公开(公告)号:US09356321B2
公开(公告)日:2016-05-31
申请号:US14419184
申请日:2013-10-22
Inventor: Etsuko Ogasawara , Misaki Harada , Kazuhiro Sugie , Kenji Izumi , Yu Kojima , Kazuhiko Shimoda , Kazunari Ando
IPC: H01M10/06 , H01M10/12 , H01M2/28 , H01M4/14 , H01M4/56 , H01M4/73 , H01M4/68 , H01M10/08 , H01M4/57 , H01M10/42 , H01M2/24 , H01M2/26 , H01M2/30 , H01M4/02
CPC classification number: H01M10/12 , H01M2/24 , H01M2/266 , H01M2/28 , H01M2/305 , H01M4/14 , H01M4/56 , H01M4/57 , H01M4/68 , H01M4/685 , H01M4/73 , H01M10/08 , H01M2004/021 , H01M2010/4292 , H01M2220/20 , Y02E60/126
Abstract: In a lead-acid battery including an electrode plate group housed in a cell chamber 6 with an electrolyte, each positive electrode plate includes a positive electrode grid made of lead or a lead alloy containing no antimony, and a positive electrode active material with which the positive electrode grid is filled. Each negative electrode plate includes a negative electrode grid made of lead or a lead alloy containing no antimony, a surface layer formed on a surface of the negative electrode grid and made of a lead alloy containing antimony, and a negative electrode active material with which the negative electrode grid is filled. A mass ratio MN/MP falls within a range of 0.70 to 1.10, where MP represents the mass of the positive electrode active material per cell chamber, and MN represents the mass of the negative electrode active material per cell chamber.
Abstract translation: 在包含电解槽室6的电极板组的铅酸蓄电池中,每个正极板包括由不含锑的铅或铅合金制成的正极栅极和正极活性物质, 正极栅格填充。 每个负极板包括由铅或不含锑的铅合金制成的负极栅极,在负极栅格的表面上形成的由含有锑的铅合金制成的表面层,以及负极活性物质, 负极栅格填充。 质量比MN / MP落在0.70〜1.10的范围内,其中MP表示每个电池室的正极活性物质的质量,MN表示每个电池室的负极活性物质的质量。
-
公开(公告)号:US10276895B2
公开(公告)日:2019-04-30
申请号:US15541890
申请日:2015-12-18
Inventor: Tetsuyuki Murata , Hideharu Takezawa , Kazunari Ando
Abstract: An objective is to improve the corrosion resistance of a positive electrode grid for lead acid batteries.Provided is a positive electrode grid for lead acid batteries, and a lead acid battery including the grid. The grid includes a lead alloy containing calcium and tin. The lead alloy has a calcium content of 0.10 mass % or less, and a tin content of 2.3 mass % or less, and a lattice constant of 4.9470 Å or less.
-
公开(公告)号:US20150200424A1
公开(公告)日:2015-07-16
申请号:US14419184
申请日:2013-10-22
Inventor: Etsuko Ogasawara , Misaki Harada , Kazuhiro Sugie , Kenji Izumi , Yu Kojima , Kazuhiko Shimoda , Kazunari Ando
CPC classification number: H01M10/12 , H01M2/24 , H01M2/266 , H01M2/28 , H01M2/305 , H01M4/14 , H01M4/56 , H01M4/57 , H01M4/68 , H01M4/685 , H01M4/73 , H01M10/08 , H01M2004/021 , H01M2010/4292 , H01M2220/20 , Y02E60/126
Abstract: In a lead-acid batter including an electrode plate group housed in a cell chamber with an electrolyte, each positive electrode plate includes a positive electrode grid made of lead or a lead alloy containing no antimony, and a positive electrode active material with which the positive electrode grid is filled. Each negative electrode plate includes a negative electrode grid made of lead or a lead alloy containing no antimony, a surface layer formed on a surface of the negative electrode grid and made of a lead alloy containing antimony, and a negative electrode active material with which the negative electrode grid is filled. A mass ratio MN/MP falls within a range of 0.70 to 1.10, where MP represents the mass of the positive electrode active material per cell chamber, and MN represents the mass of the negative electrode active material per cell chamber.
Abstract translation: 在包含容纳在具有电解质的电池室中的电极板组的铅酸电池中,每个正电极板包括由铅或不含锑的铅合金制成的正极栅极和正极活性材料,正极活性材料具有阳极 电极栅格填充。 每个负极板包括由铅或不含锑的铅合金制成的负极栅极,在负极栅格的表面上形成的由含有锑的铅合金制成的表面层,以及负极活性物质, 负极栅格填充。 质量比MN / MP落在0.70〜1.10的范围内,其中MP表示每个电池室的正极活性物质的质量,MN表示每个电池室的负极活性物质的质量。
-
-