公开(公告)号:US12098263B1
公开(公告)日:2024-09-24
申请号:US18393580
申请日:2023-12-21
申请人: SICHUAN UNIVERSITY
发明人: Junwen Ren , Zi Wang , Shenli Jia , Lihua Zhao , Huachao Wei , Chao Bian , Guoqing Jiang , Ruichi Zeng
CPC分类号: C08K9/10 , C09C1/407 , C09C3/006 , C08K2201/005
摘要: A composite insulating material based on dielectrophoretic force orientation and its preparation method are provided. The method includes: S1, preparing dielectric composite microspheres with a dielectric epoxy resin as a core and a hexagonal boron nitride sheet as a shell; S2, dispersing the hexagonal boron nitride sheet and the dielectric composite microspheres in an organic solvent to obtain a dispersion liquid, and adding an epoxy resin, an epoxy resin curing agent, and an epoxy resin accelerator to the dispersing liquid, and evaporating the organic solvent to obtain a composite substrate; S3, pouring the composite substrate into a container, wherein an upper surface and a lower surface of the container are connected with electrodes, respectively, transferring the container to a vacuum oven, and connecting a power supply of the container to adjust a voltage amplitude and a frequency of the electrodes, conducting dielectrophoretic force orientation on the dielectric composite microspheres in the composite substrate, so as to cause the dielectric composite microspheres to arrange along a direction of electric field; S4, increasing a temperature of the container to cure the composite substrate, cutting off the power supply to the container after curing, and obtaining the composite insulating material.
-
2.
公开(公告)号:US12065607B1
公开(公告)日:2024-08-20
申请号:US18395733
申请日:2023-12-25
申请人: SICHUAN UNIVERSITY
发明人: Junwen Ren , Zi Wang , Shenli Jia , Lihua Zhao , Huachao Wei , Lichuan Jia , Guoqing Jiang , Ruichi Zeng
IPC分类号: C09K5/14 , C08J3/205 , C08K3/38 , C08K9/02 , C08K9/04 , C09C3/00 , C09C3/04 , C09C3/08 , C09K9/00
CPC分类号: C09K5/14 , C08J3/2056 , C08K9/02 , C08K9/04 , C09C3/006 , C09C3/048 , C09C3/08 , C09K9/00 , C01P2004/03 , C01P2004/24 , C01P2006/32 , C08J2383/04 , C08K2003/385 , C08K2201/001 , C08K2201/011
摘要: A silicone rubber composite heat dissipation pad and a preparation method thereof are provided. The method includes: dispersing hydroxyl-functionalized boron nitride nanosheet powder into deionized water, pouring it into a specialized container, pre-freezing it using liquid nitrogen, and then freeze-drying it to obtain a boron nitride nanosheet skeleton arranged in a horizontal direction; uniformly dispersing thermochromic nanoparticles in acetone to obtain a dispersion, mixing the dispersion with liquid silicone rubber and stirring until acetone is completely evaporated, then adding a curing agent to obtain a liquid silicone rubber pre-cure solution; pouring the liquid silicone rubber pre-cure solution into a container containing the boron nitride nanosheet skeleton, so that the liquid silicone rubber pre-cure solution is fully immersed in an interior of the boron nitride nanosheet skeleton; and then curing is carried out by elevating the temperature to obtain the heat dissipation pad.
-