Magnetic recording medium and method for manufacturing the same
    3.
    发明申请
    Magnetic recording medium and method for manufacturing the same 失效
    磁记录介质及其制造方法

    公开(公告)号:US20080070066A1

    公开(公告)日:2008-03-20

    申请号:US11898757

    申请日:2007-09-14

    IPC分类号: G11B5/842 B05D5/12

    CPC分类号: G11B5/842

    摘要: A method for manufacturing a magnetic recording medium of the present invention includes a magnetic layer forming step in which a drying process is performed. The drying process includes: a pre-heating stage in which a magnetic coating film is heated until the surface temperature of the magnetic coating film stops rising and reaches a substantially constant temperature; a constant rate drying stage that is performed after the pre-heating stage in which the surface temperature of the magnetic coating film is held substantially constant; and a falling rate drying stage that is performed after the constant rate drying stage in which the surface temperature of the magnetic coating film is increased to be higher than the surface temperature during the constant rate drying stage to harden the magnetic coating film. The constant rate drying period in which the constant rate drying stage is performed is 0.2 seconds or more. The first solvent is made of one solvent or two or more solvents having different boiling points, and the difference (Tb−Ts) between the boiling point Tb of the solvent having the lowest boiling point among the solvents contained in the first solvent and the surface temperature Ts of the magnetic coating film during the constant rate drying period is 1 to 50° C.

    摘要翻译: 本发明的磁记录介质的制造方法包括进行干燥处理的磁性层形成工序。 干燥过程包括:预热阶段,其中加热磁性涂膜直到磁性涂膜的表面温度停止上升并达到基本恒定的温度; 在预热阶段之后进行恒定速率干燥阶段,其中磁性涂膜的表面温度保持在大致恒定的范围; 以及在恒速干燥阶段之后,在恒速干燥阶段使磁性涂膜的表面温度升高到高于表面温度的固定速率干燥阶段之后进行硬化处理的落下率干燥阶段。 进行恒定速率干燥阶段的恒定速率干燥时间为0.2秒以上。 第一溶剂由一种溶剂或两种或更多种沸点不同的溶剂制成,沸点T < 在恒定速率干燥期间,第一溶剂中所含溶剂中具有最低沸点的溶剂的b b和磁性涂膜的表面温度T S 1 / S 2为1〜50℃ C。

    Magnetic recording medium and method for producing the same
    4.
    发明申请
    Magnetic recording medium and method for producing the same 审中-公开
    磁记录介质及其制造方法

    公开(公告)号:US20050170214A1

    公开(公告)日:2005-08-04

    申请号:US10995314

    申请日:2004-11-24

    IPC分类号: G11B5/72 G11B5/84 G11B5/68

    CPC分类号: G11B5/8408 G11B5/72

    摘要: There is provided a magnetic recording medium comprising a flexible non-magnetic substrate, and a magnetic layer containing magnetic particles, formed on at least one surface of the flexible non-magnetic substrate, and this magnetic recording medium is characterized in that an uppermost layer formed on the side of the magnetic layer is a non-magnetic layer with a thickness of 1 to 50 nm, which contains a resin and has a surface roughness (P-V) of 2 to 20 nm. This magnetic recording medium is excellent in high density recording performance, and is highly reliable in durability.

    摘要翻译: 提供了一种磁性记录介质,其包括柔性非磁性基板和形成在柔性非磁性基板的至少一个表面上的含有磁性颗粒的磁性层,该磁性记录介质的特征在于形成了最上层 在磁性层的一侧是厚度为1〜50nm的非磁性层,其含有树脂,表面粗糙度(PV)为2〜20nm。 该磁记录介质具有优异的高密度记录性能,并且耐久性高度可靠。

    Magnetic tape
    5.
    发明申请
    Magnetic tape 审中-公开
    磁带

    公开(公告)号:US20060068232A1

    公开(公告)日:2006-03-30

    申请号:US10948259

    申请日:2004-09-24

    IPC分类号: G11B5/708

    摘要: A magnetic tape comprising a non-magnetic substrate and at least one magnetic layer formed on one surface of the non-magnetic substrate, characterized in that magnetic particles contained in an uppermost magnetic layer of the magnetic layer are substantially granular particles with a particle size of 30 nm or less, and that the ratio of a coercive force HcM in the machine direction to a coercive force HcT in the transverse direction, i.e., [HcM/HcT], is at least 2.2. This magnetic tape has a capacity capable of corresponding to mass storage of 1 TB or more, and achieves a high ratio of reproducing output to noises (C/N), particularly for signals within a short wavelength range, thus showing excellent high-density recording performance.

    摘要翻译: 一种磁带,其包含非磁性基底和形成在所述非磁性基底的一个表面上的至少一个磁性层,其特征在于,所述磁性层的最上层的磁性层中所含的磁性粒子是粒径为 30nm以下,并且矫顽力Hc在机械方向上的相对于横向的矫顽力Hc T 的比例,即[Hc M>至少为2.2。 该磁带具有能够对应于1TB以上的大容量存储容量的能力,并且实现了对于噪声(C / N)的再现输出的高比率,特别是对于短波长范围内的信号,因此显示出优异的高密度记录 性能。

    Magnetic recording medium and method for manufacturing the same
    6.
    发明授权
    Magnetic recording medium and method for manufacturing the same 失效
    磁记录介质及其制造方法

    公开(公告)号:US08613977B2

    公开(公告)日:2013-12-24

    申请号:US11898757

    申请日:2007-09-14

    IPC分类号: B05D5/12

    CPC分类号: G11B5/842

    摘要: A method for manufacturing a magnetic recording medium of the present invention includes a magnetic layer forming step in which a drying process is performed. The drying process includes: a pre-heating stage in which a magnetic coating film is heated until the surface temperature of the magnetic coating film stops rising and reaches a substantially constant temperature; a constant rate drying stage that is performed after the pre-heating stage in which the surface temperature of the magnetic coating film is held substantially constant; and a falling rate drying stage that is performed after the constant rate drying stage in which the surface temperature of the magnetic coating film is increased to be higher than the surface temperature during the constant rate drying stage to harden the magnetic coating film. The constant rate drying period in which the constant rate drying stage is performed is 0.2 seconds or more. The first solvent is made of one solvent or two or more solvents having different boiling points, and the difference (Tb−Ts) between the boiling point Tb of the solvent having the lowest boiling point among the solvents contained in the first solvent and the surface temperature Ts of the magnetic coating film during the constant rate drying period is 1 to 50° C.

    摘要翻译: 本发明的磁记录介质的制造方法包括进行干燥处理的磁性层形成工序。 干燥过程包括:预热阶段,其中加热磁性涂膜直到磁性涂膜的表面温度停止上升并达到基本恒定的温度; 在预热阶段之后进行恒定速率干燥阶段,其中磁性涂膜的表面温度保持在大致恒定的范围; 以及在恒速干燥阶段之后,在恒速干燥阶段使磁性涂膜的表面温度升高到高于表面温度的固定速率干燥阶段之后进行硬化处理的落下率干燥阶段。 进行恒定速率干燥阶段的恒定速率干燥时间为0.2秒以上。 第一溶剂由一种溶剂或两种或更多种具有不同沸点的溶剂制成,并且在第一溶剂中包含的溶剂中具有最低沸点的溶剂的沸点Tb与表面之间的差(Tb-Ts) 恒速干燥期间的磁性涂膜的温度Ts为1〜50℃。