公开(公告)号:US07445846B2
公开(公告)日:2008-11-04
申请号:US11097434
申请日:2005-04-01
CPC分类号: C08L23/10 , B32B25/04 , B32B25/08 , B32B25/16 , B32B25/18 , B32B27/08 , B32B27/18 , B32B27/32 , B32B2250/02 , B32B2250/24 , B32B2270/00 , B32B2274/00 , B32B2307/546 , B32B2307/554 , B32B2307/558 , B32B2307/56 , B32B2307/746 , B32B2419/00 , B32B2479/00 , B32B2605/08 , C08L23/16 , C08L23/22 , Y10T428/3154 , Y10T428/31544 , Y10T428/31913 , Y10T428/31917 , Y10T428/31924 , Y10T428/31931 , Y10T428/31938 , C08L2666/06
摘要: A thermoplastic vulcanizate comprising a) a dynamically vulcanized rubber, b) a thermoplastic resin, and c) optionally a synthetic oil, where the thermoplastic vulcanizate is substantially devoid of mineral oils.
摘要翻译: 一种热塑性硫化橡胶,其包含a)动态硫化橡胶,b)热塑性树脂,和c)任选的合成油,其中热塑性硫化橡胶基本上不含矿物油。
-
公开(公告)号:US06790911B2
公开(公告)日:2004-09-14
申请号:US10329592
申请日:2002-12-26
IPC分类号: C08F800
CPC分类号: C08L53/02 , C08F297/04 , C08L23/0815 , C08L23/283 , C08L53/00 , C08L2312/04 , C08L2666/02 , C08L2666/04 , C08L2666/06
摘要: A thermoplastic vulcanizate prepared by dynamically vulcanizing a halogenated butyl rubber within a mixture that includes the halogenated butyl rubber and from about 10 to about 100 parts by weight of a crystalline thermoplastic resin per 100 parts by weight rubber, to thereby form a thermoplastic vulcanizate, where the thermoplastic resin includes a resin other than polyethylene, melt mixing the thermoplastic vulcanizate with about 5 to about 75 parts by weight of polyethylene resin per 100 parts by weight rubber, from about 3 to about 60 parts by weight of a tackifier per 100 parts by weight rubber, and from about 5 to about 250 parts by weight of a block copolymer containing at least the structure S-B/S-S per 100 parts by weight rubber, where the S block of the block copolymer has a glass transition temperature above about 25° C., the B/S block has a glass transition temperature below about 25° C., and the S content of the B/S block is from about 40 to about 60 percent by weight of said S/B block, the diene content of the total block copolymer is less than 40 weight percent, and the B/S block amount to at least 50 weight percent of the total block copolymer.
摘要翻译: 通过在包含卤化丁基橡胶的混合物中动态硫化卤化丁基橡胶和每100重量份橡胶约10至约100重量份的结晶热塑性树脂制备的热塑性硫化橡胶,从而形成热塑性硫化橡胶,其中 热塑性树脂包括除了聚乙烯之外的树脂,将热塑性硫化橡胶与每100重量份橡胶约5至约75重量份的聚乙烯树脂熔融混合,每100重量份约3至约60重量份的增粘剂 和约5至约250重量份的嵌段共聚物,其至少包含每100重量份橡胶中的结构SB / SS,其中嵌段共聚物的S嵌段具有高于约25℃的玻璃化转变温度 B / S块的玻璃化转变温度低于约25℃,B / S嵌段的S含量为约40至约60重量% f所述S / B嵌段,总嵌段共聚物的二烯含量小于40重量%,B / S嵌段占总嵌段共聚物的至少50重量%。
-