Provided are ethylene propylene copolymers compositions thereof and methods for making the same. The composition may include an ethylene copolymer, comprising 40 wt % to 70 wt % of units derived from ethylene, and at least 30 wt % of units derived from at least one α-olefin having 3 to 20 carbon atoms. The composition can have a melting point (Tm) in ° C., as measured by DSC, that satisfies the relation: Tm>3.4×E−180, where E is the weight % of units derived from ethylene in the copolymer. The composition can also have a Mw/Mn ratio of about 1.5 to about 3.5. The composition can further have a content of Group 4 metals derived from a catalyst of 25 ppm or less.
摘要:
Provided are ethylene propylene copolymers compositions thereof and methods for making the same. The composition may include an ethylene copolymer, comprising 40 wt % to 70 wt % of units derived from ethylene, and at least 30 wt % of units derived from at least one α-olefin having 3 to 20 carbon atoms. The composition can have a melting point (Tm) in ° C., as measured by DSC, that satisfies the relation: Tm>3.4×E−180, where E is the weight % of units derived from ethylene in the copolymer. The composition can also have a Mw/Mn ratio of about 1.5 to about 3.5. The composition can further have a content of Group 4 metals derived from a catalyst of 25 ppm or less.
摘要:
Provided are amorphous ethylene propylene copolymer, compositions thereof, and methods for making same, whereby the copolymer can include of from about 40 wt. % to about 60 wt. % ethylene derived units; and of from about 60 wt. % to about 40 wt. % propylene derived units. The copolymer can be characterized by having no discernable melting point as measured by DSC, an MFRR (MI (21.6 kg; 230° C.)/MI (2.16 kg; 230° C.)) (MI (2.16 kg; 230° C.)) of about 38 or more, a molecular weight distribution (MWD) of from about 1.5 to about 2.5, and a shear viscosity η* at 0.01 rad/sec measured at 70° C. that satisfies the relation |η*|(70° C.; 0.01 rad/sec)>1.2*106*|MFR|−0.77, wherein MFR is the melt flow rate.
摘要:
Disclosed are rheology modifiers comprising compositionally disperse polymeric compositions and/or crystallinity disperse polymeric compositions that may be useful in modifying the rheological properties of lubrication fluids, and methods for making such compositions. The compositionally disperse polymeric composition are formed from at least two discrete compositions of ethylene copolymers. The crystallinity disperse polymeric composition are formed from ethylene copolymers having at least two discrete values of residual crystallinity.
摘要:
Provided are ethylene-based copolymers, methods of preparing the same, lubricating oil compositions including the same, methods for preparing such lubricating oil compositions, and end uses for such ethylene-based copolymers and lubricating oil compositions. The ethylene-based copolymers may include less than about 80 wt. % of units derived from ethylene and one or more alpha-olefin comonomers having 3 to 20 carbon atoms. The ethylene-based copolymers have a melting peak (Tm), as measured by DSC, of 80° C. or less, and a polydispersity index of about 2.8 or less. In some embodiments, the ethylene-based copolymers have an intramolecular composition distribution of about 50 wt. % or less and/or an intermolecular composition distribution of about 50 wt. % or less.
摘要:
Provided are ethylene-based copolymers, methods of preparing the same, lubricating oil compositions including the same, methods for preparing such lubricating oil compositions, and end uses for such ethylene-based copolymers and lubricating oil compositions. The ethylene-based copolymers may include less than about 80 wt. % of units derived from ethylene and one or more alpha-olefin comonomers having 3 to 20 carbon atoms. The ethylene-based copolymers have a melting peak (Tm), as measured by DSC, of 80° C. or less, and a polydispersity index of about 2.8 or less. In some embodiments, the ethylene-based copolymers have an intramolecular composition distribution of about 50 wt. % or less and/or an intermolecular composition distribution of about 50 wt. % or less.
摘要:
Disclosed are rheology modifiers comprising compositionally disperse polymeric compositions and/or crystallinity disperse polymeric compositions that may be useful in modifying the rheological properties of lubrication fluids, and methods for making such compositions. The compositionally disperse polymeric composition are formed from at least two discrete compositions of ethylene copolymers. The crystallinity disperse polymeric composition are formed from ethylene copolymers having at least two discrete values of residual crystallinity.
摘要:
Polymeric compositions and methods for making and using the same are provided. The polymeric composition can include a first ethylene-based copolymer and a second ethylene-based copolymer. The first ethylene-based copolymer can have a weight percent of ethylene-derived units based on a weight of the polymeric composition (EA) ranging from about 35 wt % to about 52 wt % and a weight-average molecular weight (MwA) of less than or equal to 130,000. The second ethylene-based copolymer can have a weight percent of ethylene-derived units based on the weight of the polymeric composition (EB) ranging from about 65 wt % to about 85 wt % and a weight-average molecular weight (MwB) of less than 130,000.
摘要:
Polymeric compositions and methods for making and using the same are provided. The polymeric composition can include a first ethylene-based copolymer and a second ethylene-based copolymer. The first ethylene-based copolymer can have a weight percent of ethylene-derived units based on a weight of the polymeric composition (EA) ranging from about 35 wt % to about 52 wt % and a weight-average molecular weight (MwA) of less than or equal to 130,000. The second ethylene-based copolymer can have a weight percent of ethylene-derived units based on the weight of the polymeric composition (EB) ranging from about 65 wt % to about 85 wt % and a weight-average molecular weight (MwB) of less than 130,000.
摘要:
Provided are amorphous ethylene propylene copolymer, compositions thereof, and methods for making same, whereby the copolymer can include of from about 40 wt. % to about 60 wt. % ethylene derived units; and of from about 60 wt. % to about 40 wt. % propylene derived units. The copolymer can be characterized by having no discernable melting point as measured by DSC, an MFRR (MI (2.16 kg; 230° C.)/MI 21.6 kg; 230° C.) of about 38 or more, a molecular weight distribution (MWD) of from about 1.5 to about 2.5, and a shear viscosity η* at 0.01 rad/sec measured at 70° C. that satisfies the relation |η*|(70° C.; 0.01 rad/sec)>1.2*106*|MFR|−0.77, wherein MFR is the melt flow rate and η* is the complex viscosity at 0.01 rad/sec measured at 70° C.