Catalyst that comprises a clay and an element of group VB, and its use in hydrocraking of petroleum feedstocks that contain hydrocarbon
    1.
    发明授权
    Catalyst that comprises a clay and an element of group VB, and its use in hydrocraking of petroleum feedstocks that contain hydrocarbon 失效
    包含粘土和VB族元素的催化剂,以及其用于加氢裂化含有烃的石油原料

    公开(公告)号:US06251261B1

    公开(公告)日:2001-06-26

    申请号:US09344348

    申请日:1999-06-25

    IPC分类号: C10G4702

    CPC分类号: C10G47/12 B01J21/16 B01J23/20

    摘要: The invention relates to a hydrocracking catalyst that comprises at least one oxide-type amorphous or poorly crystallized matrix, at least one element of group VB, preferably niobium, and at least one clay that is selected from the group that is formed by the 2:1 dioctahedral phyllosilicates and the 2:1 trioctahedral phyllosilicates, optionally at least one element that is selected from among the elements of group VIB and group VIII, optionally at least one element that is selected from the group that is formed by P, B, Si, and optionally at least one element of group VIIA. The invention also relates to the use of this catalyst in hydrocracking of feedstocks that contain hydrocarbon.

    摘要翻译: 本发明涉及一种加氢裂化催化剂,其包括至少一种氧化物型无定形或结晶不良的基体,VB族的至少一种元素,优选铌,以及至少一种选自由2: 1个二八面体页硅酸盐和2:1三八面体页硅酸盐,任选地至少一种选自VIB族和VIII族元素的元素,任选地至少一种选自由P,B,Si ,和任选的VIIA族的至少一种元素。 本发明还涉及该催化剂在含有烃的原料的加氢裂化中的用途。

    Hydrocracking process with catalyst comprising a zeolite Y not globally dealuminized, an element of group VB, and a promoter element of boron, phosphorus and silicon
    5.
    发明授权
    Hydrocracking process with catalyst comprising a zeolite Y not globally dealuminized, an element of group VB, and a promoter element of boron, phosphorus and silicon 有权
    含有未全面脱铝的沸石Y,VB族元素和硼,磷和硅的促进剂元素的催化剂的加氢裂化方法

    公开(公告)号:US06500330B2

    公开(公告)日:2002-12-31

    申请号:US09725131

    申请日:2000-11-29

    IPC分类号: C10G4720

    CPC分类号: C10G47/16 B01J29/166

    摘要: The invention relates to a hydrocracking catalyst comprising at least one amorphous or poorly crystallized matrix of the oxide type, at least one element of group VB, preferably niobium, and at least one zeolite Y not globally dealuminized, at least one promoter element chosen from the group consisting of boron, phosphorus and silicon, optionally at least one element chosen from the elements of group VIB and group VIII, optionally at least one element of group VIIA. The invention also relates to the use of this catalyst for hydrocracking hydrocarbon feeds.

    摘要翻译: 本发明涉及一种加氢裂化催化剂,其包含至少一种氧化物类型的无定形或不完全结晶的基质,VB族的至少一种元素,优选铌,以及至少一种未全面脱铝的沸石Y,至少一种选自 由硼,磷和硅组成的组,任选地至少一种选自VIB族和VIII族元素的元素,以及任选的至少一种VIIA族元素。 本发明还涉及该催化剂用于加氢裂化烃进料的用途。

    Hydrocracking catalyst comprising a beta zeolite and a group VB element
    6.
    发明授权
    Hydrocracking catalyst comprising a beta zeolite and a group VB element 有权
    包含β沸石和VB族元素的加氢裂化催化剂

    公开(公告)号:US06231750B1

    公开(公告)日:2001-05-15

    申请号:US09344344

    申请日:1999-06-25

    IPC分类号: C10G4706

    摘要: The invention provides a hydrocracking catalyst comprising at least one mineral matrix, at least one beta zeolite, at least one group VB element or at least one mixed sulphide phase comprising sulphur, optionally at least one group VIB or group VIII element, optionally at least one element selected from the group formed by silicon, boron or phosphorous, and optionally at least one group VIIA element.

    摘要翻译: 本发明提供一种加氢裂化催化剂,其包含至少一种矿物基质,至少一种β沸石,至少一种VB族元素或至少一种含硫混合物,任选至少一种VIB族或VIII族元素的混合硫化物,任选至少一种 元素选自由硅,硼或磷形成的基团,以及任选的至少一种VIIA族元素。

    Process for activation of catalysts with a nitrogenous compound and excess thionic compound the catalysts that is obtained and it use in hydroconversion
    9.
    发明授权
    Process for activation of catalysts with a nitrogenous compound and excess thionic compound the catalysts that is obtained and it use in hydroconversion 有权
    用含氮化合物和过量的硫辛酸化合物活化催化剂的方法,所得催化剂及其在加氢转化中的应用

    公开(公告)号:US06187708B1

    公开(公告)日:2001-02-13

    申请号:US09305285

    申请日:1999-05-05

    IPC分类号: B01J3720

    CPC分类号: B01J37/20 C10G47/12

    摘要: The invention relates to a process for the sulfurization of hydroconversion catalysts, whereby said catalyst contains at least one element of group VIII of the periodic table and optionally an element of group VI, whereby said metal is present in the oxide state. Said process comprises at least one stage that is carried out in a hydrotreatment zone in the presence of at least one thionic compound and at least one nitrogenous compound. This process is carried out in such a way that before the final sulfurization temperature is reached, at least 130% of the stoichiometric amount of sulfur that is necessary for complete sulfurization of the catalyst is injected in said catalyst.