公开(公告)号:US20150232363A1
公开(公告)日:2015-08-20
申请号:US14434572
申请日:2013-10-11
CPC分类号: C03B5/28 , C03B3/00 , C03B5/12 , C03B5/235 , C03B5/2353 , C03B5/2356 , C03B2211/23 , F23C3/004 , F23C3/006
摘要: A melt for use in the production of man-made vitreous fibres may be formed in a circulating combustion chamber (20) by melting particulate material. The material is collected in a base region of the combustion chamber (26), where it can be heated using submerged combustion apparatus (40). The submerged combustion process is controlled to ensure that the proportion of Fe(2+) based on total Fe within the melt extracted from an outlet of the chamber is greater than 80%.
摘要翻译: 用于生产人造玻璃纤维的熔体可以通过熔化颗粒材料在循环燃烧室(20)中形成。 所述材料被收集在所述燃烧室(26)的基部区域中,其中可以使用浸没式燃烧装置(40)进行加热。 控制浸没燃烧过程以确保从室的出口提取的熔体内的基于总Fe的Fe(2+)的比例大于80%。
-
公开(公告)号:US20150274578A1
公开(公告)日:2015-10-01
申请号:US14434549
申请日:2013-10-11
CPC分类号: C03B37/041 , C03B3/026 , C03B5/0275 , C03B5/12 , C03B5/185 , C03B5/2353 , C03B5/2356 , C03B5/265 , C03B5/28 , C03B37/05 , C03B37/055 , C03B2211/22 , C03B2211/23 , C03B2211/25 , C03B2211/40 , Y02P40/55
摘要: A melt for use in the production of man-made vitreous fibres may be formed in a circulating combustion chamber (20) by melting particulate material. The material is collected in a base region (26) of the combustion chamber, where it can be heated using submerged heating means (40). The submerged heating increases the homogeneity of the melt within the melt pool (30), the increase in homogeneity being encouraged by a relatively long average residence time for mineral material in the chamber (20) of at least 15 minutes.
摘要翻译: 用于生产人造玻璃纤维的熔体可以通过熔化颗粒材料在循环燃烧室(20)中形成。 该材料被收集在燃烧室的基部区域(26)中,其中可以使用浸没式加热装置(40)进行加热。 浸没加热增加了熔池(30)内的熔体的均匀性,同时促进均匀性的增加,使得室(20)中的矿物材料的平均停留时间相对长达至少15分钟。
-
公开(公告)号:US20150225274A1
公开(公告)日:2015-08-13
申请号:US14434561
申请日:2013-10-11
CPC分类号: C03B5/183 , C03B5/027 , C03B5/12 , C03B5/185 , C03B5/2353 , C03B5/2356 , C03B5/28 , C03B37/04 , Y02P40/55
摘要: A melt for use in the production of man-made vitreous fibres may be formed in a circulating combustion chamber (20) by melting particulate material. The material is collected in a base region of the combustion chamber (26), where it can be heated using submerged heating means (40). The submerged heating increases the homogeneity of the melt within the melt pool (30), the coherence of which is maintained by the use of a siphon (50) to extract melt from the combustion chamber.
摘要翻译: 用于生产人造玻璃纤维的熔体可以通过熔化颗粒材料在循环燃烧室(20)中形成。 该材料被收集在燃烧室(26)的基部区域中,在该区域中可以使用浸没式加热装置(40)进行加热。 浸没式加热增加了熔池(30)内的熔体的均匀性,通过使用虹吸(50)从燃烧室提取熔体来维持熔融物的相干性。
-
公开(公告)号:US20140228195A1
公开(公告)日:2014-08-14
申请号:US14122911
申请日:2012-10-12
摘要: The invention relates to a melt composition for the production of man-made vitreous fibres and man-made vitreous fibres comprising the following oxides, by weight of composition: SiO239-43 weight % Al2O320-23 weight % TiO2up to 1.5 weight % Fe2O35-9 weight %, preferably 5-8 weight % CaO8-18 weight % MgO5-7 weight % Na2Oup to 10 weight %, preferably 2-7 weight % K2Oup to 10 weight %, preferably 3-7 weight % P2O5up to 2% MnOup to 2% R2Oup to 10 weight % wherein the proportion of Fe(2+) is greater than 80% based on total Fe and is preferably at least 90%, more preferably at least 95% and most preferably at least 97% based on total Fe.
摘要翻译: 本发明涉及用于生产人造玻璃纤维和人造玻璃纤维的熔体组合物,其包含以下组成的以下氧化物:SiO 2 39-43重量%Al 2 O 3 20-23重量%TiO 2,至多1.5重量% Fe2O3 5-9重量%,优选5-8重量%CaO 8-18重量%MgO 5-7重量%Na 2 O至多10重量%,优选2-7重量%K 2 O至10重量%,优选3-7重量% %P 2 O 5至多2%MnO至高达2%R 2 O至10重量%,其中Fe(2+)的比例基于总Fe大于80%,优选至少90%,更优选至少95%,更优选至少95% 最优选至少97%,基于总Fe。
-
-
-