公开(公告)号:US08183168B2
公开(公告)日:2012-05-22
申请号:US12138062
申请日:2008-06-12
摘要: A lead-free glass for covering electrodes including, as represented by mass % based on the following oxides, from 30 to 50% of B2O3, from 21 to 25% of SiO2, from 10 to 35% of ZnO, from 7 to 14% in total of K2O and either one or both of Li2O and Na2O, from 0 to 10% of Al2O3, and from 0 to 10% of ZrO2, wherein when it contains at least one component selected from the group consisting of MgO, CaO, SrO and BaO, the total of their contents is at most 5%, and when the molar fractions of Li2O, Na2O and K2O are represented by l, n and k, respectively, l is at most 0.025, and l+n+k is from 0.07 to 0.17.
摘要翻译: 一种用于覆盖电极的无铅玻璃,包括以下列氧化物的质量%表示:B2O3的30-50%,SiO2的21-25%,ZnO的10-35%,7-14% K 2 O和Li 2 O和Na 2 O中的一种或两者,0至10%的Al 2 O 3和0至10%的ZrO 2,其中当其含有至少一种选自MgO,CaO,SrO 和BaO,其总含量最多为5%,当Li 2 O,Na 2 O和K 2 O的摩尔分数分别由l,n和k表示时,l最多为0.025,l + n + k来自 0.07〜0.17。
-
公开(公告)号:US20090017196A1
公开(公告)日:2009-01-15
申请号:US12138062
申请日:2008-06-12
摘要: To provide a process for producing an electrode-formed glass substrate, which increases the strength of a front substrate of a plasma display device.Electrodes formed on a glass substrate are covered with a lead-free glass comprising, as represented by mass %, from 30 to 50% of B2O3, from 21 to 25% of SiO2, from 10 to 35% of ZnO, from 7 to 14% in total of K2O and either one or both of Li2O and Na2O, from 0 to 10% of Al2O3, from 0 to 10% of ZrO2, and from 0 to 5% of MgO+CaO+SrO+BaO, and when the molar fractions of Li2O, Na2O and K2O are represented by l, n and k, respectively, l is at most 0.025, and l+n+k is from 0.07 to 0.13.
摘要翻译: 提供一种制造电极形成的玻璃基板的方法,其增加等离子体显示装置的前基板的强度。 在玻璃基板上形成的电极用无铅玻璃覆盖,其以质量%计,30%至50%的B 2 O 3,21至25%的SiO 2,10至35%的ZnO,7至14 K2O总量的百分比以及Li 2 O和Na 2 O中的一种或两者,0至10%的Al 2 O 3,0至10%的ZrO 2和0至5%的MgO + CaO + SrO + BaO,当摩尔 Li 2 O,Na 2 O和K 2 O的分数分别由l,n和k表示,l至多为0.025,l + n + k为0.07至0.13。
-
公开(公告)号:US07326666B2
公开(公告)日:2008-02-05
申请号:US10981613
申请日:2004-11-05
CPC分类号: C03C3/066
摘要: Glass for forming barrier ribs for e.g. a plasma display panel, which consists, as represented by mol % based on the following oxides, essentially of from 24 to 50% of SiO2, from 13 to 23% of B2O3, from 10 to 32% of ZnO, from 3 to 20% of Li2O, from 1 to 9% of Na2O, from 1 to 15% of Al2O3, from 0 to 20% of MgO+CaO+SrO+BaO, and from 0 to 9% of Bi2O3, wherein ((B2O3+ZnO)—Al2O3) is at least 24 mol %; in a case where ZrO2 is contained, its content is at most 2 mol %; and neither PbO nor F is contained.
摘要翻译: 用于形成阻挡肋的玻璃。 等离子体显示面板,其由以下氧化物的摩尔%表示,基本上为SiO 2的24至50%,B 2 2的13至23% ZnO,10〜32%的ZnO,3〜20%的Li 2 O,1〜9%的Na 2 O 3, 1〜15%的Al 2 O 3,0〜20%的MgO + CaO + SrO + BaO和0〜9%的Al 2 O 3 其中((B 2 O 3 + 3 + ZnO)-Al 2 O 3, / O 3 3)为至少24摩尔%。 在含有ZrO 2的情况下,其含量为2摩尔%以下。 并且不含有PbO和F。
-
公开(公告)号:US20050113241A1
公开(公告)日:2005-05-26
申请号:US10981613
申请日:2004-11-05
CPC分类号: C03C3/066
摘要: Glass for forming barrier ribs for e.g. a plasma display panel, which consists, as represented by mol % based on the following oxides, essentially of from 24 to 50% of SiO2, from 13 to 23% of B2O3, from 10 to 32% of ZnO, from 3 to 20% of Li2O, from 1 to 9% of Na2O, from 1 to 15% of Al2O3, from 0 to 20% of MgO+CaO+SrO+BaO, and from 0 to 9% of Bi2O3, wherein ((B2O3+ZnO)—Al2O3) is at least 24 mol %; in a case where ZrO2 is contained, its content is at most 2 mol %; and neither PbO nor F is contained.
摘要翻译: 用于形成阻挡肋的玻璃。 等离子体显示面板,其由以下氧化物的摩尔%表示,基本上为SiO 2的24至50%,B 2 2的13至23% ZnO,10〜32%的ZnO,3〜20%的Li 2 O,1〜9%的Na 2 O 3, 1〜15%的Al 2 O 3,0〜20%的MgO + CaO + SrO + BaO和0〜9%的Al 2 O 3 其中((B 2 O 3 + 3 + ZnO)-Al 2 O 3, / O 3 3)为至少24摩尔%。 在含有ZrO 2的情况下,其含量为2摩尔%以下。 并且不含有PbO和F。
-
公开(公告)号:US06939819B2
公开(公告)日:2005-09-06
申请号:US10463697
申请日:2003-06-18
申请人: Hiroshi Usui , Hitoshi Onoda , Kazunari Watanabe , Yumi Okuyama , Yasuko Osaki , Katsuyoshi Nakayama
发明人: Hiroshi Usui , Hitoshi Onoda , Kazunari Watanabe , Yumi Okuyama , Yasuko Osaki , Katsuyoshi Nakayama
IPC分类号: C03C3/091 , C03C10/00 , C03C14/00 , C04B35/195 , C04B35/20
CPC分类号: C03C10/0009 , C03C3/091 , C03C14/004 , C03C2214/04 , C03C2214/20 , C04B35/16 , C04B35/195 , C04B35/20 , C04B2235/3206 , C04B2235/3215 , C04B2235/3217 , C04B2235/3284 , C04B2235/3409 , C04B2235/96
摘要: A glass ceramic composition which consists essentially of an inorganic material powder having a melting point or a glass transition point of at least 1,000° C. and a glass powder having a glass transition point of from 450 to 800° C., wherein the average of the major axes L of particles of the above inorganic material powder is from 0.5 to 15 μm, and the average of the ratios L/W of the major axes L to the minor axes W is at most 1.4. Further, a glass ceramic composition which consists essentially of, as represented by mass percentage, from 10 to 58% of an inorganic material powder having a melting point or a glass transition point of at least 1,000° C. and from 42 to 90% of a glass powder having a glass transition point of from 450 to 800° C., wherein the glass powder consists essentially of, as represented by mol %, SiO2: 35 to 70%, B2O3: 0 to 30%, Al2O3: 3 to 18%, MgO: 0 to 40%, CaO: 0 to 19%, BaO: 0 to 35% and ZnO: 0 to 9%.
摘要翻译: 一种玻璃陶瓷组合物,其基本上由具有至少1000℃的熔点或玻璃化转变点的无机材料粉末和玻璃化转变点为450至800℃的玻璃粉末组成,其中平均 上述无机材料粉末的颗粒的长轴L为0.5〜15μm,长轴L与短轴W的比L / W的平均值为1.4以下。 此外,玻璃陶瓷组合物基本上由以质量百分数表示的10至58%的无机材料粉末组成,该无机材料粉末的熔点或玻璃化转变点至少为1000℃,玻璃化转变温度为42-90% 玻璃化转变点为450〜800℃的玻璃粉末,其中玻璃粉末主要由摩尔%表示,SiO 2:35〜70%,B < 2〜3%:0〜30%,3%〜3%,3%〜18%,MgO:0〜40% ,CaO:0〜19%,BaO:0〜35%,ZnO:0〜9%。
-
公开(公告)号:US06617789B2
公开(公告)日:2003-09-09
申请号:US09971618
申请日:2001-10-09
申请人: Hitoshi Onoda , Yumiko Aoki , Tsuneo Manabe , Satoshi Fujimine , Michifumi Kawai , Shoichi Iwanaga
发明人: Hitoshi Onoda , Yumiko Aoki , Tsuneo Manabe , Satoshi Fujimine , Michifumi Kawai , Shoichi Iwanaga
IPC分类号: H01J1102
CPC分类号: C03C8/245 , C03C3/074 , C03C3/0745 , C03C8/24
摘要: A glass for covering electrodes, which consists, as represented by mass percentage based on the following oxides, essentially of: Mass percentage PbO 44 to 68% Bi2O3 0 to 18%, B2O3 19 to 23%, SiO2 1.2 to 5%, Al2O3 2 to 6%, ZnO 4 to 9%, CuO 0.1 to 0.5%, In2O3 1.1 to 2%, SnO2 0 to 1%, and CeO2 0 to 1%.
摘要翻译: 用于覆盖电极的玻璃,其以由以下氧化物的质量百分比表示,主要包括:
-
公开(公告)号:US20100239971A1
公开(公告)日:2010-09-23
申请号:US12676546
申请日:2008-09-03
申请人: Tohru Moriya , Hitoshi Onoda , Kazuyoshi Hattori , Yoshihito Suwa
发明人: Tohru Moriya , Hitoshi Onoda , Kazuyoshi Hattori , Yoshihito Suwa
IPC分类号: G03G9/08
CPC分类号: G03G9/09716 , G03G9/081 , G03G9/08755 , G03G9/09708 , G03G9/09725
摘要: A toner for electrophotography includes toner particles containing at least a binder resin and a colorant, to which strontium titanate and hydrophobic silica as external additives are admixed, wherein the strontium titanate has a BET specific surface area of 20-50 m2/g and contains particles in a rectangular parallelepiped shape and wherein the hydrophobic silica contains hydrophobic silica A that has at least a BET specific surface area of 150-300 m2/g and the surface of which has been treated with an aminosilane and hexamethyldisilazane and hydrophobic silica B that has at least a BET specific surface area of 90-150 m2/g and the surface of which has been treated with hexamethyldisilazane.
摘要翻译: 用于电子照相的调色剂包括至少含有粘合剂树脂和着色剂的调色剂颗粒,其中混合钛酸锶和疏水性二氧化硅作为外部添加剂,其中钛酸锶的BET比表面积为20-50m 2 / g,并含有颗粒 其中所述疏水性二氧化硅含有至少具有150-300m 2 / g的BET比表面积的表面用氨基硅烷和六甲基二硅氮烷处理的疏水性二氧化硅A和疏水性二氧化硅B,所述疏水性二氧化硅A具有 最小BET比表面积为90-150m2 / g,其表面用六甲基二硅氮烷处理。
-
8.
公开(公告)号:US06287996B1
公开(公告)日:2001-09-11
申请号:US09393169
申请日:1999-09-10
申请人: Jiro Chiba , Takaji Shimosaka , Kenji Mukai , Shuji Taguchi , Mineyuki Ishida , Hitoshi Onoda , Hiroshi Usui , Tsuneo Manabe
发明人: Jiro Chiba , Takaji Shimosaka , Kenji Mukai , Shuji Taguchi , Mineyuki Ishida , Hitoshi Onoda , Hiroshi Usui , Tsuneo Manabe
IPC分类号: C03C814
摘要: A ceramic color composition which comprises from 5 to 40 wt % of a heat-resistant color pigment powder, from 50 to 94.5 wt % of a glass powder, from 0 to 25 wt % of a refractory filler, and from 0.1 to 40 wt % of at least one whisker-like refractory filler selected from the group consisting of aluminum borate whiskers, &agr;-alumina whiskers, potassium titanate whiskers, zinc oxide whiskers, Na2Ca2P2O18 whiskers, magnesium oxide whiskers, magnesium borate whiskers, basic magnesium sulfate (MgSO4.5MgO.8H2O) whiskers and titanium diboride whiskers.
摘要翻译: 一种陶瓷颜色组合物,其包含5至40重量%的耐热彩色颜料粉末,50至94.5重量%的玻璃粉末,0至25重量%的耐火填料和0.1至40重量% 至少一种选自硼酸铝晶须,α-氧化铝晶须,钛酸钾晶须,氧化锌晶须,Na 2 Ca 2 P 2 O 8晶须,氧化镁晶须,硼酸镁晶须,碱式硫酸镁(MgSO4.5MgO)的晶须状耐火填料 .8H2O)晶须和二硼化钛晶须。
-
公开(公告)号:US5908794A
公开(公告)日:1999-06-01
申请号:US816898
申请日:1997-03-13
申请人: Kei Maeda , Hitoshi Onoda , Yasumasa Nakao , Jeetendra Sehgal
发明人: Kei Maeda , Hitoshi Onoda , Yasumasa Nakao , Jeetendra Sehgal
IPC分类号: C03C3/087
CPC分类号: C03C3/087
摘要: A glass composition for a substrate consisting essentially of from 56 to 72 wt % of SiO.sub.2, from 1 to less than 14 wt % of Al.sub.2 O.sub.3, from 0 to 9 wt % of MgO, from 0.5 to 11 wt % of CaO, from 0 to 4 wt % of SrO, from 0 to 3 wt % of BaO, from 6 to less than 14 wt % of MgO+CaO+SrO+BaO, from 0 to 9 wt % of Na.sub.2 O, from 6 to 20 wt % of K.sub.2 O, and from 6 to 20 wt % of Na.sub.2 O+K.sub.2 O.
摘要翻译: 用于基材的玻璃组合物,其基本上由56至72重量%的SiO 2,1至小于14重量%的Al 2 O 3,0至9重量%的MgO,0.5至11重量%的CaO,0至 4重量%的SrO,0〜3重量%的BaO,6〜小于14重量%的MgO + CaO + SrO + BaO,0〜9重量%的Na 2 O,6〜20重量%的K 2 O, 和6至20重量%的Na 2 O + K 2 O。
-
公开(公告)号:US5858897A
公开(公告)日:1999-01-12
申请号:US816674
申请日:1997-03-13
申请人: Kei Maeda , Hitoshi Onoda , Yasumasa Nakao , Jeetendra Sehgal
发明人: Kei Maeda , Hitoshi Onoda , Yasumasa Nakao , Jeetendra Sehgal
IPC分类号: C03C3/087
CPC分类号: C03C3/087
摘要: A glass composition for a substrate consisting essentially of from 59 to 72 wt % of SiO.sub.2, from 1 to 15 wt % of Al.sub.2 O.sub.3, from 0.5 to 9 wt % of MgO, from 0.5 to 11 wt % of CaO, from 0 to 6 wt % of SrO, from 0 to 5 wt % of BaO, from 4 to 19 wt % of MgO+CaO+SrO+BaO, from 0 to 9 wt % of Na.sub.2 O , from 4 to 21 wt % of K.sub.2 O, from 10 to 22 wt % of Na.sub.2 O+K.sub.2 O, and from 0.5 to 10.5 wt % of ZrO.sub.2, wherein the difference between the SiO.sub.2 content and the Al.sub.2 O.sub.3 content is from 50 to 71 wt %, and the specific gravity of the composition is less than 2.6.
摘要翻译: 用于基材的玻璃组合物,其基本上由以下组成:59〜72重量%的SiO 2,1〜15重量%的Al 2 O 3,0.5〜9重量%的MgO,0.5〜11重量%的CaO,0〜6重量% 0%至5重量%的BaO,4至19重量%的MgO + CaO + SrO + BaO,0至9重量%的Na 2 O,4至21重量%的K 2 O,10至22 Na 2 O + K 2 O的重量百分数和0.5〜10.5重量%的ZrO 2,其中SiO 2含量与Al 2 O 3含量之间的差为50〜71重量%,组合物的比重小于2.6。
-
-
-
-
-
-
-
-
-