摘要:
To provide non-lead glass for covering electrodes, whereby the strength of front substrates of plasma display devices can be improved, and the dielectric constant can be made small.Non-lead glass for covering electrodes, which comprises, as represented by mol % based on the following oxides, from 42 to 52% of B2O3, from 40 to 48% of SiO2, from 3.5 to less than 7% of K2O and from 0 to 6% of ZrO2, wherein the total content of B2O3 and SiO2 is at least 88%. Further, a plasma display device comprising a front glass substrate to be used as a display surface, a rear glass substrate and barrier ribs to define cells, wherein transparent electrodes formed on the front glass substrate or the rear glass substrate are covered with the above non-lead glass for covering electrodes.
摘要翻译:为了提供用于覆盖电极的非铅玻璃,由此可以提高等离子体显示装置的前基板的强度,并且可以使介电常数小。 用于覆盖电极的非铅玻璃,其以以下氧化物的摩尔%表示,42%至52%的B 2 O 3,40至48%的SiO 2,3.5至小于7%的K 2 O和0 至6%的ZrO 2,其中B 2 O 3和SiO 2的总含量为至少88%。 此外,包括用作显示表面的前玻璃基板,后玻璃基板和限定单元的阻挡肋的等离子体显示装置,其中形成在前玻璃基板或后玻璃基板上的透明电极被上述非玻璃基板 用于覆盖电极的玻璃。
摘要:
To provide a process for producing an electrode-formed glass substrate, which is capable of suppressing warpage without lowering the strength of a front substrate of a plasma display device.Electrodes formed on a glass substrate are covered with a lead-free glass comprising, as represented by mass %, from 30 to 50% of B2O3, more than 25% and at most 35% of SiO2, from 10 to 25% of ZnO, from 7 to 19% in total of K2O and either one or both of Li2O and Na2O, from 0 to 5% of Al2O3, from 0 to 5% of MgO+CaO+SrO+BaO, and when the molar fractions of Li2O, Na2O and K2O are represented by l, n and k, respectively, l is at most 0.025, and l+n+k is from 0.07 to 0.17.
摘要翻译:提供一种能够在不降低等离子体显示装置的前基板的强度的情况下抑制翘曲的电极形成玻璃基板的制造方法。 在玻璃基板上形成的电极被无铅玻璃覆盖,所述无铅玻璃以质量%计,30%〜50%的B 2 O 3,25%以上,35%以下的SiO 2,10〜25%的ZnO, 总共K2O为7〜19%,Li2O和Na2O中的一种或两种,Al2O3的0〜5%,MgO + CaO + SrO + BaO的0〜5%,Li2O,Na2O的摩尔分数 和K2O分别由l,n和k表示,l至多为0.025,l + n + k为0.07至0.17。
摘要:
Non-lead glass consisting essentially of, as represented by mol %, from 20 to 50% of B2O3, from 5 to 35% of SiO2, from 10 to 30% of ZnO, from 0 to 10% of Al2O3, from 0 to 10% of SrO, from 6 to 16% of BaO, from 2 to 16% of Li2O, from 0 to 10% of Na2O+K2O, from 0 to 9% of Bi2O3, and from 0 to 2% of CuO+CeO2, wherein (B2O3+SiO2+Al2O3)/(Bi2O3+BaO) is at least 3.25, and MgO+CaO is at most 8 mol %. Further, a plasma display device wherein transparent electrodes formed on a glass substrate constituting a front substrate, or electrodes formed on a glass substrate constituting a rear substrate, are covered by the non-lead glass.
摘要翻译:基本上由摩尔%表示20%至50%的B 2 O 3 3,5〜35%的SiO 2的非铅玻璃 10〜30%的ZnO,0〜10%的Al 2 O 3 3,0〜10%的SrO,6〜16 %的BaO,2〜16%的Li 2 O,0〜10%的Na 2 O + K 2 O,来自 0〜9%的Bi 2 O 3 3和0〜2%的CuO + CeO 2 2,其中(B 2) 3/3 + 1/2 + 2 + 2 + 3)/(Bi 2) O 3 + BaO)为3.25以上,MgO + CaO为8摩尔%以下。 此外,其中形成在构成前基板的玻璃基板上的透明电极或形成在构成后基板的玻璃基板上的电极的等离子体显示装置被非铅玻璃覆盖。
摘要:
A lead-free glass for covering electrodes including, as represented by mass % based on the following oxides, from 30 to 50% of B2O3, from 21 to 25% of SiO2, from 10 to 35% of ZnO, from 7 to 14% in total of K2O and either one or both of Li2O and Na2O, from 0 to 10% of Al2O3, and from 0 to 10% of ZrO2, wherein when it contains at least one component selected from the group consisting of MgO, CaO, SrO and BaO, the total of their contents is at most 5%, and when the molar fractions of Li2O, Na2O and K2O are represented by l, n and k, respectively, l is at most 0.025, and l+n+k is from 0.07 to 0.17.
摘要翻译:一种用于覆盖电极的无铅玻璃,包括以下列氧化物的质量%表示:B2O3的30-50%,SiO2的21-25%,ZnO的10-35%,7-14% K 2 O和Li 2 O和Na 2 O中的一种或两者,0至10%的Al 2 O 3和0至10%的ZrO 2,其中当其含有至少一种选自MgO,CaO,SrO 和BaO,其总含量最多为5%,当Li 2 O,Na 2 O和K 2 O的摩尔分数分别由l,n和k表示时,l最多为0.025,l + n + k来自 0.07〜0.17。
摘要:
Glass for forming barrier ribs for e.g. a plasma display panel, which consists, as represented by mol % based on the following oxides, essentially of from 24 to 50% of SiO2, from 13 to 23% of B2O3, from 10 to 32% of ZnO, from 3 to 20% of Li2O, from 1 to 9% of Na2O, from 1 to 15% of Al2O3, from 0 to 20% of MgO+CaO+SrO+BaO, and from 0 to 9% of Bi2O3, wherein ((B2O3+ZnO)—Al2O3) is at least 24 mol %; in a case where ZrO2 is contained, its content is at most 2 mol %; and neither PbO nor F is contained.
摘要翻译:用于形成阻挡肋的玻璃。 等离子体显示面板,其由以下氧化物的摩尔%表示,基本上为SiO 2的24至50%,B 2 2的13至23% ZnO,10〜32%的ZnO,3〜20%的Li 2 O,1〜9%的Na 2 O 3, 1〜15%的Al 2 O 3,0〜20%的MgO + CaO + SrO + BaO和0〜9%的Al 2 O 3 其中((B 2 O 3 + 3 + ZnO)-Al 2 O 3, / O 3 3)为至少24摩尔%。 在含有ZrO 2的情况下,其含量为2摩尔%以下。 并且不含有PbO和F。
摘要:
A low melting point glass for covering electrodes, which contains Cu in a content as calculated as CuO within a range of from 0.1 to 0.9% by mass percentage and which contains neither Mo or Sb.
摘要:
A light emitting diode element having a light emitting diode; and a glass covering sealing the light emitting diode is provided. The glass of the covering consists essentially of from 30 to 70 mol % of SnO, from 15 to 50 mol % of P2O5, from 0.1 to 20 mol % of ZnO, from 0 to 10 mol % of SiO2+GeO2, from 0 to 30% of Li2O+Na2O+K2O, and from 0 to 20% of MgO+CaO+SrO+BaO. In an embodiment, a refractive index of the glass of the covering is at least 1.6 at a wavelength of 400 nm.
摘要翻译:一种具有发光二极管的发光二极管元件; 并提供密封发光二极管的玻璃盖。 该覆盖层的玻璃基本上由SnO 30-70mol%,P2O5 15-50mol%,氧化铝0.1-20mol%,SiO 2 + GeO 0至10mol%,0至30 %的Li 2 O + Na 2 O + K 2 O,0〜20%的MgO + CaO + SrO + BaO。 在一个实施例中,覆盖玻璃的折射率在波长400nm处至少为1.6。
摘要:
A glass for covering electrodes, which consists, as represented by mass percentage based on the following oxides, essentially of from 35 to 55% of PbO, from 15 to 30% of B2O3, from 4 to 15% of SiO2, from 20 to 44% of B2O3+SiO2, from 0.5 to 10% of TiO2+ZrO2+La2O3+Ta2O5, from 0 to 15% of Al2O3, from 0 to 25% of BaO, from 0 to 1% of CuO and from 0 to 1% of CeO2.
摘要翻译:用于覆盖电极的玻璃,其以由以下氧化物的质量百分比表示,基本上为35%至55%的PbO,15%至30%的B 2 O 3 4〜15%的SiO 2,20〜44%的B 2 O 3 + SiO 2, 2%,0.5至10%的TiO 2 + ZrO 2 + La 2 O 3 N 3 O 3 0〜25%,0〜25%的O 2〜5%,0〜25% 的BaO,0至1%的CuO和0至1%的CeO 2。
摘要:
A glass for covering electrodes, which consists, as represented by mass percentage based on the following oxides, essentially of: Mass percentage PbO 44 to 68% Bi2O3 0 to 18%, B2O3 19 to 23%, SiO2 1.2 to 5%, Al2O3 2 to 6%, ZnO 4 to 9%, CuO 0.1 to 0.5%, In2O3 1.1 to 2%, SnO2 0 to 1%, and CeO2 0 to 1%.
摘要:
A light emitting diode element having a light emitting diode sealed by glass, wherein the glass consists essentially of, as represented by mol % based on the following oxides, from 30 to 70% of SnO, from 15 to 50% of P2O5, from 0.1 to 20% of ZnO, from 0 to 10% of SiO2+GeO2, from 0 to 30% of Li2O+Na2O+K2O, and from 0 to 20% of MgO+CaO+SrO+BaO. Glass for covering a light emitting diode element, which has an internal transmittance of at least 80% with thickness of 1 mm for a light having a wavelength of 405. nm and which consists essentially of, as represented by mol % based on the following oxides, from 40 to 53% of TeO2, from 0 to 10% of GeO2, from 5 to 30% of B2O3, from 0 to 10% of Ga2O3, from 0 to 10% of Bi2O3, from 3 to 20% of ZnO, from 0 to 3% of Y2O3, from 0 to 3% of La2O3, from 0 to 7% of Gd2O3 and from 0 to 5% of Ta2O5, and TeO2+B2O3 is at most 75 mol %.
摘要翻译:具有由玻璃密封的发光二极管的发光二极管元件,其中所述玻璃基本上由以下氧化物的摩尔%表示:SnO 30-70%,P < 2%O 5,0.1%至20%的ZnO,0至10%的SiO 2 + GeO 2 2,来自 0〜30%的Li 2 O + Na 2 O + K 2 O,0〜20%的MgO + CaO + SrO +宝。 用于覆盖发光二极管元件的玻璃,对于具有405nm波长的光,其具有至少80%的内部透射率,厚度为1mm,并且基本上由以下氧化物的摩尔%表示 ,40〜53%的TeO 2,0〜10%的GeO 2 2,5〜30%的B 2 O 2, 0〜10%的Ga 2 O 3,0〜10%的Bi 2 O 3, 3%〜3%,3%〜20%的ZnO,0〜3%的Y 2 O 3 3,0〜3%的La 2 O> 3,0〜7%的Gd 2 O 3 3和0〜5%的Ta 2 O> 5,并且TeO 2 + B 2 O 3 3至多为75摩尔 %。