摘要:
The invention relates to a method for separating transition metals from polymers. According to the invention, a solid polymer containing transition metals is treated with an extracting agent, the duration of the treatment and the extraction temperature being selected in such a way that the transition metal content is reduced by at least 30 wt. %.
摘要:
A reactive mixture for coating mouldings by means of reaction injection moulding, containing at least 40% by weight of (meth)acrylates having at least two double bonds. The reactive mixture contains at least one photoinitiator and at least one thermal initiator. The present invention furthermore describes a coated moulding including a moulding which is obtainable by injection moulding processes and includes at least one polymer selected from polymethyl methacrylate, polymethylmethacrylimide, styrene-acrylonitrile copolymer, styrene-maleic acid copolymer and polymethyl methacrylate copolymers, and a coating which is obtainable by polymerization of (meth)acrylates having at least two double bonds. The coating has an adhesive strength rating of not more than 1 according to the cross hatch test and a decrease in gloss at 20° after a scratch resistance test according to ASTM 1044 (12/05) (applied weight 500 g, number of cycles=100) of not more than 10%.
摘要:
A reactive mixture for coating mouldings by means of reaction injection moulding, containing at least 40% by weight of (meth)acrylates having at least two double bonds. The reactive mixture contains at least one photoinitiator and at least one thermal initiator. The present invention furthermore describes a coated moulding including a moulding which is obtainable by injection moulding processes and includes at least one polymer selected from polymethyl methacrylate, polymethylmethacrylimide, styrene-acrylonitrile copolymer, styrene-maleic acid copolymer and polymethyl methacrylate copolymers, and a coating which is obtainable by polymerization of (meth)acrylates having at least two double bonds. The coating has an adhesive strength rating of not more than 1 according to the cross hatch test and a decrease in gloss at 20° after a scratch resistance test according to ASTM 1044 (12/05) (applied weight 500 g, number of cycles=100) of not more than 10%.
摘要:
The invention relates to an injection moulding machine containing a reactive mixture including at least 40% by weight of (meth)acrylates having at least two double bonds, at least one photoinitiator, and at least one thermal initiator.
摘要:
The invention relates to a flameproof PMMA moulding material, mouldings produced therefrom and the use thereof. Small amounts of an organo-phosphorus compound are sufficient to increase the glow wire flammability index by 300° C.
摘要:
A reactive mixture for coating moldings by reaction injection molding includes at least 40% by weight of (meth)acrylates having at least two double bonds. The reactive mixture also includes at least one photoinitiator and at least one thermal initiator. Furthermore, a coated molding includes a molding obtainable by injection molding processes. The molding includes polymethyl methacrylate, polymethylmethacrylimide, styrene-acrylonitrile copolymer, styrene-maleic acid copolymer, polymethyl methacrylate copolymer, or a combination thereof. A coating is obtainable by polymerization of (meth)acrylates having at least two double bonds, the coating having an adhesive strength rating of not more than 1 according to the cross hatch test and a decrease in gloss at 20° after a scratch resistance test according to ASTM 1044 (12/05) (applied weight 500 g, number of cycles=100) of not more than 10%.
摘要:
The invention relates to a method for separating transition metals from polymers. According to the invention, a solid polymer containing transition metals is treated with an extracting agent, the duration of the treatment and the extraction temperature being selected in such a way that the transition metal content is reduced by at least 30 wt. %.
摘要:
A reactive mixture for coating moldings by reaction injection molding includes at least 40% by weight of (meth)acrylates having at least two double bonds. The reactive mixture also includes at least one photoinitiator and at least one thermal initiator. Furthermore, a coated molding includes a molding obtainable by injection molding processes. The molding includes polymethyl methacrylate, polymethylmethacrylimide, styrene-acrylonitrile copolymer, styrene-maleic acid copolymer, polymethyl methacrylate copolymer, or a combination thereof. A coating is obtainable by polymerization of (meth)acrylates having at least two double bonds, the coating having an adhesive strength rating of not more than 1 according to the cross hatch test and a decrease in gloss at 20° after a scratch resistance test according to ASTM 1044 (12/05) (applied weight 500 g, number of cycles=100) of not more than 10%.
摘要:
The present invention relates to a reactive mixture for coating mouldings by means of reaction injection moulding, comprising at least 40% by weight of (meth)acrylates having at least two double bonds, the reactive mixture comprising at least one photoinitiator and at least one thermal initiator.The present invention furthermore describes a coated moulding comprising a moulding which is obtainable by injection moulding processes and comprises at least one polymer selected from the group consisting of polymethyl methacrylate, polymethylmethacrylimide, styrene-acrylonitrile copolymer, styrene-maleic acid copolymer and polymethyl methacrylate copolymers, and a coating which is obtainable by polymerization of (meth)acrylates having at least two double bonds, the coating having an adhesive strength rating of not more than 1 according to the cross hatch test and a decrease in gloss at 20° after a scratch resistance test according to ASTM 1044 (12/05) (applied weight 500 g, number of cycles=100) of not more than 10%.