摘要:
In the method according to the invention cold or unheated hardened glass and/or glass-ceramic parts are bonded together with a metallic ductile joining material, preferably silver, copper, aluminum or an alloy of those metals, to form a brittle article. The parts to be joined in an initial unheated state are placed with the metallic ductile joining material between them in a high frequency alternating field with frequencies preferably from 100 to 500 kHz. Then the joining material is inductively heated locally to melt it by means of the alternating field and the parts are pressed together to form a sufficiently strong bond between the parts.
摘要:
The invention concerns a photonic device comprising a first section including a material adapted to interact with photons, a second section including a material adapted to interact with photons, with an area of said first section and an area of said second section abutting each other wherein at least a part of said first area and a part of said second area defines a low temperature bonding area to provide adaptability for a plurality of applications based on a combination of materials having specific characteristic benefits, however without introducing unwanted effects having a negative influence on the quality of optical signals.
摘要:
A unit is provided which comprises a first substrate (1) and a second substrate (2). At least one optoelectronic component (4) containing at least one organic material is arranged on the first substrate (1). The first substrate (1) and the second substrate (2) are arranged relative to one another such that the optoelectronic component (4) is arranged between the first substrate (1) and the second substrate (2). In addition, a bonding material (3) is arranged between the first substrate (1) and the second substrate (2), which material encloses the optoelectronic component (4) and bonds the first and second substrates (1, 2) together mechanically. The bonding material (3) contains silver oxide in a proportion of more than 0 wt. % and less than 100 wt. %, preferably between 5 wt. % and 80 wt. % inclusive, ideally between 10 wt. % and 70 wt. % inclusive. The bonding material (3) may further contain at least one filler (5), which changes, preferably reduces, the coefficient of thermal expansion of the bonding material (3). In addition, a method of producing such a unit is provided.
摘要:
Production of an organic optoelectronic component comprising the following steps: A) providing a first substrate (1) having an active region (12) and a first connection region (11) surrounding said active region (12), wherein an organic, functional layer sequence (3) is formed in said active region (12), B) providing a second substrate (2) having a cover region (22) and a second connection region (21) surrounding said cover region (22), C) applying a first connection layer (4) made from a first glass solder material directly to said second substrate (2) in said second connection region (21), D) vitrifying (91) said first glass solder material of said first connection layer (4), E) applying a second connection layer (5) to said vitrified first connection layer (4) or to said first connection region (11) of said first substrate (1) and F) connecting said first substrate (1) to said second substrate (2) such that said second connection layer (5) connects said first connection region (11) to said first connection layer (4). The invention furthermore relates to an organic optoelectronic component.