Abstract:
This invention relates to a polyalpha-olefin (and hydrogenated analogs thereof) comprising more than 50 mole % of one or more C5 to C24 alpha-olefin monomers where the polyalpha-olefin has: a) 40 mole % or more of mm triads, b) a Bromine number of Y or greater, where Y is equal to 89.92*(V)′°5863, where V is the Kinematic Viscosity of the polyalpha-olefin measured at 100° C. in cSt, and c) 1,2 disubstituted olefins present at 7 mole % or more, preferably having Z mole % or more of units represented by the formula: where j, k and m are each, independently, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, or 22, n is an integer from 1 to 350, and where Z=8.420*Log(V)−4.048, where V is the kinematic viscosity of the polyalpha-olefin measured at 1000 C in cSt This invention also relates to process to produce such polyalpha-olefins.
Abstract:
Disclosed herein is an in-reactor produced multi-component copolymer comprises a semi-crystalline component having a crystallinity of 20% or more, and an amorphous component having a crystallinity of 5% or less. The copolymer comprises at least 80 wt % of units derived from propylene and from about 1 to about 20 wt % of units derived from at least one C6 to C12 alpha-olefin. The copolymer has a viscosity at 190° C. of at least 530 mPa sec and a heat of fusion between about 10 and about 70 J/g. An adhesive containing the copolymer exhibits a good balance of adhesive properties and mechanical strength.
Abstract:
Provided are catalyst systems, processes for polymerizing one or more olefins, polymers resulting therefrom, and articles prepared from such polymers. The processes comprise contacting under polymerization conditions one or more olefin monomers, preferably propylene, with a catalyst system comprising a transition metal compound and an activator of the formula (1) or (2) as described herein. The polymer compositions described herein exhibit advantageously narrow composition distributions and high melting points in comparison to conventional polymers having the same comonomer content. The polymers described herein exhibit improved properties, e.g., pellet stability, impact properties, heat seal properties, and structural integrity in film and fabricated parts applications.
Abstract:
The present invention describes polymer comprising one or more C3 to C40 olefins and having a Mw of 100,000 or less and a Dot T-Peel of 1 Newton or more. The polymer may have a branching index (g′) of 0.95 or less measured at the Mz of the polymer, and a heat of fusion of 1 to 70 J/g. Also described are polymers of homopolypropylene or a copolymer of propylene and up to 5 mole % ethylene having: an isotactic run length of 1 to 30 as determined by Carbon 13 NMR and a percent of r dyad of greater than 20%, preferably from 20 to 70% as determined by Carbon 13 NMR. Also described are methods of making these and other polymers.
Abstract:
This invention relates to a blend composition comprising: 1) a linear ethylene containing polymer, such as a LLDPE, a HDPE or the like; and at least 1 weight percent of an in-reactor polymer blend comprising: (a) a first ethylene containing polymer having a density of greater than 0.90 g/cm3 and a Mw of more than 20,000 g/mol; and (b) a second ethylene containing polymer having a density of less than 0.90 g/cm3, wherein the polymer blend has a Tm of at least 90° C. (DSC second melt), a density of less than 0.92 g/cm3, and the densities of the first and second polymers differ by at least 1%.
Abstract translation:本发明涉及一种共混组合物,其包含:1)含线性乙烯的聚合物,例如LLDPE,HDPE等; 和至少1重量%的反应器内聚合物共混物,其包含:(a)密度大于0.90g / cm 3和Mw大于20,000g / mol的第一含乙烯聚合物; 和(b)密度小于0.90g / cm 3的第二含乙烯聚合物,其中聚合物共混物具有至少90℃的Tm(DSC第二熔体),小于0.92g / cm 3的密度, 并且第一和第二聚合物的密度相差至少1%。
Abstract:
This invention relates to an in-reactor polymer blend comprising: (a) a first ethylene-containing polymer having a density of greater than 0.90 g/cm3 and a Mw of more than 20,000 g/mol and (b) a second ethylene-containing polymer having a density of less than 0.90 g/cm3 wherein the polymer blend has a Tm of at least 90° C. (DSC second melt), a density of less than 0.92 g/cm3, and the densities of the first and second polymers differ by at least 1%.
Abstract translation:本发明涉及一种反应器内聚合物共混物,其包含:(a)密度大于0.90g / cm 3,Mw大于20,000g / mol的第一含乙烯聚合物和(b)第二含乙烯的聚合物 聚合物的密度小于0.90g / cm 3,其中聚合物共混物具有至少90℃的Tm(DSC第二熔体),小于0.92g / cm 3的密度和第一和第二聚合物的密度 至少1%不等。
Abstract:
This invention relates to in-reactor polymer blends comprising at least 60 mole % of propylene and from 0.01 to 10 mole % of at least one diene selected from the group of C6 to C12 α,ω-diene, norbornadiene, vinyl norbornene and mixtures thereof with the balance being ethylene. The blend comprises first and second polymers having different crystallinities and or different Tg's.
Abstract:
This invention relates to a process for polymerization, comprising (i) contacting, at a temperature greater than 35° C., one or more monomers comprising ethylene and/or propylene, with a catalyst system comprising a metallocene catalyst compound and an activator, (ii) converting at least 50 mol % of the monomer to polyolefin; and (iii) obtaining a branched polyolefin having greater than 50% allyl chain ends, relative to total unsaturated chain ends. The invention also relates to the branched polyolefins and functionalized branched polyolefins.
Abstract:
A low viscosity poly(alpha-olefin) (PAO) is produced by contacting one or more C3 to C24 alpha-olefins with an unbridged, substituted bis-cyclopentadienyl transition metal compound, a non-coordinating anion activator, and an alkyl-aluminum compound. The molar ratio of transition metal compound to activator is 10:1 to 0.1:1 and the molar ratio of alkyl aluminum compound to transition metal compound is 1:4 to 4000:1. The transition metal compound has either (a) at least one non-isoolefin substitution on both cyclopentadienyl rings, or (b) at least two substitutions on at least one cyclopentadienyl ring. The PAO is comprised of at least 50 mole % of C3 to C24 alpha-olefins, has a Mw/Mn between 1 and 1.4, and a kinematic viscosity at 100° C. of 20 cSt or less.
Abstract:
A heat-shrinkable film. The film comprising at least one layer having at least one propylene-based polymer comprising 60 wt % to 98 wt % propylene derived units and 2 wt % to 40 wt % one or more other alpha olefins, the propylene-based polymer having: a triad tacticity of 70% or more, a heat of fusion of less than 80 J/g, a weight average molecular weight (Mw) as measured by GPC of from 70,000 to 250,000. The layer also comprises at least one thermoplastic resin and at least one hydrocarbon resin.