公开(公告)号:US4385077A
公开(公告)日:1983-05-24
申请号:US012933
申请日:1979-02-16
IPC分类号: A62D3/00 , A62D3/30 , A62D3/38 , A62D101/41 , A61K7/40
CPC分类号: A62D3/38 , A62D3/30 , D06M7/005 , A62D2101/41 , Y10T428/2907 , Y10T428/2958 , Y10T428/2993 , Y10T428/31652 , Y10T442/2926
摘要: A method of treating asbestos comprising depositing on at least a portion of the asbestos a material consisting essentially of an oxide of at least one metal selected from the group consisting of first series transition metals, second series transition metals, and group II B metals.
摘要翻译: 一种处理石棉的方法,包括在至少一部分石棉上沉积材料,该材料基本上由选自第一系列过渡金属,第二系列过渡金属和IIB族金属的至少一种金属的氧化物组成。
-
公开(公告)号:US4025449A
公开(公告)日:1977-05-24
申请号:US624363
申请日:1975-10-21
CPC分类号: C01G49/0036 , C04B35/2683 , C01P2002/02 , C01P2002/34 , C01P2002/76 , C01P2004/62 , C01P2006/42 , C01P2006/60 , C01P2006/80
摘要: A method to produce a magnetic barium or strontium ferrite comprising solubilizing an alkaline earth metal compound in an aqueous solution containing about 20 to about 60 weight percent alkali metal hydroxide. The resulting solution is heated to within the range of about 90.degree. to about 130.degree. C and thereafter admixed with a sufficient amount of a soluble iron compound to form a magnetic precipitate. A crystalline, magnetic ferrite is formed by heating the precipitate to within the range of about 800.degree. to about 1500.degree. C.
摘要翻译: 一种制造磁性钡或锶铁氧体的方法,其包括在含有约20至约60重量%碱金属氢氧化物的水溶液中溶解碱土金属化合物。 将所得溶液加热至约90℃至约130℃的范围,然后与足量的可溶性铁化合物混合以形成磁性沉淀。 通过将沉淀物加热至约800℃至约1500℃的范围来形成结晶的磁性铁氧体。
-
公开(公告)号:US4448654A
公开(公告)日:1984-05-15
申请号:US389835
申请日:1982-06-18
CPC分类号: C25C7/02
摘要: An uncoated ceramic anode comprising titanium having a formal valence of +4; titanium having a formal valence of +3; and a dopant which prevents at least a portion of the titanium +3 from converting to titanium +4 when the ceramic anode is at operating cell conditions. The ceramic anode may have an electrically conductive substance enclosed in its interior. The substance serves to transfer electrical energy from a power source to the ceramic member. These anodes are particularly useful when used in molten salt electrolytic cells because they give good electrolytic production rates while demonstrating exceptionally low wear rates.
摘要翻译: 包含正价为+4的钛的未涂覆的陶瓷阳极; 钛的正式化合价为+3; 以及当陶瓷阳极处于工作电池条件时,防止至少一部分钛+3转化为钛+4的掺杂剂。 陶瓷阳极可以具有封闭在其内部的导电物质。 该物质用于将电能从电源传递到陶瓷构件。 这些阳极在熔盐电解槽中使用时特别有用,因为它们在显示出非常低的磨损率的同时提供良好的电解生产率。
-
公开(公告)号:US4370216A
公开(公告)日:1983-01-25
申请号:US204733
申请日:1980-11-06
CPC分类号: C25C7/025
摘要: An uncoated ceramic anode comprising titanium having a formal valence of +4; titanium having a formal valence of +3; and a dopant which prevents at least a portion of the titanium +3 from converting to titanium +4 when the ceramic anode is at operating cell conditions. The ceramic anode may have an electrically conductive substance enclosed in its interior. The substance serves to transfer electrical energy from a power source to the ceramic member. These anodes are particularly useful when used in molten salt electrolytic cells because they give good electrolytic production rates while demonstrating exceptionally low wear rates.
摘要翻译: 包含正价为+4的钛的未涂覆的陶瓷阳极; 钛的正式化合价为+3; 以及当陶瓷阳极处于工作电池条件时,防止至少一部分钛+3转化为钛+4的掺杂剂。 陶瓷阳极可以具有封闭在其内部的导电物质。 该物质用于将电能从电源传递到陶瓷构件。 这些阳极在熔盐电解槽中使用时特别有用,因为它们在显示出非常低的磨损率的同时提供良好的电解生产率。
-
公开(公告)号:US5145833A
公开(公告)日:1992-09-08
申请号:US494938
申请日:1990-03-14
IPC分类号: C04B35/45 , C04B35/645 , C04B35/80 , H01L39/24
CPC分类号: C04B35/80 , C04B35/4508 , C04B35/645 , C04B35/6455 , H01L39/2419 , Y10S505/733 , Y10S505/739 , Y10S505/742
摘要: This invention provides a process for producing a ceramic body by heating a ceramic material, such as particulate zirconium oxide, to a temperature greater than about 30 percent of the material's melting temperature, but less than said melting temperature, and thereafter applying sufficient isostatic pressure to consolidate the ceramic material into a body having a density of at least 85 percent of the theoretical density of the material.This invention also provides a process for producing superconducting ceramic articles such as those represented by the general formula YBa.sub.2 Cu.sub.3 O.sub.7-x where 0
摘要翻译: 本发明提供一种通过将诸如颗粒状氧化锆的陶瓷材料加热到大于材料的熔融温度的约30%但小于所述熔融温度的温度来制造陶瓷体的方法,然后施加足够的等静压力 将陶瓷材料固结成具有至少材料理论密度的85%的密度的体。 本发明还提供一种制造超导陶瓷制品的方法,例如由通式YBa2Cu3O7-x表示的那些,其中0
-
-
-
-