公开(公告)号:US20240247132A1
公开(公告)日:2024-07-25
申请号:US18419640
申请日:2024-01-23
Applicant: SEIKO EPSON CORPORATION
Inventor: Tomohiro FUJITA , Takashi HIRAIWA , Shinobu YOKOKAWA , Hirofumi HOKARI
IPC: C08L1/02
CPC classification number: C08L1/02 , C08L2205/02
Abstract: A molding material contains cellulose fibers, aliphatic polyester, and esterified cellulose, and the amount of the cellulose fibers is 50% to 80% by mass. The amount of the esterified cellulose in the molding material may be 48 to 25% by mass. The amount of the aliphatic polyester, XP mass %, and the amount of the esterified polyester, XE mass %, may satisfy 1.0≤XP/XE≤54.0.
-
公开(公告)号:US20230226782A1
公开(公告)日:2023-07-20
申请号:US18153385
申请日:2023-01-12
Applicant: SEIKO EPSON CORPORATION
Inventor: Makoto YOSHIDA , Shinobu YOKOKAWA , Tomohiro FUJITA
CPC classification number: B29C70/504 , B29C70/12 , B29K2201/00
Abstract: A molded-material manufacturing apparatus includes a deposition section configured to deposit a material containing fibers in air to form a web, a first heating section of a noncontact type configured to heat the web, and a second heating section of a contact type configured to heat and pressurize the web heated in the first heating section to form a molded material.
-
公开(公告)号:US20240262996A1
公开(公告)日:2024-08-08
申请号:US18427917
申请日:2024-01-31
Applicant: SEIKO EPSON CORPORATION
Inventor: Tomohiro FUJITA , Masaaki AOTA , Takashi HIRAIWA
IPC: C08L23/12
CPC classification number: C08L23/12 , C08L2205/16
Abstract: A molding material of the present disclosure includes cellulose fibers, a binder, and urethane fibers. The content of the cellulose fibers in the molding material of the present disclosure is preferably 2% by mass or more and 40% by mass or less. The average length of the cellulose fibers is preferably less than 3 mm. The content of the binder in the molding material of the present disclosure is preferably 35% by mass or more and 94% by mass or less. The content of the urethane fibers in the molding material of the present disclosure is preferably 2% by mass or more and 40% by mass or less.
-
公开(公告)号:US20240101792A1
公开(公告)日:2024-03-28
申请号:US18473335
申请日:2023-09-25
Applicant: SEIKO EPSON CORPORATION
Inventor: Tomohiro FUJITA , Shinobu YOKOKAWA , Chieko NAKAJIMA
IPC: C08L1/02
CPC classification number: C08L1/02 , C08L2201/02 , C08L2201/06 , C08L2205/025 , C08L2205/03 , C08L2205/16
Abstract: A molding material is a molding material including linear alkyl-based polyester, highly polar polyester, and cellulose fibers, in which a content of the linear alkyl-based polyester is greater than a content of the highly polar polyester, and a total content of the linear alkyl-based polyester and the highly polar polyester is less than or equal to a content of the cellulose fibers.
-
公开(公告)号:US20250002713A1
公开(公告)日:2025-01-02
申请号:US18757700
申请日:2024-06-28
Applicant: SEIKO EPSON CORPORATION
Inventor: Tomohiro FUJITA , Takashi HIRAIWA , Chieko NAKAJIMA , Kiyoaki SAKAGUCHI
IPC: C08L67/04 , C08K5/53 , C08K5/5399 , C08L1/02
Abstract: A molding material according to one embodiment of the present disclosure is a molding material containing cellulose fibers and a resin, and the resin includes a saturated aliphatic polyester and a highly polar polyester. In a molecular weight distribution curve by a GPC method, the resin has a maximum value 2 at a weight average molecular weight of 100,000 or more and a maximum value 1 at a weight average molecular weight less than that at the maximum value 2, and an area value in the maximum value 2 is smaller than an area value in the maximum value 1.
-
公开(公告)号:US20240199856A1
公开(公告)日:2024-06-20
申请号:US18545064
申请日:2023-12-19
Applicant: SEIKO EPSON CORPORATION
Inventor: Tomohiro FUJITA , Shinobu YOKOKAWA , Chieko NAKAJIMA , Kiyoaki SAKAGUCHI
IPC: C08L1/02
CPC classification number: C08L1/02 , C08L2205/03 , C08L2205/16
Abstract: A molding material contains a polyester-based elastomer, a highly polar polyester, and cellulose fibers, a content of the polyester-based elastomer with respect to a content of the highly polar polyester is 25 percent by mass or more, and a total content of the polyester-based elastomer and the highly polar polyester is equal to or lower than a content of the cellulose fibers.
-
公开(公告)号:US20240101813A1
公开(公告)日:2024-03-28
申请号:US18473339
申请日:2023-09-25
Applicant: SEIKO EPSON CORPORATION
Inventor: Tomohiro FUJITA , Shinobu YOKOKAWA , Chieko NAKAJIMA
CPC classification number: C08L67/02 , B29C45/0001 , C08K5/5399 , C08K7/02 , C08L1/02 , C08L67/04 , B29K2067/046 , C08K2201/004 , C08L2201/02 , C08L2203/30 , C08L2205/025
Abstract: A molding material is a molding material including linear alkyl-based polyester, highly polar polyester, cellulose fibers, and a flame retardant, in which a total content of the linear alkyl-based polyester and the highly polar polyester is less than or equal to a content of the cellulose fibers, the flame retardant has a phosphazene skeleton or a phosphoric acid ester skeleton in a molecular structure, and a content of the flame retardant is 1% by mass or greater and 10% by mass or less with respect to the total content of the linear alkyl-based polyester, the highly polar polyester, and the cellulose fibers.
-
公开(公告)号:US20180094153A1
公开(公告)日:2018-04-05
申请号:US15714075
申请日:2017-09-25
Applicant: Seiko Epson Corporation
Inventor: Tomohiro FUJITA , Chikako FUJITA , Kana OZAKI , Yoshifumi ITO
IPC: C09D11/328 , C09D11/40 , C09B67/46 , C09B3/60 , C07C317/14
CPC classification number: C09D11/328 , C07C317/14 , C09B3/60 , C09B67/0084 , C09D11/38 , C09D11/40
Abstract: An ink jet ink composition contains a disperse dye, and a compound represented by the following formula (1): In the formula, Ar1 and Ar2 each independently represent an aryl group; R1 and R2 each independently represent a chemical species selected from the group consisting of hydrogen, alkyl groups having a carbon number of 1 to 3, a sulfo group, —O—SO3H, a carboxy group, and a hydroxy group; and n's each independently represent an integer of 0 to 5.
-
公开(公告)号:US20250002712A1
公开(公告)日:2025-01-02
申请号:US18756155
申请日:2024-06-27
Applicant: SEIKO EPSON CORPORATION
Inventor: Tomohiro FUJITA , Takashi HIRAIWA , Chieko NAKAJIMA , Kiyoaki SAKAGUCHI
Abstract: A molding material according to one embodiment of the present disclosure contains cellulose fibers and a resin, and the resin includes a polyester-based elastomer and a highly polar polyester. In a molecular weight distribution curve by a GPC method, the resin has a maximum value 2 at a weight average molecular weight of 100,000 or more and a maximum value 1 at a weight average molecular weight less than that at the maximum value 2, and an area value in the maximum value 2 is smaller than an area value in the maximum value 1.
-
公开(公告)号:US20250002686A1
公开(公告)日:2025-01-02
申请号:US18757770
申请日:2024-06-28
Applicant: SEIKO EPSON CORPORATION
Inventor: Tomohiro FUJITA , Masaaki AOTA , Takashi HIRAIWA
IPC: C08K7/02
Abstract: A material for molding according to an embodiment of the present disclosure is a material for molding containing cellulose fibers and a resin. The resin contains a binder and urethane fibers. The resin has a maximum 1 at a weight average molecular weight of 50,000 to 150,000 and a maximum 2 at a weight average molecular weight of 75,000 to 300,000 in a molecular weight distribution curve by a GPC method with chloroform as an eluate. An area value at the maximum 2 is smaller than an area value at the maximum 1.
-
-
-
-
-
-
-
-
-