GAS BARRIER FILM AND METHOD FOR PRODUCING THE SAME

    公开(公告)号:US20220411598A1

    公开(公告)日:2022-12-29

    申请号:US17899507

    申请日:2022-08-30

    Applicant: TOPPAN INC.

    Abstract: A gas barrier film comprising a resin base material, an oxygen barrier coating provided on at least one surface of the resin base material, and a base layer and/or an inorganic oxide layer provided between the resin base material and the oxygen barrier coating, wherein the black area ratio of one surface measured by the following measuring method is 0.15% or less: An arbitrary region of 1281 μm square on one surface of a resin base material is photographed with an optical microscope to acquire a photographed image of 1024×1024 pixels, the photographed image is converted into a monochrome image of 256 gradations using an image analysis software, and the value obtained by subtracting 30 from the most frequent value of the luminance in the monochrome image is set as the threshold, the value less than the threshold is set to black, and the value not less than the threshold is set to white, thus binarizing the luminance, and the ratio of the total area of the black regions having a size of 100 μm2 or more in the 1281 μm square region is defined as the black area ratio.

    GAS BARRIER LAMINATE AND PACKAGING BAG
    8.
    发明公开

    公开(公告)号:US20230356904A1

    公开(公告)日:2023-11-09

    申请号:US18246921

    申请日:2021-09-29

    Applicant: TOPPAN INC.

    CPC classification number: B65D65/40 B65D31/02 B65D2565/387

    Abstract: Provided is a gas barrier laminate being capable of hermetic sealing by heat sealing, and having a paper substrate and a vapor-deposited layer, in which the paper substrate has a basis weight of 30 to 100 g/m2, the water vapor transmission rate is 3 g/m2/d or less at 40° C. and 90%RH, the water vapor transmission rate obtained by folding the gas barrier laminate with the paper substrate placed on the outer side, rolling a roller having a weight of 2 kg thereon one time, opening a fold, and making measurement, is 4 g/m2/d or less at 40° C. and 90%RH, and the water vapor transmission rate obtained by folding the gas barrier laminate with the paper substrate placed on the inner side, rolling a roller having a weight of 2 kg thereon one time, opening a fold, and making measurement, is 4 g/m2/d or less at 40° C. and 90%RH.