Method of measuring the period of surface defects
    1.
    发明授权
    Method of measuring the period of surface defects 失效
    测量表面缺陷周期的方法

    公开(公告)号:US4982600A

    公开(公告)日:1991-01-08

    申请号:US405215

    申请日:1989-09-11

    摘要: To measure the period with which a surface defect recurs in a surface of a web-like material moving in its lengthwise direction, surface defects distributed over the surface are detected in that lengthwise direction. Positional data and distance data as to the detected surface defects relative to one another are collected for a predetermined length of the web-like material. The web-like material is determined to have a periodic surface defect appearing with a period between predetermined maximum and minimum periods when the distance data include a distance equivalent to an elemental period that is a whole-number multiple of a fundamental period.

    Method for electrolytic treatment
    3.
    发明授权
    Method for electrolytic treatment 失效
    电解处理方法

    公开(公告)号:US4536264A

    公开(公告)日:1985-08-20

    申请号:US652996

    申请日:1984-09-21

    摘要: A method for continuously electrolytically processing a metal web in which the consumption rate of graphite electrodes is remarkably reduced. Auxiliary anodes made of a nonreactive material are provided separately from the graphite electrodes. One half of a symmetrical waveform is applied directly between the graphite electrodes, while for the other half of the waveform, a portion of the current is distributed through the auxiliary anodes. In this manner, the magnitude of the current contributing to a cathode reaction on the surfaces of the graphite electrodes is made larger than the magnitude of the current contributing to an anode reaction on the surfaces of the graphite electrodes, thereby reducing the consumption rate of the graphite electrodes.

    摘要翻译: 一种连续电解处理金属网的方法,其中石墨电极的消耗率显着降低。 由非反应性材料制成的辅助阳极与石墨电极分开设置。 对称波形的一半直接施加在石墨电极之间,而对于波形的另一半,电流的一部分通过辅助阳极分布。 以这种方式,使有助于石墨电极表面上的阴极反应的电流的大小大于有助于石墨电极表面上的阳极反应的电流的大小,从而降低了 石墨电极。

    Method and apparatus for manufacturing sensitized printing plate
    4.
    发明授权
    Method and apparatus for manufacturing sensitized printing plate 失效
    敏化印版的制造方法及装置

    公开(公告)号:US06672193B2

    公开(公告)日:2004-01-06

    申请号:US09847350

    申请日:2001-05-03

    IPC分类号: B26D124

    摘要: A clearance between an upper knife and a lower knife of a slitter is set at 30 to 100 &mgr;m, and the slitter cuts a sensitized printing plate. In the sensitized printing plate cut by the slitter, there is a shear droop which is 20 to 30 &mgr;m high at the cut part, and a burr which is less than 50 &mgr;m high. If the maximum height of a surface roughness of a cut surface of the sensitized printing plate is 1.2 &mgr;m to 12 &mgr;m on the average, a hydrophilic property of the cut part improves and the stain of a frame can be decreased.

    摘要翻译: 分切机的上刀和下刀之间的间隙设定为30〜100um,切割机切割感光印版。 在由切割机切割的致敏印刷版中,在切割部分存在高度为20至30μm的剪切下垂和小于50μm的毛刺。 如果感光印版的切割面的表面粗糙度的最大高度平均为1.2μm〜12μm,则切割部的亲水性提高,并且可以降低框的污点。

    Method and apparatus for manufacturing sensitized printing plate
    5.
    发明授权
    Method and apparatus for manufacturing sensitized printing plate 失效
    敏化印版的制造方法及装置

    公开(公告)号:US06258410B1

    公开(公告)日:2001-07-10

    申请号:US09235296

    申请日:1999-01-22

    IPC分类号: B05D312

    摘要: A clearance between an upper knife and a lower knife of a slitter is set at 30 to 100 &mgr;m, and the slitter cuts a sensitized printing plate. In the sensitized printing plate cut by the slitter, there is a shear droop which is 20 to 30 &mgr;m high at the cut part, and a burr which is less than 50 &mgr;m high. If the maximum height of a surface roughness of a cut surface of the sensitized printing plate is 1.2 &mgr;m to 12 &mgr;m on the average, a hydrophilic property of the cut part improves and the stain of a frame can be decreased.