公开(公告)号:US06596785B2
公开(公告)日:2003-07-22
申请号:US09906981
申请日:2001-07-17
申请人: Sharon A. Free
发明人: Sharon A. Free
IPC分类号: C08G1810
CPC分类号: B41J2/17513 , C08G18/4837 , C08G18/7607 , C08G2101/0008 , C08G2101/005 , C08G2101/0083
摘要: An ink retaining flexible polyurethane foam is prepared by reacting a polyether polyol with from 50 to 80 parts by weight, based on the weight of polyol, of a polyisocyanate component having one or a mixture of methylene diisocyanates. The foam has pore sizes above 70 pores per linear inch, preferably in the range of 70 to 90 pores per linear inch in an uncompressed state. The foam is reticulated to improve liquid holding capacity, and, depending upon cell size, compressed into a container. The foam absorbs and retains ink, and is resistant against attack from ink, producing less than 2.0% solvent extractables.
摘要翻译: 通过使聚醚多元醇与基于多元醇重量的50至80重量份的具有一个或多个亚甲基二异氰酸酯的混合物的多异氰酸酯组分反应制备墨水保持软质聚氨酯泡沫。 在未压缩状态下,该泡沫具有大于70个细孔的线性英寸,优选在每立方英寸的70至90个孔的范围内。 泡沫被网状化以改善液体保持能力,并且取决于细胞尺寸,压缩成容器。 泡沫吸收并保留油墨,并且耐油墨侵蚀,产生小于2.0%的溶剂可萃取物。
-
公开(公告)号:US20080213566A1
公开(公告)日:2008-09-04
申请号:US12037196
申请日:2008-02-26
申请人: Chiu Y. Chan , Sharon A. Free , Joshua D. Land , Marc J. Albero , Jagdish Patel , William P. Burke
发明人: Chiu Y. Chan , Sharon A. Free , Joshua D. Land , Marc J. Albero , Jagdish Patel , William P. Burke
IPC分类号: B32B27/40
CPC分类号: C08G18/42 , B32B5/24 , B32B5/32 , C08G2101/0008 , C08G2101/005 , C08G2101/0083 , C08J5/121 , C08J2375/06 , Y10T428/249953 , Y10T428/249981 , Y10T428/249991
摘要: A hydrophilic ester polyurethane foam is flame laminated to a substrate using a thin sacrificial layer, preferably a sacrificial foam layer. The sacrificial layer in the resulting laminate structure has a thickness of 1.5 mm or less, and preferably is substantially burnt away. The resulting laminate exhibits good bond strength along its length and width without loss of liquid wicking and absorptive properties.
摘要翻译: 使用薄牺牲层,优选牺牲泡沫层将亲水性聚酯酯泡沫体火焰层压到基底上。 所得层压结构中的牺牲层的厚度为1.5mm以下,优选大致燃烧。 所得到的层压体在其长度和宽度上显示出良好的粘合强度,而不损失液体芯吸和吸收性能。
-
公开(公告)号:US06371606B1
公开(公告)日:2002-04-16
申请号:US09907297
申请日:2001-07-17
申请人: Sharon A. Free
发明人: Sharon A. Free
IPC分类号: B41J2175
CPC分类号: B41J2/17513
摘要: An ink retaining flexible polyurethane foam is prepared by reacting a polyether polyol with from 20 to 50 parts by weight, based on the weight of polyol, of a polyisocyanate component having one or a mixture of toluene diisocyanates, such that the 2,4 isomer of toluene diisocyanate includes no more than seventy-five percent by weight of the polyisocyanate component, preferably no more than seventy two and one half percent by weight. The foam has pore sizes in the range of 70 to 88 pores per inch in an uncompressed state. The foam is reticulated to improve liquid holding capacity, and, depending upon pore size, felted to compression ratios from 1 to 2 up to from 1 to 20. The foam absorbs and retains ink, and is resistant against attack from ink, emitting less than 2.0% solvent extractables, preferably less than 1.1% solvent extractables.
摘要翻译: 通过使聚醚多元醇与基于多元醇的重量的20至50重量份的具有一个或多个甲苯二异氰酸酯的混合物的多异氰酸酯组分反应制备墨水保持性柔性聚氨酯泡沫,使得2,4- 甲苯二异氰酸酯包括不超过75重量%的多异氰酸酯组分,优选不超过75重量%。 在未压缩状态下,泡沫的孔径在每英寸70至88孔的范围内。 泡沫被网状化以提高液体保持能力,并且取决于孔径,从1至2的压缩比至1至20。泡沫吸收并保留油墨,并且抵抗油墨的侵蚀,发射少于 2.0%溶剂萃取物,优选低于1.1%的溶剂可萃取物。
-
4.
公开(公告)号:US20130245159A1
公开(公告)日:2013-09-19
申请号:US13611973
申请日:2012-09-12
申请人: F. Brent Neal , Sharon A. Free , Keith A. Keller
发明人: F. Brent Neal , Sharon A. Free , Keith A. Keller
IPC分类号: C08K3/30 , C08K5/1515
CPC分类号: C08K3/30 , C08K5/1515 , C08K2003/3045 , C08K2003/3063 , C08L63/00
摘要: An epoxy resin composition comprises an epoxy resin, a plurality of particles, and a diluent. The particles can comprise a magnesium oxysulfate compound. The diluent can be selected from the group consisting of monoglycidyl compounds, diglycidyl compounds, bisphenol-A alkoxylates, and mixtures thereof. The epoxy resin composition can be reacted with an activator composition to produce an epoxy polymer. The activator composition can comprise one or more compounds selected from the group consisting of polyamine compounds, anhydride compounds, and mixtures thereof.
摘要翻译: 环氧树脂组合物包含环氧树脂,多个颗粒和稀释剂。 颗粒可以包含硫代硫酸镁化合物。 稀释剂可以选自单缩水甘油基化合物,二缩水甘油基化合物,双酚A烷氧基化物及其混合物。 环氧树脂组合物可以与活化剂组合物反应以制备环氧聚合物。 活化剂组合物可以包含一种或多种选自多胺化合物,酸酐化合物及其混合物的化合物。
-
公开(公告)号:US06841586B2
公开(公告)日:2005-01-11
申请号:US10744052
申请日:2003-12-23
申请人: Sharon A. Free , Charles V. Rose
发明人: Sharon A. Free , Charles V. Rose
CPC分类号: C08J9/38 , B29C44/5636 , C08G18/4202 , C08G18/4238 , C08G18/4252 , C08G2101/0008 , C08G2101/005 , C08G2101/0083 , C08J9/40 , C08J2375/04
摘要: An ester polyurethane foam is prepared by reacting a mixture of one or more polyester polyols with one or more isocyanates and one or more silicone surfactants in the presence of a blowing agent, such as water, and other additives, such as catalysts. The cured foam is chemically treated in a caustic solution and is then felted (compressed under heat and pressure) to form a hydrophilic ester polyurethane foam having a water absorption rate of at least 30 pounds of water per square foot per minute (1.44 kPa/min). The foam also has greater water holding capacity and wet strength than cellulose.
摘要翻译: 通过使一种或多种聚酯多元醇与一种或多种异氰酸酯和一种或多种有机硅表面活性剂的混合物在发泡剂如水和其它添加剂如催化剂存在下反应来制备酯聚氨酯泡沫。 固化的泡沫体在苛性碱溶液中进行化学处理,然后被加热(在加热和压力下压缩)以形成亲水性聚酯酯泡沫,其吸水率为每平方英尺每分钟至少30磅水(1.44kPa / min )。 该泡沫还具有比纤维素更大的保水能力和湿强度。
-
公开(公告)号:US06756416B2
公开(公告)日:2004-06-29
申请号:US10074606
申请日:2002-02-12
IPC分类号: C08G1828
CPC分类号: C08J9/40 , C08G18/4202 , C08G18/4252 , C08G2101/0008 , C08G2101/005 , C08G2101/0083 , C08J2375/04
摘要: An ester polyurethane foam is prepared by reacting a mixture of one or more polyester polyols with one or more isocyanates and one or more silicone surfactants in the presence of a blowing agent, such as water, and other additives, such as catalysts. The cured foam is chemically treated in a caustic solution to form a hydrophilic ester polyurethane foam having a water absorption rate of at least 20 pounds of water per square foot per minute, preferably at least 25 pounds of water per square foot per minute. The foam also has greater water holding capacity and wet strength than cellulose.
摘要翻译: 通过使一种或多种聚酯多元醇与一种或多种异氰酸酯和一种或多种有机硅表面活性剂的混合物在发泡剂如水和其它添加剂如催化剂存在下反应来制备酯聚氨酯泡沫。 固化的泡沫体在苛性碱溶液中进行化学处理以形成亲水性聚酯酯泡沫,其吸水率为每平方英尺每分钟至少20磅水,优选每平方英尺至少25磅水。 该泡沫还具有比纤维素更大的保水能力和湿强度。
-
公开(公告)号:US5034422A
公开(公告)日:1991-07-23
申请号:US630306
申请日:1990-12-19
申请人: Rocco P. Triolo , Sharon A. Free , David J. Kelly
发明人: Rocco P. Triolo , Sharon A. Free , David J. Kelly
CPC分类号: C08J9/42 , C08J9/26 , C08J2201/0464 , C08J2205/05 , C08J2427/00 , C08J2433/00 , C08J2483/00
摘要: A low density, open cell polymeric body is formed by coating or filling a reticulated polymeric foam with a liquid-form polymer which is resistant to high temperatures, curing the liquid form polymer in and on the foam and then removing the foam skeleton by dissolving and leaching the foam out of the solid polymeric body which remains.
摘要翻译: 通过用耐高温的液态聚合物涂覆或填充网状聚合物泡沫来固化低密度开孔聚合物体,固化泡沫中和泡沫上的液体形式的聚合物,然后通过溶解和 将泡沫从保留的固体聚合物中浸出。
-
公开(公告)号:US07687139B2
公开(公告)日:2010-03-30
申请号:US12037196
申请日:2008-02-26
申请人: Chiu Y. Chan , Sharon A. Free , Joshua D. Land , Marc J. Albero , Jagdish Patel , William Patrick Burke, III
发明人: Chiu Y. Chan , Sharon A. Free , Joshua D. Land , Marc J. Albero , Jagdish Patel , William Patrick Burke, III
CPC分类号: C08G18/42 , B32B5/24 , B32B5/32 , C08G2101/0008 , C08G2101/005 , C08G2101/0083 , C08J5/121 , C08J2375/06 , Y10T428/249953 , Y10T428/249981 , Y10T428/249991
摘要: A hydrophilic ester polyurethane foam is flame laminated to a substrate using a thin sacrificial layer, preferably a sacrificial foam layer. The sacrificial layer in the resulting laminate structure has a thickness of 1.5 mm or less, and preferably is substantially burnt away. The resulting laminate exhibits good bond strength along its length and width without loss of liquid wicking and absorptive properties.
摘要翻译: 使用薄牺牲层,优选牺牲泡沫层将亲水性聚酯酯泡沫体火焰层压到基底上。 所得层压结构中的牺牲层的厚度为1.5mm以下,优选大致燃烧。 所得到的层压体在其长度和宽度上显示出良好的粘合强度,而不损失液体芯吸和吸收性能。
-
9.
公开(公告)号:US6136878A
公开(公告)日:2000-10-24
申请号:US802033
申请日:1997-02-18
CPC分类号: C08G18/7607 , C08G18/4072 , C08G18/7664 , C08G2101/0008 , C08G2101/005 , C08G2101/0083
摘要: The present invention relates to very fine cell flexible polyurethane foams having at least 87 pores per linear inch (as measured by pressure drop techniques) wherein at least 65% of the isocyanate equivalents of said polyurethane are obtained from MDI. The invention also relates to processes for preparing the very fine cell polyurethane foams.
摘要翻译: 本发明涉及具有每线性英寸至少87个孔(通过压降技术测量)的非常细小的柔性聚氨酯泡沫,其中至少65%的所述聚氨酯的异氰酸酯当量是从MDI获得的。 本发明还涉及制备极细细胞聚氨酯泡沫体的方法。
-
公开(公告)号:US5650450A
公开(公告)日:1997-07-22
申请号:US591040
申请日:1996-01-25
申请人: Joseph W. Lovette , Sharon A. Free
发明人: Joseph W. Lovette , Sharon A. Free
CPC分类号: C08G18/4837 , C08G18/4833 , C08G18/7607 , C08G18/7664 , C08G2101/0008 , C08G2101/0083 , Y10S521/905 , Y10S521/914
摘要: Hydrophilic polyurethane foams with rapid wet out properties are formed from the reaction product of an MDI-based or polymeric MDI-based isocyanate capped prepolymer with an aqueous component, such as water, and about 0.5 to 2.0 parts by weight, based on 100 parts by weight prepolymer, of a silicone glycol copolymer liquid surfactant with a polyether portion, said surfactant having a viscosity of about 175 to 350 CST at 25.degree. C., a molecular weight in the range of about 1500 to 20,000, with the polyether portion having a molecular weight in the range of about 200 to 2000 and containing about 40 to 100 percent by weight ethylene oxide. The surface of the hydrophilic foam wets out or absorbs droplets of water in less than thirty (30) seconds, preferably instantaneously (less than one second).
摘要翻译: 具有快速润湿特性的亲水性聚氨酯泡沫由MDI基或聚合MDI基异氰酸酯封端的预聚物与水组分如水组成的反应产物形成,约为0.5-2.0重量份,基于100份 重量预聚物,具有聚醚部分的硅氧烷二醇共聚物液体表面活性剂,所述表面活性剂在25℃下具有约175至350CST的粘度,分子量在约1500至20,000的范围内,聚醚部分具有 分子量在约200至2000范围内,并含有约40至100重量%的环氧乙烷。 亲水性泡沫的表面在少于三十(30)秒钟内,优选瞬时(少于一秒))滴入或吸收水滴。
-
-
-
-
-
-
-
-
-