CPC分类号: B32B27/12 , B32B5/18 , B32B5/245 , B32B27/065 , B32B27/308 , B32B27/40 , B32B2266/0278 , B32B2270/00 , B32B2307/536 , B32B2437/00 , B32B2601/00 , B32B2605/003 , C08G2101/0008 , C08G2101/005 , C08G2170/20 , C08L75/08 , Y10S428/904 , Y10T428/24355 , Y10T428/24364 , Y10T428/24405 , Y10T428/24438 , Y10T428/24479 , Y10T428/24521 , Y10T428/249953 , Y10T428/249958 , Y10T428/249987 , Y10T428/249991 , Y10T428/31551 , Y10T428/31573 , Y10T442/2352 , Y10T442/3325 , Y10T442/3366 , Y10T442/469 , Y10T442/647 , Y10T442/652 , C08L33/12
摘要: The present invention provides a surface material which can be replaced to the conventional surface material made of soft polyvinylchloride resin. This surface material is useful for the various uses such as the material for car interior, surface material furniture or the material for porches. The present invention is the urethane resin surface material comprising, a mixed resin sheet composed of 50-95 wt. % thermoplastic polyurethane and 50-5 wt. % of acrylic soft resin and the Shore A hardness of said urethane resin surface material is 60-80. On one side surface of the mixed resin sheet, a layer of knitted, woven, nonwoven fabric or soft foam sheet can be provided. As the thermoplastic polyurethane resin, the thermoplastic polyurethane resin of Shore A hardness 65-90 is desirable, and as the acrylic soft resin, the acrylic soft resin of Shore A hardness 50-80 is desirable.
摘要翻译: 本发明提供一种表面材料,可以用由柔性聚氯乙烯树脂制成的常规表面材料代替。 该表面材料可用于各种用途,例如用于汽车内饰,表面材料家具或用于门廊的材料的材料。 本发明是一种聚氨酯树脂表面材料,包括:由50-95重量% %热塑性聚氨酯和50-5wt。 丙烯酸软树脂的%和所述聚氨酯树脂表面材料的肖氏A硬度为60-80。 在混合树脂片的一个侧表面上,可以提供编织,编织,非织造织物或软泡沫片层。 作为热塑性聚氨酯树脂,肖氏A硬度为65-90的热塑性聚氨酯树脂是理想的,作为丙烯酸软树脂,肖氏A硬度为50-80的丙烯酸类软质树脂是理想的。