Activated carbon for use in electric double layer capacitor and method of producing the same
    1.
    发明授权
    Activated carbon for use in electric double layer capacitor and method of producing the same 失效
    用于双电层电容器的活性炭及其制造方法

    公开(公告)号:US06592838B1

    公开(公告)日:2003-07-15

    申请号:US09692281

    申请日:2000-10-19

    IPC分类号: C01B3100

    CPC分类号: H01G11/34 H01G11/24 Y02E60/13

    摘要: Activated carbon for use in an electric double layer capacitor which has at least activated carbon, electrolyte solution and a separator, the activated carbon having properties of: the total specific surface area of 1000 m2/g or larger; the pore volume distribution of 400 &mgr;l/g or larger for the pores larger than 12 Å and smaller than 40 Å in diameter and of 50 &mgr;l/g or larger for the pores larger than 40 Å in diameter; and the total pore volume of 1000 &mgr;l/g or smaller.

    摘要翻译: 活性炭用于具有至少活性炭,电解质溶液和隔膜的双电层电容器中,所述活性炭具有以下性质:总比表面积为1000m 2 / g以上; 直径大于直径小于40埃的孔的孔体积分布为400mul / g或更大,直径大于40埃的孔的孔体积分布为50mul / g以上; 总孔体积为1000mul / g以下。

    WOUND ELECTRIC DOUBLE-LAYER CAPACITOR
    2.
    发明申请
    WOUND ELECTRIC DOUBLE-LAYER CAPACITOR 有权
    电动双层电容器

    公开(公告)号:US20090310281A1

    公开(公告)日:2009-12-17

    申请号:US12065637

    申请日:2006-11-21

    IPC分类号: H01G9/155

    摘要: A wound electric double-layer capacitor suppresses electrochemical reaction on polarized electrode layers, reduces characteristic degradation, and has high reliability. The capacitor has a capacitor element formed by winding positive and negative electrodes with a separator interposed between them, a metal case for storing the capacitor element and an electrolyte for driving, and a sealing member for sealing an opening of the metal case. In the positive and negative electrodes, positive and negative electrode lead wires are coupled to exposed parts of current collectors having polarized electrode layers on their both surfaces, respectively. The negative electrode is wound at least one extra turn from the winding end of the positive electrode of the capacitor element, and hence a part where the polarized electrode layers formed in the negative electrode face each other through the separator is formed on the outermost periphery of the capacitor element.

    摘要翻译: 缠绕电双层电容器抑制极化电极层的电化学反应,降低特性劣化,并具有高可靠性。 电容器具有电容器元件,该电容器元件是通过将正极和负极之间夹有隔板而形成的,用于存储电容器元件的金属壳和用于驱动的​​电解质,以及用于密封金属壳的开口的密封构件。 在正极和负极中,正极和负极引线分别与两个表面上具有极化电极层的集电体的露出部分相连。 负极从电容器元件的正极的绕组端缠绕至少一个额外的匝,并且因此形成在负极中的极化电极层通过隔板彼此面对的部分形成在 电容器元件。

    ELECTRIC DOUBLE-LAYER CAPACITOR AND METHOD FOR MANUFACTURING THE SAME
    3.
    发明申请
    ELECTRIC DOUBLE-LAYER CAPACITOR AND METHOD FOR MANUFACTURING THE SAME 有权
    电双层电容器及其制造方法

    公开(公告)号:US20090122467A1

    公开(公告)日:2009-05-14

    申请号:US12300619

    申请日:2007-05-25

    IPC分类号: H01G9/155 H01G9/00

    摘要: In an electric double-layer capacitor, resistance of a polarizable electrode layer is reduced and gas generation inside a case is suppressed in an attempt to improve reliability. On that account, an electric double-layer capacitor is provided, which is obtained by housing in a case, together with a driving electrolyte, a capacitor element wound with a separator interposed between electrodes being paired anode and cathode electrodes in each of which polarizable electrode layers are formed on and lead wires are fixed to both sides of a current collector made of metallic foil, such that the polarizable electrode layers are opposed to each other. Further, an electric double-layer capacitor is provided in which the lead wire is fixed to a polarizable-electrode-layer-removed section on the electrode where the polarizable electrode layer has been removed, and an area of the polarizable-electrode-layer-removed section is not smaller than 1 and not larger than 2.0 when a project area of a portion where the lead wire is connected with the current collector is set to 1.

    摘要翻译: 在双电层电容器中,为了提高可靠性,可以降低极化电极层的电阻,并抑制气体产生。 因此,提供了一种双电层电容器,其通过壳体与驱动电解质一起容纳电容器元件而获得,所述电容器元件被插入电极之间的间隔件,所述电极元件设置在成对的阳极和阴极电极之间,其中每个极化电极 在金属箔的集电体的两侧固定引线,使可极化电极层相对。 此外,提供一种双电层电容器,其中引线固定到已去除可极化电极层的电极上的可极化电极层去除部分上,并且可极化电极层 - 当引线与集电器连接的部分的投影区域设定为1时,取出部分不小于1且不大于2.0。

    Electric double-layer capacitor and method for manufacturing the same
    4.
    发明授权
    Electric double-layer capacitor and method for manufacturing the same 有权
    双电层电容器及其制造方法

    公开(公告)号:US07706129B2

    公开(公告)日:2010-04-27

    申请号:US12300619

    申请日:2007-05-25

    IPC分类号: H01G9/00

    摘要: In an electric double-layer capacitor, resistance of a polarizable electrode layer is reduced and gas generation inside a case is suppressed in an attempt to improve reliability. On that account, an electric double-layer capacitor is provided, which is obtained by housing in a case, together with a driving electrolyte, a capacitor element wound with a separator interposed between electrodes being paired anode and cathode electrodes in each of which polarizable electrode layers are formed on and lead wires are fixed to both sides of a current collector made of metallic foil, such that the polarizable electrode layers are opposed to each other. Further, an electric double-layer capacitor is provided in which the lead wire is fixed to a polarizable-electrode-layer-removed section on the electrode where the polarizable electrode layer has been removed, and an area of the polarizable-electrode-layer-removed section is not smaller than 1 and not larger than 2.0 when a project area of a portion where the lead wire is connected with the current collector is set to 1.

    摘要翻译: 在双电层电容器中,为了提高可靠性,可以降低极化电极层的电阻,并抑制气体产生。 因此,提供了一种双电层电容器,其通过壳体与驱动电解质一起容纳电容器元件而获得,所述电容器元件被插入电极之间的间隔件,所述电极元件设置在成对的阳极和阴极电极之间,其中每个极化电极 在金属箔的集电体的两侧固定引线,使可极化电极层相对。 此外,提供一种双电层电容器,其中引线固定到已去除可极化电极层的电极上的可极化电极层去除部分上,并且可极化电极层 - 当引线与集电器连接的部分的投影区域设定为1时,取出部分不小于1且不大于2.0。

    ELECTRIC DOUBLE LAYER CAPACITOR
    5.
    发明申请
    ELECTRIC DOUBLE LAYER CAPACITOR 有权
    电双层电容器

    公开(公告)号:US20090231781A1

    公开(公告)日:2009-09-17

    申请号:US11994068

    申请日:2006-08-07

    IPC分类号: H01G9/155

    摘要: An electric double layer capacitor includes a first collector, a first polarizable electrode layer provided on the first collector, a second collector, a second polarizable electrode layer provided on the second collector and facing the first polarizable electrode layer, a separator having an insulating property and provided between the first polarizable electrode layer and the second polarizable electrode layer, and a driving electrolyte impregnated in the first polarizable electrode layer and the second polarizable electrode layer. The polarizable electrode layers mainly contain activated carbon made from phenol resin, have a surface roughness not larger than 0.6 μm, and have an electrode density ranging from 0.5 g/cm3 to 0.7 g/cm3. This electric double layer capacitor has characteristics deteriorating little even at low temperatures, thus having a reliability for a long time.

    摘要翻译: 双电层电容器包括:第一集电体,设置在第一集电极上的第一可极化电极层,第二集电体,设置在第二集电体上并面向第一可极化电极层的第二可极化电极层,具有绝缘性的隔膜; 设置在第一可极化电极层和第二可极化电极层之间,以及浸渍在第一可极化电极层和第二可极化电极层中的驱动电解质。 可极化电极层主要含有由酚醛树脂制成的活性炭,表面粗糙度不大于0.6μm,电极密度为0.5g / cm 3至0.7g / cm 3。 该双电层电容器即使在低温下也具有劣化的特性,因此具有长时间的可靠性。

    Material of case for storage cell
    6.
    发明申请
    Material of case for storage cell 有权
    储存盒的材料

    公开(公告)号:US20070065717A1

    公开(公告)日:2007-03-22

    申请号:US10577342

    申请日:2004-12-15

    IPC分类号: H01M2/02 C22C38/44

    摘要: There is provided a casing material for a storage cell having sufficient corrosion resistance and strength even under a charging environment of a high voltage exceeding 2.8 V. This casing material for the storage cell comprises C: not more than 0.03 mass %, Si: 0.01-0.50 mass %, Mn: not more than 0.20 mass %, P: not more than 0.04 mass %, S: not more than 0.0010 mass %, Ni: 20.0-40.0 mass %, Cr: 20.0-30.0 mass %, Mo: 5.0-10.0 mass %, Al: 0.001-0.10 mass %, N: 0.10-0.50 mass %, Ca: not more than 0.001 mass %, Mg: 0.0001-0.0050 mass %, 0: not more than 0.005 mass %, provided that contents of Cr, Mo and N satisfy Cr+3.3×Mo+20×N≧43, and the balance being substantially Fe and inevitable impurities, in which a content of CaO as an oxide inclusion in steel is not more than 20 mass %.

    摘要翻译: 即使在超过2.8V的高电压的充电环境下,也提供了具有足够的耐腐蚀性和强度的蓄电池的外壳材料。该蓄电池用外壳材料包括C:0.03质量%以下,Si:0.01〜 0.50质量%,Mn:0.20质量%以下,P:0.04质量%以下S:0.0010质量%以下Ni:20.0〜40.0质量%Cr:20.0〜30.0质量%Mo:5.0 -10.0质量%,Al:0.001-0.10质量%,N:0.10〜0.50质量%,Ca:0.001质量%以下,Mg:0.0001-0.0050质量%,0:0.005质量%以下, 的Cr,Mo和N满足Cr + 3.3xMo + 20xN> = 43,余量实质上为Fe和不可避免的杂质,其中钢中作为氧化物夹杂物的CaO含量不超过20质量%。

    Electric double layer capacitor
    7.
    发明授权
    Electric double layer capacitor 有权
    双电层电容器

    公开(公告)号:US08351182B2

    公开(公告)日:2013-01-08

    申请号:US11994068

    申请日:2006-08-07

    IPC分类号: H01G9/00

    摘要: An electric double layer capacitor includes a first collector, a first polarizable electrode layer provided on the first collector, a second collector, a second polarizable electrode layer provided on the second collector and facing the first polarizable electrode layer, a separator having an insulating property and provided between the first polarizable electrode layer and the second polarizable electrode layer, and a driving electrolyte impregnated in the first polarizable electrode layer and the second polarizable electrode layer. The polarizable electrode layers mainly contain activated carbon made from phenol resin, have a surface roughness not larger than 0.6 μm, and have an electrode density ranging from 0.5 g/cm3 to 0.7 g/cm3. This electric double layer capacitor has characteristics deteriorating little even at low temperatures, thus having a reliability for a long time.

    摘要翻译: 双电层电容器包括:第一集电体,设置在第一集电极上的第一可极化电极层,第二集电体,设置在第二集电体上并面向第一可极化电极层的第二可极化电极层,具有绝缘性的隔膜; 设置在第一可极化电极层和第二可极化电极层之间,以及浸渍在第一可极化电极层和第二极化电极层中的驱动电解质。 可极化电极层主要含有由酚醛树脂制成的活性炭,表面粗糙度不大于0.6μm,电极密度为0.5g / cm 3至0.7g / cm 3。 该双电层电容器即使在低温下也具有劣化的特性,因此具有长时间的可靠性。

    Wound electric double-layer capacitor
    8.
    发明授权
    Wound electric double-layer capacitor 有权
    绕线电双层电容器

    公开(公告)号:US07881043B2

    公开(公告)日:2011-02-01

    申请号:US12065637

    申请日:2006-11-21

    IPC分类号: H01G9/00

    摘要: A wound electric double-layer capacitor suppresses electrochemical reaction on polarized electrode layers, reduces characteristic degradation, and has high reliability. The capacitor has a capacitor element formed by winding positive and negative electrodes with a separator interposed between them, a metal case for storing the capacitor element and an electrolyte for driving, and a sealing member for sealing an opening of the metal case. In the positive and negative electrodes, positive and negative electrode lead wires are coupled to exposed parts of current collectors having polarized electrode layers on their both surfaces, respectively. The negative electrode is wound at least one extra turn from the winding end of the positive electrode of the capacitor element, and hence a part where the polarized electrode layers formed in the negative electrode face each other through the separator is formed on the outermost periphery of the capacitor element.

    摘要翻译: 缠绕电双层电容器抑制极化电极层的电化学反应,降低特性劣化,并具有高可靠性。 电容器具有电容器元件,该电容器元件是通过将正极和负极之间夹有隔板而形成的,用于存储电容器元件的金属壳和用于驱动的​​电解质,以及用于密封金属壳的开口的密封构件。 在正极和负极中,正极和负极引线分别与两个表面上具有极化电极层的集电体的露出部分相连。 负极从电容器元件的正极的绕组端缠绕至少一个额外的匝,并且因此形成在负极中的极化电极层通过隔板彼此面对的部分形成在 电容器元件。

    Material of case for storage cell
    9.
    发明授权
    Material of case for storage cell 有权
    储存盒的材料

    公开(公告)号:US07515395B2

    公开(公告)日:2009-04-07

    申请号:US10577342

    申请日:2004-12-15

    IPC分类号: H01G2/10 H01G9/08

    摘要: There is provided a casing material for a storage cell having sufficient corrosion resistance and strength even under a charging environment of a high voltage exceeding 2.8 V. This casing material for the storage cell comprises C: not more than 0.03 mass %, Si: 0.01-0.50 mass %, Mn: not more than 0.20 mass %, P: not more than 0.04 mass %, S: not more than 0.0010 mass %, Ni: 20.0-40.0 mass %, Cr: 20.0-30.0 mass %, Mo: 5.0-10.0 mass %, Al: 0.001-0.10 mass %, N: 0.10-0.50 mass %, Ca: not more than 0.001 mass %, Mg: 0.0001-0.0050 mass %, 0: not more than 0.005 mass %, provided that contents of Cr, Mo and N satisfy Cr+3.3×Mo+20×N≧43, and the balance being substantially Fe and inevitable impurities, in which a content of CaO as an oxide inclusion in steel is not more than 20 mass %.

    摘要翻译: 即使在超过2.8V的高电压的充电环境下,也提供了具有足够的耐腐蚀性和强度的蓄电池的外壳材料。该蓄电池用外壳材料包括C:0.03质量%以下,Si:0.01〜 0.50质量%,Mn:0.20质量%以下,P:0.04质量%以下S:0.0010质量%以下Ni:20.0〜40.0质量%Cr:20.0〜30.0质量%Mo:5.0 -10.0质量%,Al:0.001-0.10质量%,N:0.10〜0.50质量%,Ca:0.001质量%以下,Mg:0.0001-0.0050质量%,0:0.005质量%以下, 的Cr,Mo和N满足Cr + 3.3xMo + 20xN> = 43,余量实质上为Fe和不可避免的杂质,其中钢中作为氧化物夹杂物的CaO含量不超过20质量%。