A heterogeneous polymer blend comprises a continuous phase comprising a thermoplastic first polymer having a crystallinity of at least 30% and a dispersed phase comprising particles of a second polymer different from the first polymer dispersed in said continuous phase, the second polymer having a crystallinity of less than 20% and being at least partially cross-linked, and the average particle size of the particles of the second polymer being less than 1 micron.
摘要:
In a process for producing a heterogeneous polymer blend, at least one first monomer is polymerized in a first reaction zone in the presence of a supported catalyst to produce a thermoplastic first polymer having a crystallinity of at least 30%. At least part of said first polymer is then contacted with at least one second monomer and at least one polyene in a second reaction zone under conditions sufficient to polymerize said second monomer to produce a second polymer having a crystallinity of less than 20%. The second polymer is at least partially cross-linked in the second reaction zone such that at least a fraction of the second polymer is insoluble in xylene and such that the first and second polymers form different phases of the blend.
摘要:
A heterogeneous polymer blend comprises a dispersed phase comprising a thermoplastic first polymer having a crystallinity of at least 30% and a continuous phase comprising a second polymer different from the first polymer. The second polymer has a crystallinity of less than 20% and is at least partially cross-linked.
摘要:
A heterogeneous polymer blend comprises a continuous phase comprising a thermoplastic first polymer having a crystallinity of at least 30% and a dispersed phase comprising particles of a second polymer different from the first polymer dispersed in said continuous phase and having an average particle size of less than 5 micron. The second polymer has a crystallinity of less than 20% and is at least partially cross-linked such that no more than about 50 wt % of the second polymer is extractable in cyclohexane at 23° C.
摘要:
A homogeneous polymer blend comprises a thermoplastic first polymer having a crystallinity of at least 30%; and a second polymer having a crystallinity of more than 5% and being at least partially cross-linked.
摘要:
The present invention relates to a process for preparing a thermoplastic vulcanizate (TPV) comprising: contacting a thermoplastic polymer, a cross-linkable elastomer, at least one curative, and at least one cure activator in a solvent to form Composition A. The solvent is then removed, and thereafter the cross-linkable elastomer is at least partially cured. The average particle size of the cross-linkable elastomer is 10 microns or less after the solvent is removed.
摘要:
The present invention relates to a process for preparing a thermoplastic vulcanizate (TPV) comprising: contacting a thermoplastic polymer, a cross-linkable elastomer, at least one curative, and at least one cure activator in a solvent to form Composition A. The solvent is then removed, and thereafter the cross-linkable elastomer is at least partially cured. The average particle size of the cross-linkable elastomer is 10 microns or less after the solvent is removed.
摘要:
The present invention relates to a process for preparing a thermoplastic vulcanizate (TPV) comprising: contacting a thermoplastic polymer, a cross-linkable elastomer, at least one curative, and at least one cure activator in a solvent to form Composition A. The solvent is then removed, and thereafter the cross-linkable elastomer is at least partially cured. The average particle size of the cross-linkable elastomer is 10 microns or less after the solvent is removed.
摘要:
The present invention relates to a process for preparing a thermoplastic vulcanizate (TPV) comprising: contacting a thermoplastic polymer, a cross-linkable elastomer, at least one curative, and at least one cure activator in a solvent to form Composition A. The solvent is then removed, and thereafter the cross-linkable elastomer is at least partially cured. The average particle size of the cross-linkable elastomer is 10 microns or less after the solvent is removed.
摘要:
An illuminable sign (1) including a plate (2) of a light-transmitting material, at least one three-dimensional body, such as a convex strip (7), also of a light-transmitting material, in the form of a symbol, lettering, decoration or the like, and positioned on or over a surface of the plate (2), and a light source (4). The light source (4) is positioned along at least part of an edge (3) of the plate (2), such that, when the light source (4) is switched on, light from the source (4) is coupled into the plate (2). The illuminable sign (1) closely resembles a neon sign.