公开(公告)号:US06649270B2
公开(公告)日:2003-11-18
申请号:US09984366
申请日:2001-10-30
申请人: Toshiharu Kinoshita , Shigeru Ogura
发明人: Toshiharu Kinoshita , Shigeru Ogura
IPC分类号: B32B904
CPC分类号: C04B38/00 , C04B35/573 , H01J2217/49264 , H01L21/673 , Y10T428/30 , C04B35/14 , C04B35/565 , C04B38/0074
摘要: There is provided a jig for use in heat treatment onto which a vitreous plate having had films exhibiting respective given functions formed on its surface is to be loaded when the vitreous plate undergoes heat treatment. The jig contains 50% by weight or more phase containing SiC, its thermal conductivity is 10 W/mK or more, its apparent porosity 0.2 to 25%, and in that its coefficient of thermal expansion is 3.8×10−6/°C. to 5.5×10−6/°C.
摘要翻译: 提供了一种用于热处理的夹具,当玻璃板进行热处理时,其上装有具有在其表面上形成有各自的功能的膜的玻璃板被装载。 夹具含有50重量%以上的含SiC相,其导热率为10W / mK以上,表观孔隙率为0.2〜25%,热膨胀系数为3.8×10 -6 /℃ 。 至5.5×10 -6 /℃。
-
公开(公告)号:US4432533A
公开(公告)日:1984-02-21
申请号:US364414
申请日:1982-04-01
申请人: Masuto Shimizu , Tadashi Morimoto , Motoyasu Yaji , Masaaki Tsukamoto , Takao Suzuki , Shigeru Ogura
发明人: Masuto Shimizu , Tadashi Morimoto , Motoyasu Yaji , Masaaki Tsukamoto , Takao Suzuki , Shigeru Ogura
CPC分类号: C21C5/443 , B05B7/20 , B22D41/02 , F27D1/1652 , F27D19/00 , F27D2001/1657
摘要: A method of repairing a refractory lining of a vessel lined with refractory by flame gunning process, in which a patching material consisting of refractory particles and carbonaceous fuel powder is flame-gunned together with an oxygen containing gas to fuse or semi-fuse the refractory particles in a region surrounded by high-temperature flame and struck against the surface of the refractory lining to produce a deposit layer of the refractory particles, is disclosed. In this method, a patching material having a higher mixing ratio of the fuel powder or only the fuel powder is flame-gunned at an initial stage of the repairing and subsequently patching materials, in which the mixing ratio of the fuel powder is lowered stepwise, are flame-gunned in order with the progress of the repairing, during which a blow rate of the oxygen containing gas is controlled in accordance with the change of the mixing ratio of the fuel powder in the patching material.
摘要翻译: 一种通过火焰喷涂方法修复耐火材料衬里耐火衬里的方法,其中将由耐火颗粒和含碳燃料粉末组成的修补材料与含氧气体一起火焰喷射以熔化或半熔融耐火颗粒 在由高温火焰包围并撞击耐火衬里表面以产生耐火颗粒的沉积层的区域中。 在该方法中,在燃料粉末的混合比逐步降低的修理初期和随后的修补材料中,燃料粉末或仅燃料粉末的混合比高的修补材料被火焰喷射, 按照修补进度的顺序进行火焰喷射,根据修补材料中的燃料粉末的混合比的变化,控制含氧气体的吹入速率。
-
公开(公告)号:US5429655A
公开(公告)日:1995-07-04
申请号:US952891
申请日:1992-11-20
申请人: Shigeru Ogura , Masayuki Onishi , Hidenari Kitaoka , Mitsuru Sakurai , Toshikazu Sakuraya , Yozo Tanino , Tsukasa Terashima , Yoshiro Tomiyama , Yuki Nabeshima , Yuji Miki , Saburo Moriwaki , Noboru Yasukawa
发明人: Shigeru Ogura , Masayuki Onishi , Hidenari Kitaoka , Mitsuru Sakurai , Toshikazu Sakuraya , Yozo Tanino , Tsukasa Terashima , Yoshiro Tomiyama , Yuki Nabeshima , Yuji Miki , Saburo Moriwaki , Noboru Yasukawa
IPC分类号: B22D11/10 , B22D11/11 , B22D11/114 , B22D41/005
CPC分类号: B22D11/114 , B22D11/11
摘要: An apparatus for removing non-metallic foreign matter in a molten steel includes a tundish and a coil device. The tundish is an intermediate container receiving the molten steel from a ladle and feeding a purified molten steel by removing the non-metallic foreign matter in the molten steel. For removing the non-metallic foreign matter, the tundish has a swirl flow bath and a floatation bath. In the circumference of the swirl flow bath of the tundish, a coil device is arranged for flowing the molten steel in the swirl flow bath in swirl fashion. The tundish and the coil device are formed separately and constructed for relative movement to each other. The molten steel in the swirl flow bath of the tundish is flown in swirl fashion in the horizontal direction by a magnetic field generated by the coil device. At this time, the molten steel forms a parabolic concaved surface. The non-metallic foreign matter in the molten steel is forcedly floated up on the parabolic surface portion of the molten steel, which is removed by an appropriate means. The molten steel thus purified flows into the floatation bath from the swirl flow bath. With the static flow in the floatation bath, the residual non-metallic foreign matter floats up. The purified molten steel is poured into the mold through the bottom of the floatation bath.
摘要翻译: PCT No.PCT / JP92 / 00388 Sec。 371日期:1992年11月20日 102(e)日期1992年11月20日PCT提交1992年3月27日PCT公布。 出版物WO92 / 17295 日期:1992年10月15日。用于除去钢水中的非金属异物的设备包括中间包和线圈装置。 中间包是从钢包中接收钢水的中间包,并且通过去除钢水中的非金属异物来送入精炼的钢水。 为了去除非金属异物,中间包具有旋流池和漂浮浴。 在中间包的涡流槽的圆周上,设置有一个线圈装置,用于以漩涡的方式使旋转流槽中的钢水流动。 中间包和线圈装置分别形成并相互相对移动构造。 在中间包的涡流槽中的钢水由螺旋装置产生的磁场沿水平方向旋转地流动。 此时,钢水形成抛物面凹面。 钢水中的非金属杂质被强制地悬浮在钢水的抛物面上,通过适当的方式去除。 这样净化的钢水从涡流浴流入浮选槽。 随着浮选槽中的静态流动,剩余的非金属异物浮起。 将纯化的钢水通过浮选槽的底部倒入模具中。
-
公开(公告)号:US4955126A
公开(公告)日:1990-09-11
申请号:US341142
申请日:1989-04-20
申请人: Masaru Shibata , Masayuki Onishi , Hitoshi Ohsugi , Shigeru Ogura , Masaru Washio , Hideo Kuguminato , Yoshiaki Hara
发明人: Masaru Shibata , Masayuki Onishi , Hitoshi Ohsugi , Shigeru Ogura , Masaru Washio , Hideo Kuguminato , Yoshiaki Hara
IPC分类号: B21B1/02 , B21B1/22 , B22D11/126 , B23K7/00 , B24B27/033
CPC分类号: B22D11/126 , B23K7/003 , B24B27/033 , Y10T29/49989
摘要: A process for fusing a steel slab in a longitudinal direction thereof is disclosed, wherein when the steel slab is fused in the longitudinal direction at more than 500.degree. C. and at a speed of more than 300 mm/min., a surface portion of the slab including at least a lower portion of a longitudinally fused surface portion thereof is mechanically removed by cutting or grinding.
摘要翻译: 公开了一种将钢坯沿其长度方向熔融的方法,其中当钢坯沿纵向熔融在大于500℃并以大于300mm / min的速度时,表面部分 包括其纵向熔融表面部分的至少下部的板坯通过切割或研磨被机械地去除。
-
公开(公告)号:US06739894B2
公开(公告)日:2004-05-25
申请号:US10153638
申请日:2002-05-24
申请人: Shigeru Ogura
发明人: Shigeru Ogura
IPC分类号: H01R1362
CPC分类号: H01R13/2421
摘要: A socket for an IC package avoids deformation or damage of an IC package body. The socket includes a socket body having a receptacle portion of the IC package and a plurality of contacts arranged on a bottom surface of the receptacle portion and resiliently displaceable in up and down directions. Latches are pivotably provided in the socket body and being biased toward the receptacle portion by springs. The socket further includes connecting metals provided for relative motion with respect to the socket body and for moving the latches away from the receptacle portion against the springs, slots and projections restricting motion magnitude toward the bottom surface of the receptacle portion at a predetermined value.
摘要翻译: 用于IC封装的插座避免IC封装体的变形或损坏。 插座包括具有IC封装的插座部分的插座主体和布置在插座部分的底表面上并可沿上下方向弹性移位的多个触点。 闩锁可枢转地设置在插座主体中并且通过弹簧朝向插座部分偏置。 插座还包括为相对于插座本体提供相对运动的连接金属,并且用于将闩锁远离插座部分抵靠弹簧,槽和突起以预定值朝着插座部分的底表面限制运动大小。
-
公开(公告)号:US06379425B1
公开(公告)日:2002-04-30
申请号:US09588465
申请日:2000-06-06
IPC分类号: C21C530
CPC分类号: C21C1/025 , C21C7/0645
摘要: Desulfurization is carried out by blowing CaO into molten iron, and a gas mixture of an inert gas and a hydrocarbon gas is used as a carrier. The ratio of the hydrocarbon gas to the desulfurizing agent is maintained in the range of from about 2.0 to about 50 Nl/kg. This desulfurizing method improves the desulfurization efficiency of the desulfurizing agent, increases the productivity of the desulfurizing process, and reduces the amount of slag generated in the desulfurizing process. Alternatively, a desulfurizing flux is blown into the molten iron together with a carrier gas comprising a gas mixture of an inert gas and a hydrocarbon gas or an inert gas alone at the start of desulfurization. The hydrocarbon gas in the carrier gas is increased, is added, or the unit gas is replaced by the hydrocarbon gas at adequate timing, whereby the desulfurization efficiency is improved.
摘要翻译: 通过将CaO吹入铁水中进行脱硫,使用惰性气体和烃气体的气体混合物作为载体。 烃气体与脱硫剂的比率保持在约2.0至约50Nl / kg的范围内。 该脱硫方法提高脱硫剂的脱硫效率,提高脱硫工序的生产率,并且减少脱硫过程中产生的炉渣的量。 或者,在脱硫开始时,将脱硫助熔剂与包含惰性气体和烃气体或惰性气体的气体混合物的载气一起吹入铁水中。 载气中的烃气体被添加,或者在合适的时间单位气体被烃气体代替,从而提高了脱硫效率。
-
公开(公告)号:US06328784B1
公开(公告)日:2001-12-11
申请号:US09605741
申请日:2000-06-29
IPC分类号: C21C102
CPC分类号: C21C1/025 , C21C1/06 , C21C7/0645 , Y02P10/212
摘要: A process for desulfurizing a molten iron alloy in which a desulfurizing agent is applied to the molten iron alloy under agitation. Concurrently, a gas containing a hydrocarbon gas is blown onto the bath surface of the molten iron alloy, or a substance generating a hydrocarbon gas is added to the bath surface.
摘要翻译: 在搅拌下向铁水合金中施加脱硫剂的铁水合金脱硫方法。 同时,将含有烃气体的气体吹入到铁水合金的熔池表面,或者向浴槽表面添加产生烃气体的物质。
-
公开(公告)号:US5028033A
公开(公告)日:1991-07-02
申请号:US415346
申请日:1989-09-07
CPC分类号: B22D2/001 , B22D37/00 , C21C5/4653 , C21C5/4673 , C21C7/0043
摘要: A method is disclosed for accurately detecting an outflow of a slag into a stream of a molten steel when the molten steel is poured from a first vessel such as a refining furnace or a ladle into an intermediate vessel such as a ladle or a tundish through a melt-discharging hole or a nozzle. At that time, an inert gas is fed into the stream of the molten steel in the nozzle through a side portion of the melt-discharging hole or the nozzle, and the detection is made based on a change in a flow rate of the inert gas sucked into the stream of the molten steel and/or in a back pressure.
-
-
-
-
-
-
-