摘要:
There are provided a nonaqueous-type electrolyte solution having high flame retardancy and a good capacity retention rate, and a device comprising the nonaqueous-type electrolyte solution. The nonaqueous-type electrolyte solution is used in a device comprising a positive electrode, a negative electrode and the nonaqueous-type electrolyte solution, and contains a lithium salt and a compound having a phosphazene structure, and further contains 0.05% by mass or more and 12.0% by mass or less of at least one disulfonate ester selected from a cyclic disulfonate ester and a chain disulfonate ester based on the total of the nonaqueous-type electrolyte solution.
摘要:
A non-aqueous electrolyte can suppress decomposition of a solvent, improve the cycle life of a secondary battery, suppress the rise of resistance of a secondary battery and improve the capacity maintenance ratio of a secondary battery. A non-aqueous electrolyte secondary battery formed by using such a non-aqueous electrolyte includes a non-aqueous electrolyte containing an aprotic solvent and a disulfonic acid ester as expressed by chemical formula 1 shown below, a positive electrode and a negative electrode:
摘要:
To provide high energy density, good cycle properties and rate characteristics and long-term safety of a lithium ion battery containing at least an ionic liquid and a lithium salt. The above problems are solved by suppressing reduction and decomposition of the ionic liquid on an anode by using a graphite coated with an amorphous carbon or onto which an amorphous carbon is deposited as an anode active material.
摘要:
There are provided a nonaqueous-type electrolyte solution having high flame retardancy and a good capacity retention rate, and a device comprising the nonaqueous-type electrolyte solution. The nonaqueous-type electrolyte solution is used in a device comprising a positive electrode, a negative electrode and the nonaqueous-type electrolyte solution, and contains a lithium salt and a compound having a phosphazene structure, and further contains 0.05% by mass or more and 12.0% by mass or less of at least one disulfonate ester selected from a cyclic disulfonate ester and a chain disulfonate ester based on the total of the nonaqueous-type electrolyte solution.
摘要:
A non-aqueous electrolyte can suppress decomposition of a solvent, improve the cycle life of a secondary battery, suppress the rise of resistance of a secondary battery and improve the capacity maintenance ratio of a secondary battery A non-aqueous electrolyte secondary battery formed by using such a non-aqueous electrolyte includes a non-aqueous electrolyte containing an aprotic solvent and a disulfonic acid ester as expressed by chemical formula 1 shown below, a positive electrode and a negative electrode:
摘要:
There is provided a lithium ion battery which maintains the flame retardancy of an electrolyte over a long period of time, has high energy density, and has improved charge/discharge cycle characteristics, high temperature storage characteristics, and rate characteristics. The lithium ion battery according to the present exemplary embodiment is a lithium ion battery comprising an electrolyte containing at least an ionic liquid and a lithium salt, a positive electrode, and a negative electrode, wherein the negative electrode includes a negative electrode active material which is a carbon material treated with a surface treatment agent.
摘要:
An object of the present invention is to provide a gel electrolyte for a lithium ion secondary battery having flame retardancy over a long period and a good capacity maintenance rate. The gel electrolyte for a lithium ion secondary battery according to the exemplary embodiment contains a lithium salt, a copolymer of at least one first monomer selected from compounds represented by chemical formulae (1) and (2) and a second monomer represented by chemical formula (4), at least one oxo-acid ester derivative of phosphorus selected from compounds represented by chemical formulae (5) to (7), and at least one disulfonate ester selected from a cyclic-chain type disulfonate ester represented by chemical formula (8) and a linear-chain type disulfonate ester represented by chemical formula (9).
摘要:
An object of the present invention is to provide a gel electrolyte for a lithium ion secondary battery having flame retardancy over a long period and a good capacity maintenance rate. The gel electrolyte for a lithium ion secondary battery according to the exemplary embodiment contains a lithium salt, a copolymer of at least one first monomer selected from compounds represented by chemical formulae (1) and (2) and a second monomer represented by chemical formula (4), at least one oxo-acid ester derivative of phosphorus selected from compounds represented by chemical formulae (5) to (7), and at least one disulfonate ester selected from a cyclic-chain type disulfonate ester represented by chemical formula (8) and a linear-chain type disulfonate ester represented by chemical formula (9).
摘要:
The present invention provides a stack-type lithium-ion polymer battery wherein: the battery capacity is not being degraded; the generation of the wrinkles and fracture of the separator is being suppressed; the battery has gas releasing paths; the displacement of an electrode stack hardly occurs; and the workability at the time of placing the electrode stack in a package body is improved by fixing the electrode stack. A stack-type lithium-ion polymer battery of the present invention comprises: a cathode 13; an anode 14; a separator 15; and a gel electrolyte; wherein an electrode stack 23 in which the cathode 13 and the anode 14 are stacked through the separator 15 is enclosed and fixed by insulating porous sheets 21 and 24, and is packaged with a laminate material.
摘要:
A lithium ion secondary battery electrode according to the present invention includes (A) a non-fluorinated polymer; (B) an active material; (C) a thickener; and (D) a conductive auxiliary agent. An elution ratio of (A) the non-fluorinated polymer in an electrolytic solution solvent at 60° C. is equal to or less than 1.0 mass %, and a swelling ratio of (A) the non-fluorinated polymer in the electrolytic solution solvent at 60° C. is equal to or more than 10 mass % and equal to or less than 50 mass %.