摘要:
A method of fabricating a multi-element magnetic head core is provided in which a plurality of first grooves are formed in a surface of a magnetic block to form a plurality of magnetic circuits, a plurality of second grooves are formed in this surface in directions perpendicular to the first grooves to separate the magnetic circuits from each other, the first and second grooves are filled with a non-magnetic material, the magnetic block is then cut along lines parallel to the second grooves to obtain a plurality of core blocks, and a third groove is formed in each core block from a side wall thereof to isolate the magnetic circuits completely from each other. According to this method, the number of fabrication steps required for forming a multi-element magnetic head core can be reduced, and moreover a multiplicity of magnetic head cores can be formed at the same time.
摘要:
A method of fabricating a thin-film magnetic in which a mask pattern in etching a bottom pole is formed of first and second mask films in this order when viewed from the bottom pole, the first mask film is used for defining, by self-alignment, the length of that portion of the side edge of a top pole which is nearly perpendicular to a magnetic gap, the second mask film makes it possible to etch the bottom pole with high dimensional accuracy, a non-magnetic film is formed on the mask pattern having the bottom pole thereunder and the exposed region of a substrate, and the top pole is formed after the mask pattern has been exposed and removed.
摘要:
A magnetic head element has one or more rails formed on the surface thereof. Each rail is formed so as to have a tapered angle of 55.degree.-85.degree.. To form such a rail, ion milling is conducted; the rail substrate used is allowed to have an inclination angle to 15.degree.-60.degree. and is rotated; and there is used, as the ion milling gas, a fluorinated hydrocarbon (e.g. CH.sub.2 FCF.sub.3) gas alone or a mixed gas of said fluorinated hydrocarbon gas and Ar, SF.sub.6 or the like. Accordingly, a magnetic head rail shape gives a small variation in flying height between magnetic head and magnetic disc.
摘要:
A magnetic head element has one or more rails formed on the surface thereof. Each rail is formed so as to have a tapered angle of 55-85°. To form such a rail, ion milling is conducted; the rail substrate used is allowed to have an inclination angle to 15-60° and is rotated; and there is used, as the ion milling gas, a fluorinated hydrocarbon (e.g., CH2FCF3) gas alone or a mixed gas of said fluorinated hydrocarbon gas and Ar, SF6 or the like. Accordingly, a magnetic head rail shape gives a small variation in flying height between magnetic bead and magnetic disc.
摘要:
A fine grain milling method which mixes powder into a high-pressure fluid, and injects the mixture to a workpiece covered with a mask or pattern to process the workpiece to a desired shape. Another high-pressure fluid is injected to remove the powder adhering to the workpiece thereby enabling an accurate transfer of the mask or pattern to the workpiece.
摘要:
A fine grain milling method mixes powder into a high-pressure fluid, and injects the mixture to a work material covered with a mask to form the work material to a desired shape. In addition, the method injects anther high-pressure fluid to the powder adhered to the work material to remove the powder. The method can accurately transfer the mask pattern to the work material.
摘要:
A magnetic head element has one or more rails formed on the surface thereof. Each rail is formed so as to have a tapered angle of 55-85.degree.. To form such a rail, ion milling is conducted; the rail substrate used is allowed to have an inclination angle to 15-60.degree. and is rotated; and there is used, as the ion milling gas, a fluorinated hydrocarbon (e.g., CH.sub.2 FCF.sub.3) gas alone or a mixed gas of said fluorinated hydrocarbon gas and Ar, SF.sub.6 or the like. Accordingly, a magnetic head rail shape gives a small variation in flying height between magnetic head and magnetic disc.
摘要:
A thin film magnetic head comprising a sintered ceramic substrate, an underlayer, a bottom magnetic core film, a magnetic gap film, an insulating film containing coil windings, a top magnetic core film, and a protective layer. The substrate and other films and layers form an air bearing surface. The under layer, the magnetic gap film and the protective layer comprise Al.sub.2 O.sub.3, and the bottom and the top magnetic core films comprise Ni--Fe alloy. This structure gives substantially the same etching rate, when the air bearing surface is polished using a working fluid of pH 6-8, for any of the substrate, the films comprising Al.sub.2 O.sub.3 and metal oxide described above, and the films of Ni--Fe alloy. Thus, steps (pole top recessions) on the air bearing surface can be made as small as 0.015 .mu.m or less. Accordingly, the magnetic head can be held in a stable attitude, thus obtaining good recording characteristics.
摘要翻译:一种薄膜磁头,包括烧结陶瓷衬底,底层,底部磁芯膜,磁隙膜,含有线圈绕组的绝缘膜,顶部磁芯膜和保护层。 衬底和其它膜和层形成空气轴承表面。 底层,磁隙膜和保护层包括Al2O3,底部和顶部磁芯膜包括Ni-Fe合金。 当使用pH6-8的工作流体对任何基板,包含上述Al 2 O 3和金属氧化物的膜以及Ni-Fe合金膜进行抛光时,该结构基本上具有相同的蚀刻速率 。 因此,空气轴承表面上的台阶(极顶部凹陷)可以制成小至0.015μm或更小。 因此,可以将磁头保持在稳定的姿态,从而获得良好的记录特性。
摘要:
A thin-film magnetic head has a first ferrite block on which a plurality of transducing elements are aligned on a predetermined surface, and a second ferrite block bonded to the first ferrite block, and has multi-track capabilities in accordance with the transducing elements. Eithr bonding surface of the first and second ferrite block is formed with an insulating film layer, the entire bonding surface is coated with an adhesive or formed with a plurality of recesses to be externally filled with the adhesive, and the adhesive is filled in gaps defined by the recesses and the surface of the opposed ferrite block. Thus, since the bonding portions of the first and second ferrite blocks are distributed over a wide region, the bonding strength can be largely increased, the transducing gap lengths are uniformly maintained, and the transducing element characteristic is not affected by the aging of the adhesive thereby improving the reliability of the magnetic head.