Method of producing ultra-low-carbon steel
    2.
    发明授权
    Method of producing ultra-low-carbon steel 失效
    生产超低碳钢的方法

    公开(公告)号:US5221326A

    公开(公告)日:1993-06-22

    申请号:US700605

    申请日:1991-05-15

    IPC分类号: C21C7/10

    CPC分类号: C21C7/10

    摘要: A method of producing an ultra-low-carbon steel by conducting vacuum-decarburization of a molten steel by means of a vacuum degasifier of the type having recirculation pipes and a vacuum chamber. When the carbon content of the molten steel has come down to a level of 50 ppm or less, hydrogen gas is introduced together with an inert gas into the molten steel either by directly injecting a hydrogen-containing gas into the molten steel in the vacuum chamber through a tuyere provided in the wall of the vacuum chamber or by blowing the hydrogen-containing gas onto the surface of the molten steel in the vacuum chamber through a lance provided in the vacuum chamber. In order to enhance the effect produced by the method of the present invention, it is possible to take an additional measure such as blowing of hydrogen gas through a tuyere provided in the wall of the recirculation pipe or injection of hydrogen or hydrogen-containing gas through an injection lance immersed in the molten steel held in, a ladle.

    Method of producing ultra-low-carbon steel
    4.
    发明授权
    Method of producing ultra-low-carbon steel 失效
    生产超低碳钢的方法

    公开(公告)号:US5152831A

    公开(公告)日:1992-10-06

    申请号:US767984

    申请日:1991-09-30

    IPC分类号: C21C7/10

    CPC分类号: C21C7/10

    摘要: A method of producing an ultra-low-carbon steel by using a vacuum degasser on a molten steel has the steps of conducting vacuum decarburization to attain a predetermined level of carbon content, e.g., 25 ppm or below, in the molten steel while progressively reducing the pressure in said vacuum degasser, conducting addition of hydrogen in which hydrogen is dissolved in said molten steel while said pressure is temporarily elevated to 20 Torr or above, and conducting final decarburization after reducing said pressure to 2 Torr or below. The addition of hydrogen may be conducted to meet the following conditions:[H].gtoreq.{([C]-[C]final)/5}+4wherein [H] represents the hydrogen content (ppm) in said molten steel in the state after the addition of hydrogen, [C] represents the carbon content (ppm) in the molten steel in the state after the addition of hydrogen, and [C] final represents the final carbon content (ppm) to be obtained.