公开(公告)号:US20240239961A1
公开(公告)日:2024-07-18
申请号:US18559423
申请日:2022-05-03
申请人: OULUN YLIOPISTO
发明人: Jarkko TOLVANEN , Mikko NELO , Jari HANNU , Jari JUUTI , Heli JANTUNEN
CPC分类号: C08G77/20 , C08K3/38 , C08K2201/005 , C08K2201/011
摘要: The invention relates to a method for manufacturing a self-healing elastomer, comprising preparing, with respect to the total weight of the self-healing elastomer, 0.1-5 wt. % of boron trioxide (B2O3), 65-90 wt. % of hydroxyl-terminated polydimethylsiloxane (PDMS-OH), 5-30 wt. %, when measured in combined, of polysiloxane precursors, being a first composition comprising a siloxane base, and a second composition comprising a siloxane crosslinker, wherein the ratio by weight of the first composition and the second composition is 1:1 to 50:1; homogeneously mixing B2O3, PDMS-OH, and the first composition, thereby obtaining a mixture, reacting the mixture and the second composition at an elevated temperature ranging from 60° C. to 150° C., endpoints inclusive, thereby obtaining the self-healing elastomer.
-
公开(公告)号:US20240228781A1
公开(公告)日:2024-07-11
申请号:US18559401
申请日:2022-05-03
申请人: OULUN YLIOPISTO
发明人: Jarkko TOLVANEN , Mikko NELO , Jari HANNU , Jari JUUTI , Heli JANTUNEN
CPC分类号: C08L83/06 , C08G77/56 , C08L2205/025 , C08L2205/04
摘要: The invention relates to a method for manufacturing a self-healing elastomer, comprising preparing, with respect to the total weight of the self-healing elastomer, 0.1-5 wt. % of boron trioxide (B2O3), 65-90 wt. % of hydroxyl-terminated polydimethylsiloxane (PDMS-OH), 5-30 wt. %, when measured in combined, of polysiloxane precursors, being a first composition comprising a siloxane base, and a second composition comprising a siloxane crosslinker, wherein the ratio by weight of the first composition and the second composition is 1:1 to 50:1; reacting B2O3 and PDMS-OH at an elevated temperature ranging from 60° C. to 200° C., endpoints inclusive, thereby obtaining a first mixture, mixing the first mixture with an alcohol, and then the first composition, thereby obtaining a second mixture, reacting the second mixture and the second composition, thereby obtaining the self-healing elastomer.
-
公开(公告)号:US20230192553A1
公开(公告)日:2023-06-22
申请号:US18113432
申请日:2023-02-23
申请人: Oulun yliopisto
发明人: Jari HANNU , Jari JUUTI , Heli JANTUNEN , Mikko NELO , Tuomo SIPONKOSKI , Hanna KÄHÄRI
CPC分类号: C04B35/00 , B22F3/02 , C22C1/051 , C22C32/0015 , B22F1/052 , B22F2302/25
摘要: A process for manufacturing ceramic-metal composite material, comprises dissolving ceramic powder into water to obtain an aqueous solution of ceramic; mixing metal powder having a multimodal particle size where largest particle size is one fourth of the minimum dimension of a device, with the aqueous solution of ceramic to obtain a powder containing ceramic precipitated on the surface of metal particles; mixing the powder containing ceramic precipitated on the surface of the metal particles, with ceramic powder having a particle size below 50 μm, to obtain a powder mixture; adding saturated aqueous solution of ceramic to the powder mixture to obtain an aqueous composition containing ceramic and metal; compressing the aqueous composition to form a disc of ceramic-metal composite material containing ceramic and metal; and removing water from the ceramic-metal composite material; wherein ceramic content of the disc is 10 vol-% to 35 vol-%. Alternatively, ceramic-ceramic composite material may be manufactured.
-
-