Abstract:
The disclosure relates to a process that includes blending a polyimide resin and a primary alky amine organic compound to produce an aryl amine functionalized polyimide, having aryl amine functionality in excess of any anhydride functionality. The polyimide resin can have a weight average molecular weight (Mw) from 5,000 to 100,000 daltons. The organic compound can include at least one primary aliphatic amine without a direct linkage of a nitrogen to an aryl group and without a functionality selected from a halogen functionality, a hydroxyl functionality, a sulfonic acid functionality, a sulfonic acid salt functionality, and combinations thereof. The disclosure also relates to alkyl imide functionalized polyimides also with aryl amine functionalized polyimides, having aryl amine functionality in excess of any anhydride functionality and articles produced therefrom.
Abstract:
The disclosure relates to a process that includes blending a polyimide resin and a primary alky amine organic compound to produce an aryl amine functionalized polyimide, having aryl amine functionality in excess of any anhydride functionality. The polyimide resin can have a weight average molecular weight (Mw) from 5,000 to 100,000 daltons. The organic compound can include at least one primary aliphatic amine without a direct linkage of a nitrogen to an aryl group and without a functionality selected from a halogen functionality, a hydroxyl functionality, a sulfonic acid functionality, a sulfonic acid salt functionality, and combinations thereof. The disclosure also relates to alkyl imide functionalized polyimides also with aryl amine functionalized polyimides, having aryl amine functionality in excess of any anhydride functionality and articles produced therefrom.
Abstract:
The invention is directed to a process for preparing a linear or branched amine-modified thermoplastic resin with high flowability using as starting materials a linear or branched polyester and a primary or secondary aliphatic amine. The process does not require that the amine and polyester be combined in a liquid organic solvent during the process, and can be performed readily at ambient pressure. The amine-modified resins can be extruded and pelletized using normal operating conditions, making this process a versatile option for achieving a wide variety of viscosities in a simple, low cost, continuous operation.