effectively suppress internal reflection in the resulting laminate.
Abstract:
A touchscreen sensor includes a transparent base material, a first index-matching layer, a first transparent electrode pattern, a second index-matching layer and a first adhesive layer disposed in this order at one side of the transparent base material, and a third index-matching layer, a second transparent electrode pattern, a fourth index-matching layer and a second adhesive layer disposed in this order at another side of the transparent base material. Each of the first, second, third and fourth index-matching layers has a refractive index of 1.6 to 1.8 and a thickness of 50 nm to 150 nm.
Abstract:
A method for manufacturing a water resistant optically anisotropic film capable of suppressing the generation of a defect such as a crack or separation is provided. The method for manufacturing the water resistant optically anisotropic of the present invention includes a water resistant treatment step of bringing an optically anisotropic film containing an organic dye having an anionic group into contact with a water resistant treatment liquid containing a multivalent cationic compound and a monovalent cationic compound, and the mass ratio of the multivalent cationic compound and the monovalent cationic compound contained in the water resistant treatment liquid, monovalent cationic compound/multivalent cationic compound, is 0.01 to 2.
Abstract:
The present invention provides a method for producing a waterproof organic thin film being capable of restraining the generation of defects such as a crack. The method for producing a waterproof organic thin film includes a waterproofing step of preparing a long laminate having an organic thin film and bringing at least the organic thin film into contact with a waterproofing-treatment liquid, a washing step of washing at least the organic thin film surface of the long laminate, and a conveying step to be performed between the waterproofing step and the washing step, the conveying step being a step of conveying the long laminate from the waterproofing step to the washing step, wherein in the conveying step, the long laminate is conveyed while the waterproofing-treatment liquid remaining on the organic thin film surface is caused to flow relatively to the organic thin film surface.