Method to produce nanoporous polymeric membranes
    5.
    发明授权
    Method to produce nanoporous polymeric membranes 有权
    制备纳米多孔聚合物膜的方法

    公开(公告)号:US09203070B2

    公开(公告)日:2015-12-01

    申请号:US14213112

    申请日:2014-03-14

    CPC classification number: H01M2/145 H01M2/1653

    Abstract: A method for making a flat polymer foam having a core layer of nano-sized open, interconnected cells that includes saturating a solid-state polymer with a supercritical fluid, allowing the gas to desorb for at least 35 minutes, and then heating the gas-saturated solid polymer for at least 3 minutes while constraining the foam in the thickness dimension. Any skin layer formed on the exterior may be removed via polishing, thus creating a foam with an open structure from side to side. The foam can be used as a battery separator.

    Abstract translation: 一种制备扁平聚合物泡沫的方法,其具有纳米尺寸的开放互连电池的核心层,其包括用超临界流体使固态聚合物饱和,允许气体解吸至少35分钟,然后加热气 - 饱和固体聚合物至少3分钟,同时限制泡沫体的厚度尺寸。 形成在外部的任何表层可以通过抛光去除,从而从一侧到另一侧产生具有开放结构的泡沫。 泡沫可以用作电池隔膜。

    METHOD TO PRODUCE NANOPOROUS POLYMERIC MEMBRANES
    7.
    发明申请
    METHOD TO PRODUCE NANOPOROUS POLYMERIC MEMBRANES 有权
    生产纳米聚合物膜的方法

    公开(公告)号:US20140287321A1

    公开(公告)日:2014-09-25

    申请号:US14213112

    申请日:2014-03-14

    CPC classification number: H01M2/145 H01M2/1653

    Abstract: A method for making a flat polymer foam having a core layer of nano-sized open, interconnected cells that includes saturating a solid-state polymer with a supercritical fluid, allowing the gas to desorb for at least 35 minutes, and then heating the gas-saturated solid polymer for at least 3 minutes while constraining the foam in the thickness dimension. Any skin layer formed on the exterior may be removed via polishing, thus creating a foam with an open structure from side to side. The foam can be used as a battery separator.

    Abstract translation: 一种制备扁平聚合物泡沫的方法,其具有纳米尺寸的开放互连电池的核心层,其包括用超临界流体使固态聚合物饱和,允许气体解吸至少35分钟,然后加热气 - 饱和固体聚合物至少3分钟,同时限制泡沫体的厚度尺寸。 形成在外部的任何表层可以通过抛光去除,从而从一侧到另一侧产生具有开放结构的泡沫。 泡沫可以用作电池隔膜。

    METHOD FOR MAKING SHAPEABLE MICROCELLULAR POLY LACTIC ACID ARTICLES
    9.
    发明申请
    METHOD FOR MAKING SHAPEABLE MICROCELLULAR POLY LACTIC ACID ARTICLES 审中-公开
    制备可形成微晶聚乳酸的方法

    公开(公告)号:US20150093564A1

    公开(公告)日:2015-04-02

    申请号:US14564930

    申请日:2014-12-09

    Abstract: A method for making a shapeable article from poly(lactic acid) includes treating solid poly(lactic acid) that results in the solid poly(lactic acid) having a crystallinity of at least 20% by weight based on the weight of the solid poly(lactic acid) and a gas concentration of 6% to 16% by weight based on the weight of the solid poly(lactic acid); and heating the solid poly(lactic acid) having said minimum crystallinity and gas concentration to produce a cellular poly(lactic acid) article that is shapeable. The shapeable cellular poly(lactic acid) article is advantageous in that the article can be further shaped by heat and/or pressure (or vacuum), such as via thermoforming, into a variety of useful products.

    Abstract translation: 由聚(乳酸)制造可成型制品的方法包括处理固体聚乳酸,其导致基于固体聚(重量)的至少20重量%的结晶度的固体聚(乳酸) 乳酸),基于固体聚(乳酸)的重量计,气体浓度为6重量%至16重量%; 并加热具有最小结晶度和气体浓度的固体聚(乳酸)以产生可成形的细胞多(乳酸)制品。 可成形的细胞多(乳酸)制品的优点在于,可以通过热和/或压力(或真空)例如通过热成型将制品进一步成型为各种有用的产品。