摘要:
Methods for forming optical fiber preforms with low-index trenches are disclosed. According to one embodiment, the method includes depositing silica-based glass soot on a bait rod to form a low-index trench region of the optical fiber preform. The silica-based glass soot is deposited such that the low-index trench region has a first density. Thereafter a barrier layer having a second density greater than the first density is formed around the low-index trench region. Therafter, an overclad region is deposited around the barrier layer. The bait rod is then removed from a central channel of the trench-overclad assembly. A separate core assembly is inserted into the central channel. A down-dopant gas is then directed through the central channel of the trench-overclad assembly as the trench-overclad assembly is heated to dope the low-index trench region. The barrier layer prevents diffusion of the down-dopant from the low-index trench region into the overclad region.
摘要:
Methods for forming optical fiber preforms with low-index trenches are disclosed. According to one embodiment, the method includes depositing silica-based glass soot on a bait rod to form a low-index trench region of the optical fiber preform. The silica-based glass soot is deposited such that the low-index trench region has a first density. Thereafter a barrier layer having a second density greater than the first density is formed around the low-index trench region. Therafter, an overclad region is deposited around the barrier layer. The bait rod is then removed from a central channel of the trench-overclad assembly. A separate core assembly is inserted into the central channel. A down-dopant gas is then directed through the central channel of the trench-overclad assembly as the trench-overclad assembly is heated to dope the low-index trench region. The barrier layer prevents diffusion of the down-dopant from the low-index trench region into the overclad region.
摘要:
According to some embodiments a single mode fiber includes: a germania doped central core region having outer radius r1 and relative refractive index Δ1; and a cladding region comprising (i) a first inner cladding region having an outer radius r2>6 microns and relative refractive index Δ2 and 0.3≦r1/r2≦0.85; and (ii) a second inner cladding region having an outer radius r3>9 microns and comprising a minimum relative refractive index Δ3, wherein said second inner cladding region has at least one region with a relative refractive index delta that becomes more negative with increasing radius; and (iii) an outer cladding region surrounding the second inner cladding region and comprising relative refractive index Δ4, wherein Δ1>Δ2>Δ3, Δ3
摘要:
A method and an apparatus for making an optical fiber preform comprising the steps of (i) depositing a plurality of rods are deposited into an inner cavity of an apparatus; (ii) depositing particulate glass material in the inner cavity between the rods and the inner wall; and (iii) applying pressure against the particulate glass material to pressurize the particulate glass material against the plurality of rods.
摘要:
A method and an apparatus for making an optical fiber preform comprising the steps of (i) depositing a plurality of rods are deposited into an inner cavity of an apparatus; (ii) depositing particulate glass material in the inner cavity between the rods and the inner wall; and (iii) applying pressure against the particulate glass material to pressurize the particulate glass material against the plurality of rods.
摘要:
According to some embodiments a single mode fiber includes: a germania doped central core region having outer radius r1 and relative refractive index Δ1; and a cladding region comprising (i) a first inner cladding region having an outer radius r2>6 microns and relative refractive index Δ2 and 0.3≦r1/r2≦0.85; and (ii) a second inner cladding region having an outer radius r3>9 microns and comprising a minimum relative refractive index Δ3, wherein said second inner cladding region has at least one region with a relative refractive index delta that becomes more negative with increasing radius; and (iii) an outer cladding region surrounding the inner cladding region and comprising relative refractive index Δ4, wherein Δ1>Δ2>Δ3, Δ3
摘要:
An optical fiber comprising: a silica based core having a first index of refraction n1; and at least one silica based cladding surrounding the core, the at least one silica based cladding comprising index lowering non-periodic voids containing a gas, wherein at least 80% of said voids have a maximum cross-sectional dimension of less than 2000 nm, and the NA of the fiber layer situated immediately adjacent to and inside said at least one silica based cladding is at least 0.2.
摘要:
A method of forming a cladding portion of an optical fiber preform assembly includes positioning a glass core cane in a mold cavity and loading the mold cavity with silica glass soot. The silica glass soot is compressed in an axial direction as the vibratory energy is applied to the mold body to form a soot compact around the glass core cane, wherein the soot compact is the cladding portion of an optical fiber preform assembly and the glass core cane is a core portion of the optical fiber preform assembly.
摘要:
A method of forming a cladding portion of an optical fiber preform assembly includes positioning a glass core cane in a mold cavity and loading the mold cavity with silica glass soot. The silica glass soot is compressed in an axial direction as the vibratory energy is applied to the mold body to form a soot compact around the glass core cane, wherein the soot compact is the cladding portion of an optical fiber preform assembly and the glass core cane is a core portion of the optical fiber preform assembly.
摘要:
An optical fiber comprising: a silica based core having a first index of refraction n1; and at least one silica based cladding surrounding the core, the at least one silica based cladding comprising index lowering non-periodic voids containing a gas, wherein at least 80% of said voids have a maximum cross-sectional dimension of less than 2000 nm, and the NA of the fiber layer situated immediately adjacent to and inside said at least one silica based cladding is at least 0.2.