摘要:
The present invention provides a method for making an offset printing plate according to the silver salt diffusion transfer process using rinsing water, characterized in that said rinsing water before washing at most 20 m.sup.2 of said exposed and developed imaging element and/or before being in use for more than 24 hours is brought in contact with (i) a metal of the group IB or IIB or VIII of the periodic table or (ii) with an alloy containing at least one of said metals or (iii) with a salt containing an ion of at least one of said metals.
摘要:
The present invention concerns a method for the treatment of stimulable phosphors and/or screens for use in diagnosis, in particular medical radiography. The method comprises subjecting the stimulable phosphors and/or screens to an epoxide containing gaseous compound, promptly following their manufacture. By applying the method according to the invention yellowing of the stimulable phosphors and/or screens is prevented in a safe and efficient manner; thereby the disadvantages known as such resulting from such yellowing will not occur.
摘要:
In favor of adhesion between phosphor layer and support in a radiation image phosphor or scintillator panel comprising as an arrangement of layers, in consecutive order, a support, a precoat layer and a phosphor or scintillator layer having needle-shaped phosphor or scintillator crystals, said precoat layer comprises as a binder an organic cross-linkable monomer, oligomer, polymer or a mixture thereof and a pigment in a weight ratio of pigment to binder in the range from 1/10 to 10/1.
摘要:
In a method of reading a radiation image, stored in a CsBr:Eu type binderless needle-shaped photostimulable or storage phosphor screen after X-ray exposure of said screen, said method comprises the steps of: (1) erasing thermally stimulable energy by exposing said screen to infrared radiation in the wavelength range from 1000 nm to 1550 nm; (2) stimulating said phosphor screen by means of stimulating radiation in the range from 550 to 850 nm; (3) detecting light emitted by the phosphor screen upon stimulation and converting the detected light into a signal representation of said radiation image; (4) erasing said phosphor screen by exposing it to erasing light in the wavelength range of 300 nm to 1500 nm.
摘要:
In favor of lowering corrosion of a radiation image phosphor or scintillator panel comprising, as a layer arrangement of consecutive layers, an anodized aluminum support, a sublayer and a phosphor or scintillator layer having needle-shaped phosphor or scintillator crystals, said sublayer comprises an inorganic metal oxide or a metal compound and has a thickness in the range from 0.1 μm to 2.5 μm.
摘要:
In a method for producing CsX:Eu stimulable phosphors and screens or panels provided with said phosphors as powder phosphors or vapor deposited needle-shaped phosphors suitable for use in image forming methods for recording and reproducing images of objects made by high energy radiation, said CsX:Eu stimulable phosphors are essentially free from oxygen in their crystal structure, wherein X represents a halide selected from the group consisting of Br, Cl and combinations thereof; and wherein the method further comprises the steps of mixing CsX with a compound or combinations of compounds having as a composition CsxEuyX′x+αy, wherein the ratio of x to y exceeds a value of 0.25, wherein α≧2 and wherein X′ is a halide selected from the group consisting of Cl, Br and I and combinations thereof; heating said mixture at a temperature above 450° C.; cooling said mixture, and, optionally, annealing and recovering said CsX:Eu phosphor.
摘要:
In a method for producing CsX:Eu stimulable phosphors and screens or panels provided with said phosphors as powder phosphors or vapor deposited needle-shaped phosphors suitable for use in image forming methods for recording and reproducing images of objects made by high energy radiation, said CsX:Eu stimulable phosphors are essentially free from oxygen in their crystal structure, wherein X represents a halide selected from the group consisting of Br, Cl and combinations thereof; and wherein the method further comprises the steps of mixing CsX with a compound or combinations of compounds having as a composition CsxEuyX′x+αy, wherein the ratio of x to y exceeds a value of 0.25, wherein α≧2 and wherein X′ is a halide selected from the group consisting of Cl, Br and I and combinations thereof; heating said mixture at a temperature above 450° C.; cooling said mixture, and, optionally, annealing and recovering said CsX:Eu phosphor.
摘要:
In a method of increasing humidity stability of a storage phosphor panel having a phosphor layer coated onto a support by vapor depositing raw phosphor precursor materials of a matrix and an activator component from one or more crucible(s) and/or crucible unit(s) in a vapor deposition apparatus, after ending vapor depositing an additional “over-annealing” step is performed in humidity conditions wherein more than 10 g of water per cubic meter of dry conditioning air is present.
摘要:
A method for preparing a composition containing between 0.08 and 3.0% by weight of a polymer or copolymer of a 3,4-dialkoxythiophene in which said two alkoxy groups may be the same or different or together represent a oxy-alkylene-oxy bridge optionally substituted with substituents selected from the group consisting of alkyl, alkoxy, alkyoxyalkyl, carboxy, alkylsulphonato, alkyloxyalkylsulphonato and carboxy ester groups, a polyanion and at least one polyhydroxy non-aqueous solvent from a dispersion of said polymer or copolymer of (3,4-dialkoxythiophene) and said polyanion in water comprising in the following order the steps of: i) mixing at least one of said non-aqueous solvents with said aqueous dispersion of said polymer or copolymer of (3,4-dialkoxythiophene) and said polyanion; and ii) evaporating water from the mixture prepared in step i) until the content of water therein is reduced by at least 65% by weight; a printing ink, printing paste or coating composition, capable of yielding layers with an enhanced transparency at a given surface resistance, prepared according to the above-described method; a coating process with the coating composition thereby producing a layer with enhanced transparency at a given surface resistance; and a printing process with the printing ink or paste thereby producing a layer with enhanced transparency at a given surface resistance.
摘要:
A laminate including a glass layer and a second layer, the glass layer having a pattern of crack lines, dividing the glass layer into pattern elements.