SEALING MATERIAL SHEET FOR SOLAR CELL MODULE AND A METHOD OF MANUFACTURING SOLAR CELL MODULE
    1.
    发明申请
    SEALING MATERIAL SHEET FOR SOLAR CELL MODULE AND A METHOD OF MANUFACTURING SOLAR CELL MODULE 审中-公开
    用于太阳能电池模块的密封材料片和制造太阳能电池模块的方法

    公开(公告)号:US20120184061A1

    公开(公告)日:2012-07-19

    申请号:US13498787

    申请日:2009-09-21

    IPC分类号: H01L31/18 C08L31/04 B32B7/02

    摘要: Disclosed are a sealing material sheet for a solar cell module and a method of manufacturing a solar cell module capable of reducing damage to a photoelectric conversion cell and leakage of a sealing material during manufacturing of a solar cell module, and easily manufacturing a high-quality solar cell module. A sealing material sheet for a solar cell module includes transparent resin (A) exhibiting an MFR (190° C., 2.16 kg load) of 10 to 20 g/10 min and transparent resin (B) exhibiting an MFR (190° C., 2.16 kg load) of 30 to 40 g/10 min. The mass ratio α (=WA/WB) of the transparent resin (A) (mass: WA) and the transparent resin (B) (mass: WB) is 0.7 to 1.5. A solar cell module uses the sealing material sheet for a solar cell module.

    摘要翻译: 公开了一种用于太阳能电池模块的密封材料片和一种太阳能电池模块的制造方法,该太阳能电池模块能够减少光电转换元件的损坏,并且在制造太阳能电池模块期间密封材料的泄漏,并且容易地制造高品质 太阳能电池模块 用于太阳能电池组件的密封材料片包括表现出MFR(190℃,2.16kg负载)为10-20g / 10min的透明树脂(A)和MFR(190℃)的透明树脂(B) ,2.16kg负荷)为30〜40g / 10min。 透明树脂(A)(质量:WA)和透明树脂(B)(质量:WB)的质量比α(= WA / WB)为0.7〜1.5。 太阳能电池组件使用太阳能电池模块的密封材料片。

    Antiglare film and transmissive liquid crystal display
    2.
    发明申请
    Antiglare film and transmissive liquid crystal display 有权
    防盗胶片和透射液晶显示屏

    公开(公告)号:US20090002832A1

    公开(公告)日:2009-01-01

    申请号:US12001922

    申请日:2007-12-12

    IPC分类号: G02B5/02

    摘要: An antiglare film satisfies both (1) high antiglare property in the front direction and (2) absence of white blurring. One embodiment of the invention is an antiglare film provided with an antiglare layer on a transparent substrate, wherein the antiglare layer has a rugged structure on the surface opposite to the transparent substrate; the 5° reflectance of the antiglare film surface on the antiglare layer side is in a range of from 0.30% to 0.70%; the antiglare film surface on the antiglare layer side is provided with a rugged structure having arithmetic average roughness (Ra1) in the range of from 0.020 μm to 0.040 μm when a cutoff wavelength (λC) is 0.008 mm; and the antiglare film surface on the antiglare layer side is provided with a rugged structure having arithmetic average roughness (Ra2) in the range of from 0.35 μm to 0.45 μm when a cutoff wavelength (c) is 0.8 mm.

    摘要翻译: 防眩膜满足(1)前方的高防眩性和(2)不存在白色模糊。 本发明的一个实施例是在透明基板上设有防眩层的防眩膜,其中防眩层在与透明基板相对的表面上具有凹凸的结构; 防眩层侧的防眩膜表面的5°反射率在0.30%〜0.70%的范围内; 当防眩层一侧的防眩膜表面设置有当截止波长(λC)为0.008mm时算术平均粗糙度(Ra1)在0.020μm至0.040μm的范围内的凹凸结构; 并且当防眩层一侧的防眩膜表面设置有当截止波长(c)为0.8mm时算术平均粗糙度(Ra2)在0.35μm至0.45μm的范围内的凹凸结构。

    Antiglare film
    3.
    发明申请
    Antiglare film 审中-公开
    防盗片

    公开(公告)号:US20080213513A1

    公开(公告)日:2008-09-04

    申请号:US11899900

    申请日:2007-09-06

    IPC分类号: C09K19/00 B32B5/16

    摘要: The present invention includes an antiglare film including an antiglare layer which layer includes a silica particle and a binder matrix, wherein refractive index of the silica particle is 1.46-1.50, wherein the silica particle is an amorphous silica which includes an aggregate of fine silica particles, wherein average particle diameter of the silica fine particles is 0.003-0.1 μm, wherein average particle diameter of the silica particle is 1.0-3.0 μm, wherein the binder matrix is formed by curing a binder matrix curable material with ionizing radiation, and wherein the binder matrix curable material includes trifunctional acrylic monomer and tetrafunctional acrylic monomer of 80 part by weight or more based on a binder matrix forming material of 100 part by weight.

    摘要翻译: 本发明包括防眩光膜,该防眩光层包括二氧化硅颗粒层和粘合剂基质层,其中二氧化硅颗粒的折射率为1.46-1.50,其中二氧化硅颗粒是无定形二氧化硅,其包括二氧化硅微粒的聚集体 其中,所述二氧化硅微粒的平均粒径为0.003〜0.1μm,其中,所述二氧化硅粒子的平均粒径为1.0〜3.0μm,其中,所述粘合剂基体是通过用电离辐射固化粘合剂基质固化性材料形成的, 粘合剂基质可固化材料包括基于形成100重量份的粘合剂基质的三官能丙烯酸单体和80重量份以上的四官能丙烯酸单体。

    Antiglare Film
    4.
    发明申请
    Antiglare Film 有权
    防盗片

    公开(公告)号:US20090244708A1

    公开(公告)日:2009-10-01

    申请号:US12405951

    申请日:2009-03-17

    IPC分类号: G02B1/11 G02B1/10 C08F2/46

    摘要: This invention provides an antiglare film which has high antiglare property and show little white-blurring. An embodiment of the present invention is an antiglare film having a binder matrix and particles on a transparent substrate. The binder matrix is an acrylic material. The particles are made of a copolymer of styrene and methyl methacrylate. The copolymerization ratio by weight of the styrene and methyl methacrylate is in the styrene:methacrylic acid=60:40 to 80:20 range. In addition, a quotient R/H, which is obtained by dividing an average diameter of the particles (R) by the average thickness of the antiglare layer (H), is in the 0.45-0.65 range. Moreover, a quotient wP/wB, which is obtained by dividing a content of the particles in the antiglare layer (wP) by a content of the binder matrix in the antiglare layer (wB) is in the 0.08-0/164.

    摘要翻译: 本发明提供一种抗眩光性好,白色模糊少的防眩膜。 本发明的一个实施方案是在透明基材上具有粘合剂基质和颗粒的防眩膜。 粘合剂基质是丙烯酸材料。 颗粒由苯乙烯和甲基丙烯酸甲酯的共聚物制成。 苯乙烯和甲基丙烯酸甲酯的共聚比例为苯乙烯:甲基丙烯酸= 60:40〜80:20。 此外,通过将颗粒(R)的平均直径除以防眩光层(H)的平均厚度获得的商R / H在0.45-0.65范围内。 此外,通过将防眩层(wP)中的颗粒的含量除以防眩层(wB)中的粘合剂基质的含量获得的商wP / wB为0.08-0 / 164。

    Antiglare Film
    5.
    发明申请
    Antiglare Film 有权
    防盗片

    公开(公告)号:US20090096972A1

    公开(公告)日:2009-04-16

    申请号:US12246424

    申请日:2008-10-06

    IPC分类号: G02F1/1335 G02B1/11

    CPC分类号: G02B1/111 G02F1/133502

    摘要: An antiglare film includes an antiglare layer having a binder matrix, and particles A and particles B therein on a transparent substrate. A difference in density between the particles A and particles B is 0.2 g/cm3 or less. The quotient value (RA/H), which is obtained by division of the average diameter of the particles A (RA) by the average thickness of the antiglare layer (H), is in the 0.40-0.80 range. The quotient value (RB/RA), which is obtained by division of the average diameter of the particles B (RB) by the average diameter of the particles A (RA), is in the 0.20-0.60 range. The quotient value ((wA+wB)/wM), which is obtained by dividing the sum of the content of the particles A (wA) and that of the particles B (wB) in the antiglare layer (wA+wB) by the content of the binder matrix in the antiglare layer (wM), is in the 0.10-0.40 range. The quotient value (wB/wA), which is obtained by division of the content of the particles B (wB) by that of the particles A (wA) in the antiglare layer, is in the 0.50-1.50 range.

    摘要翻译: 防眩膜包括具有粘合剂基质的防眩层,在其上的颗粒A和颗粒B在透明基材上。 颗粒A和颗粒B之间的密度差为0.2g / cm 3以下。 通过将颗粒A(RA)的平均直径除以防眩光层(H)的平均厚度而得到的商值(RA / H)在0.40-0.80范围内。 通过将颗粒B(RB)的平均直径除以颗粒A(RA)的平均直径而得到的商值(RB / RA)在0.20-0.60范围内。 通过将防眩层(wA + wB)中的颗粒A(wA)和颗粒B(wB)的含量的总和除以所得到的商值((wA + wB)/ wM) 防眩层(wM)中的粘合剂基质的含量为0.10-0.40。 通过将颗粒B(wB)的含量除以防眩层中的颗粒A(wA)的含量获得的商值(wB / wA)为0.50-1.50的范围。

    Antiglare film
    6.
    发明申请
    Antiglare film 有权
    防盗片

    公开(公告)号:US20080212005A1

    公开(公告)日:2008-09-04

    申请号:US11899651

    申请日:2007-09-06

    IPC分类号: G02B1/11 G02F1/1333

    摘要: An antiglare film is disclosed comprising a transparent substrate and an antiglare layer including a binder matrix and a particle, wherein center line average roughness Ra of a surface of an antiglare film which surface is on an antiglare layer side among both sides of an antiglare film is 0.06-0.17 μm, wherein reflectivity of 5° angle of the surface is 2.4-4.4%, and wherein difference in refractive index between the binder matrix and the particle is equal to or less than 0.07.

    摘要翻译: 公开了一种防眩膜,其包括透明基材和包含粘合剂基质和颗粒的防眩光层,其中防眩膜两面之间的防眩光层表面的防眩光膜表面的中心线平均粗糙度Ra为 0.06-0.17μm,其中表面的5°角的反射率为2.4-4.4%,其中粘合剂基质和颗粒之间的折射率差等于或小于0.07。

    Antiglare film
    7.
    发明授权
    Antiglare film 有权
    防盗片

    公开(公告)号:US08163383B2

    公开(公告)日:2012-04-24

    申请号:US12405951

    申请日:2009-03-17

    IPC分类号: B32B5/16 B05D3/02

    摘要: This invention provides an antiglare film which has high antiglare property and show little white-blurring. An embodiment of the present invention is an antiglare film having a binder matrix and particles on a transparent substrate. The binder matrix is an acrylic material. The particles are made of a copolymer of styrene and methyl methacrylate. The copolymerization ratio by weight of the styrene and methyl methacrylate is in the styrene:methacrylic acid=60:40 to 80:20 range. In addition, a quotient R/H, which is obtained by dividing an average diameter of the particles (R) by the average thickness of the antiglare layer (H), is in the 0.45-0.65 range. Moreover, a quotient wP/wB, which is obtained by dividing a content of the particles in the antiglare layer (wP) by a content of the binder matrix in the antiglare layer (wB) is in the 0.08-0/164.

    摘要翻译: 本发明提供一种抗眩光性好,白色模糊少的防眩膜。 本发明的一个实施方案是在透明基材上具有粘合剂基质和颗粒的防眩膜。 粘合剂基质是丙烯酸材料。 颗粒由苯乙烯和甲基丙烯酸甲酯的共聚物制成。 苯乙烯和甲基丙烯酸甲酯的共聚比例为苯乙烯:甲基丙烯酸= 60:40〜80:20。 此外,通过将颗粒(R)的平均直径除以防眩光层(H)的平均厚度获得的商R / H在0.45-0.65范围内。 此外,通过将防眩层(wP)中的颗粒的含量除以防眩层(wB)中的粘合剂基质的含量获得的商wP / wB为0.08-0 / 164。

    Antiglare film having first and second particles with different average diameters
    8.
    发明授权
    Antiglare film having first and second particles with different average diameters 有权
    防斜纹薄膜具有不同平均直径的第一和第二颗粒

    公开(公告)号:US07973895B2

    公开(公告)日:2011-07-05

    申请号:US12246424

    申请日:2008-10-06

    IPC分类号: G02F1/1335 G02B27/00

    CPC分类号: G02B1/111 G02F1/133502

    摘要: An antiglare film includes an antiglare layer having a binder matrix, and particles A and particles B therein on a transparent substrate. A difference in density between the particles A and particles B is 0.2 g/cm3 or less. The quotient value (RA/H), which is obtained by division of the average diameter of the particles A (RA) by the average thickness of the antiglare layer (H), is in the 0.40-0.80 range. The quotient value (RB/RA), which is obtained by division of the average diameter of the particles B (RB) by the average diameter of the particles A (RA), is in the 0.20-0.60 range. The quotient value ((wA+wB)/wM), which is obtained by dividing the sum of the content of the particles A (wA) and that of the particles B (wB) in the antiglare layer (wA+wB) by the content of the binder matrix in the antiglare layer (wM), is in the 0.10-0.40 range. The quotient value (wB/wA), which is obtained by division of the content of the particles B (wB) by that of the particles A (wA) in the antiglare layer, is in the 0.50-1.50 range.

    摘要翻译: 防眩膜包括具有粘合剂基质的防眩层,在其上的颗粒A和颗粒B在透明基材上。 颗粒A和颗粒B之间的密度差为0.2g / cm 3以下。 通过将颗粒A(RA)的平均直径除以防眩光层(H)的平均厚度而得到的商值(RA / H)在0.40-0.80范围内。 通过将颗粒B(RB)的平均直径除以颗粒A(RA)的平均直径而得到的商值(RB / RA)在0.20-0.60范围内。 通过将防眩层(wA + wB)中的颗粒A(wA)和颗粒B(wB)的含量的总和除以所得到的商值((wA + wB)/ wM) 防眩层(wM)中的粘合剂基质的含量为0.10-0.40。 通过将颗粒B(wB)的含量除以防眩层中的颗粒A(wA)的含量获得的商值(wB / wA)为0.50-1.50的范围。

    Antiglare film
    9.
    发明授权
    Antiglare film 有权
    防盗片

    公开(公告)号:US07839474B2

    公开(公告)日:2010-11-23

    申请号:US12202128

    申请日:2008-08-29

    IPC分类号: G02F1/1335 B32B5/16

    摘要: An antiglare film includes an antiglare layer having particles and a binder matrix on a transparent base material. An antiglare film surface on the antiglare layer side has a concave-convex structure with a ten-point average roughness (Rz1) equal to or larger than 0.08 μm and equal to or smaller than 0.10 μm at a cutoff wavelength (λc) of 0.008 mm, the antiglare film surface on the antiglare layer side has a concave-convex structure with a ten-point average roughness (Rz2) equal to or larger than 1.90 μm and equal to or smaller than 2.50 μm at a cutoff wavelength (λc) of 0.8 mm, and the antiglare film surface on the antiglare layer side has a concave-convex structure with an average spacing (S) between local peaks equal to or larger than 0.033 mm and equal to or smaller than 0.050 mm at a cutoff wavelength (λc) of 0.8 mm.

    摘要翻译: 防眩膜包括在透明基材上具有颗粒和粘合剂基质的防眩层。 防眩层一侧的防眩膜表面具有在0.008mm的截止波长(λc)下具有等于或大于0.08μm且等于或小于0.10μm的十点平均粗糙度(Rz1)的凹凸结构 ,防眩层侧的防眩膜表面具有在截止波长(λc)为0.8时具有等于或大于1.90μm且等于或小于2.50μm的十点平均粗糙度(Rz2)的凹凸结构 mm,防眩层侧的防眩膜表面具有在截止波长(λc)下在局部峰值等于或大于0.033mm且等于或小于0.050mm的平均间隔(S)的凹凸结构, 为0.8mm。

    Antiglare film
    10.
    发明授权
    Antiglare film 有权
    防盗片

    公开(公告)号:US07542118B2

    公开(公告)日:2009-06-02

    申请号:US11899651

    申请日:2007-09-06

    IPC分类号: G02F1/1335 G02B27/00 G02B1/11

    摘要: An antiglare film is disclosed comprising a transparent substrate and an antiglare layer including a binder matrix and a particle, wherein center line average roughness Ra of a surface of an antiglare film which surface is on an antiglare layer side among both sides of an antiglare film is 0.06-0.17 μm, wherein reflectivity of 5° angle of the surface is 2.4-4.4%, and wherein difference in refractive index between the binder matrix and the particle is equal to or less than 0.07.

    摘要翻译: 公开了一种防眩膜,其包括透明基材和包含粘合剂基质和颗粒的防眩光层,其中防眩光膜两侧的防眩光层表面的防眩光膜表面的中心线平均粗糙度Ra为 0.06-0.17μm,其中表面的5°角的反射率为2.4-4.4%,其中粘合剂基质和颗粒之间的折射率差等于或小于0.07。