公开(公告)号:US20090022461A1
公开(公告)日:2009-01-22
申请号:US12235123
申请日:2008-09-22
申请人: Yasuo NAKAJIMA , Kouji Mochizuki , Hiroki Tanaka
发明人: Yasuo NAKAJIMA , Kouji Mochizuki , Hiroki Tanaka
CPC分类号: G02B6/4482 , G02B6/02395 , G02B6/4403
摘要: An optical fiber which reduces transmission loss increase even in a high humidity environment or under water is provided. To solve the above issue, an optical fiber according to the present invention comprises a glass optical fiber coated with at least two coating layers, soft and hard layers. The optical fiber is further coated by a colored resin to make a colored optical fiber. The hard layer and the color layer of the colored optical fiber have a free volume radius of at least 0.290 nm according to positron annihilation lifetime spectroscopy.
摘要翻译: 提供即使在高湿度环境或水下也能降低传输损耗的光纤。 为了解决上述问题,根据本发明的光纤包括涂覆有至少两个涂层的软玻璃光纤和软层和硬层。 光纤被着色树脂进一步涂覆以制成着色光纤。 根据正电子湮没寿命光谱,有色光纤的硬层和彩色层的自由体积半径至少为0.290nm。
-
公开(公告)号:US20110274396A1
公开(公告)日:2011-11-10
申请号:US13101377
申请日:2011-05-05
CPC分类号: G02B6/4482 , G02B6/02395 , G02B6/4403
摘要: The present invention provides an optical fiber in which the transmission loss increase is suppressed even under a high-humidity condition or under a water-immersed condition. A colored optical fiber (22) according to an embodiment of the present invention is a colored optical fiber (22) formed by applying a colored layer to an optical fiber (14) including a glass optical fiber coated with at least a double-layered coating layer of a soft layer and a hard layer, and the ratio of thermal expansion coefficient between the coating layer after the colored layer of the colored optical fiber (22) is applied and the coating layer of the optical fiber (14) before the colored layer is applied is 0.87 or more. Furthermore, an optical fiber ribbon (32) according to another embodiment of the present invention is an optical fiber (32) formed by arranging a plurality of the colored optical fiber (22) in the form of a plane and coating them all together with a ribbon resin and the ratio of thermal expansion coefficient between the coating layer after the colored layer of the colored optical fiber (22) is applied and the coating layer of the optical fiber before the colored layer is applied is 0.90 or more.
摘要翻译: 本发明提供即使在高湿度条件下或在水浸条件下即可抑制传输损失增加的光纤。 根据本发明的实施例的着色光纤(22)是通过将着色层施加到包括至少涂覆有双层涂层的玻璃光纤的光纤(14)而形成的着色光纤(22) 软层和硬层的层,并且施加着色光纤(22)的着色层之后的涂层之间的热膨胀系数与光纤(14)的涂层之前的着色层 被应用为0.87以上。 此外,根据本发明的另一实施例的光纤带(32)是通过将多个着色光纤(22)以平面形式布置并且将它们全部涂覆在一起而形成的光纤(32) 带状树脂,着色光纤(22)的着色层之后的涂层之间的热膨胀系数与涂布着色层之前的光纤涂层的比例为0.90以上。
-
公开(公告)号:US20100266257A1
公开(公告)日:2010-10-21
申请号:US12770807
申请日:2010-04-30
申请人: Yasuo NAKAJIMA , Hiroki Tanaka , Kouji Mochizuki
发明人: Yasuo NAKAJIMA , Hiroki Tanaka , Kouji Mochizuki
IPC分类号: G02B6/00
CPC分类号: G01M11/088 , C03C25/1065 , G02B6/02395
摘要: An optical fiber, which is less likely to increase its transmission loss even when it is exposed to a high-humidity environment or immersed in water, is provided. The optical fiber comprises a glass fiber and at least two coating layers (a soft layer and a hard layer) coated at the circumference of the glass fiber, wherein the limit-adhesion strength between the glass fiber and the coating layer under a hot and humid environment is 0.50N/10 mm or more. Preferably, the glass-transition temperature of the hard layer is less than 90° C.
摘要翻译: 提供了即使在暴露于高湿度环境或浸入水中时也不太可能增加其传输损失的光纤。 该光纤包括玻璃纤维和在玻璃纤维周围涂覆的至少两层涂层(软层和硬质层),其中玻璃纤维与涂层在热湿度下的极限粘附强度 环境为0.50N / 10mm以上。 优选地,硬质层的玻璃化转变温度低于90℃
-
公开(公告)号:US20100119198A1
公开(公告)日:2010-05-13
申请号:US12626814
申请日:2009-11-27
申请人: Yasuo NAKAJIMA , Hiroki TANAKA , Kouji MOCHIZUKI
发明人: Yasuo NAKAJIMA , Hiroki TANAKA , Kouji MOCHIZUKI
IPC分类号: G02B6/036
CPC分类号: C03C25/1065 , G02B6/02395 , G02B6/4403
摘要: A coated optical fiber of the present invention comprises a glass fiber coated by at least two coating layers (a soft layer and a hard layer), wherein the glass surface of the glass fiber, where the at least two coating layers of the optical fiber are removed, has a peak intensity ratio of 0.6 or more in C3H7O+ (m/z 59) or C4H9O+ (m/z 73) with respect to Si+ (m/z 28) peak in cation analysis of TOF-SIMS. The optical fiber suppresses increase in its transmission loss even when it is exposed to a high-humidity environment or immersed in water.
摘要翻译: 本发明的涂覆光纤包括由至少两层涂层(软层和硬层)涂覆的玻璃纤维,其中玻璃纤维的玻璃表面,其中光纤的至少两层涂层为 在TOF-SIMS的阳离子分析中,在C3H7O +(m / z59)或C4H9O +(m / z73)相对于Si +(m / z 28)峰的峰强度比为0.6以上。 即使在暴露于高湿环境或浸入水中时,光纤也抑制了传输损耗的增加。
-
公开(公告)号:US20130062718A1
公开(公告)日:2013-03-14
申请号:US13477128
申请日:2012-05-22
申请人: Hitoshi TADA , Yasuo NAKAJIMA , Yasuhiro KUNITSUGU
发明人: Hitoshi TADA , Yasuo NAKAJIMA , Yasuhiro KUNITSUGU
IPC分类号: H01L31/0232
CPC分类号: H01L31/02327 , H01L31/035281 , H01L31/105 , Y02E10/50
摘要: A back-surface-incidence semiconductor light element includes: a semiconductor substrate of a first conductivity type; a first semiconductor layer of a first conductivity type on the semiconductor substrate; a light absorbing layer on the first semiconductor layer; a second semiconductor layer on the light absorbing layer; and an impurity diffusion region of a second conductivity type in a portion of the second semiconductor layer. A region including a p-n junction between the first semiconductor layer and the impurity diffusion region, and extending through the light absorbing layer, is a light detecting portion that detects light incident on a back surface of the semiconductor substrate. A groove in the back surface of the semiconductor substrate surrounds the light detecting portion, as viewed in plan.
摘要翻译: 背面入射半导体光元件包括:第一导电类型的半导体衬底; 半导体衬底上的第一导电类型的第一半导体层; 在第一半导体层上的光吸收层; 在所述光吸收层上的第二半导体层; 以及在第二半导体层的一部分中具有第二导电类型的杂质扩散区。 包括第一半导体层和杂质扩散区之间并延伸穿过光吸收层的p-n结的区域是检测入射在半导体衬底的背面上的光的光检测部分。 半导体衬底的后表面中的凹槽围绕光检测部分,如在平面图中所示。
-
-
-
-