公开(公告)号:US20230383118A1
公开(公告)日:2023-11-30
申请号:US18032416
申请日:2021-10-15
Applicant: TOYOBO CO., LTD.
Inventor: Kenzo OYA , Takuya AKAISHI , Eri MORIO
IPC: C08L67/02 , C08G63/183 , C08G63/66 , C08F212/08 , C08F220/32 , C08J9/00 , C08J9/34 , B29C44/00
CPC classification number: C08L67/025 , C08G63/183 , C08G63/66 , C08F212/08 , C08F220/325 , C08J9/0061 , C08J9/34 , B29C44/00 , C08L2207/04 , C08L2203/14 , C08L2201/08 , C08G2110/005 , C08G2101/00
Abstract: The present invention aims to provide a thermoplastic polyester elastomer resin composition suitable for foam molded product which exhibits light weight, excellent rebound resilience and excellent surface smoothness. The present invention provides a thermoplastic polyester elastomer resin composition for counter-pressure foam molding, containing a thermoplastic polyester elastomer and a thickener, wherein the thermoplastic polyester elastomer is prepared by bonding a hard segment and a soft segment, wherein the hard segment consists of polyester constituted from aromatic dicarboxylic acid and aliphatic and/or alicyclic diol as constituting components, wherein the soft segment is at least one member selected from a group consisting of aliphatic polyether, aliphatic polyester and aliphatic polycarbonate, wherein the thermoplastic polyester elastomer has a soft segment content of 25 to 90% by mass, and wherein a content of the thickener is 0.05 to 4.5 parts by mass relative to 100 parts by mass of the thermoplastic polyester elastomer. The present invention also provides a foam molded product that includes a continuous phase formed of the thermoplastic polyester elastomer resin composition.
-
公开(公告)号:US20230390975A1
公开(公告)日:2023-12-07
申请号:US18032279
申请日:2021-10-15
Applicant: TOYOBO CO., LTD.
Inventor: Kenzo OYA , Takuya AKAISHI , Eri MORIO
CPC classification number: B29C44/06 , B29C44/3403 , B29K2067/00
Abstract: The present invention is to provide a thermoplastic polyester elastomer resin foam molded product which exhibits light weight, excellent rebound resilience and excellent surface smoothness. A foam molded product including a continuous phase formed of a resin component containing a thermoplastic polyester elastomer, wherein the thermoplastic polyester elastomer is prepared by bonding a hard segment and a soft segment, wherein the hard segment consists of polyester constituted from aromatic dicarboxylic acid and aliphatic and/or alicyclic diol as constituting components, wherein the soft segment is at least one member selected from a group consisting of aliphatic polyether, aliphatic polyester and aliphatic polycarbonate, wherein the foam molded product is constituted from, as a surface layer ranging from a surface of the foam molded product to a depth of 1000 μm, a surface layer consisting of only a foamed region in which a non-foamed portion having a cell density of 10% or less is not present, or the foam molded product has, as a surface layer ranging from a surface of the foam molded product to a depth of 1000 μm, a surface layer consisting of both a foamed region in which the non-foamed portion is present and a foamed region in which the non-foamed portion is not present, and wherein the foam molded product has a density of 0.01 to 0.70 g/cm3.
-