Method of manufacturing a ferritic stainless steel plate
    1.
    发明授权
    Method of manufacturing a ferritic stainless steel plate 失效
    铁素体不锈钢板的制造方法

    公开(公告)号:US06645324B2

    公开(公告)日:2003-11-11

    申请号:US10103445

    申请日:2002-03-21

    IPC分类号: C21D802

    摘要: A ferritic stainless steel plate of excellent ridging resistance and formability, as well as a manufacturing method thereof are proposed. Specifically, the rolling is conducted at a rolling reduction of 30% or more in at least 1 pass and at a temperature difference between the center of the plate thickness and the surface of 200° C. or lower in a pass for the maximum rolling reduction to cause the area ratio of a {111} orientation colony to be present by 30% or more in the regions of ⅛ to ⅜ and ⅝ to ⅞ of the plate thickness. The {111} orientation colony is an assembly of adjacent crystals in which the angle of orientation vector for each of the crystals relative to the direction vector vertical to the rolling surface is within 15°.

    摘要翻译: 提出了具有优异抗皱性和成形性的铁素体不锈钢板及其制造方法。 具体而言,在至少1次通过中的压下率为30%以上,在板厚中心与200℃以下的温度差之间进行轧制,最终轧制压下率 使{111}取向菌落的面积比在板厚的1/8〜3/8〜5/8〜7/8的范围内存在30%以上。 {111}取向菌落是相邻晶体的组合,其中每个晶体相对于垂直于滚动表面的方向矢量的<111>取向矢量的角度在15°以内。

    Chromium steel sheets having an excellent press formability
    2.
    发明授权
    Chromium steel sheets having an excellent press formability 失效
    具有优异压制成形性的铬钢板

    公开(公告)号:US5709836A

    公开(公告)日:1998-01-20

    申请号:US602857

    申请日:1996-02-28

    CPC分类号: C22C27/06 C22C38/28 C22C38/32

    摘要: A chromium steel sheet having excellent press formability, particularly deep-drawing formability and resistance to secondary work brittleness. The construction is a chromium steel sheet including C: not more than 0.03 wt %, Si: not more than 1.0 wt %, Mn: not more than 1.0 wt %, P: not more than 0.05 wt %, S: not more than 0.015 wt %, Al: not more than 0.10 wt %, N: not more than 0.02 wt %, Cr: 5-60 wt %, Ti: 4(C+N)-0.5 wt %, Nb: 0.003-0.020 wt %, B: 0.0002-0.005 wt %, and, if necessary, one or more selected from Mo: 0.01-5.0 wt %, Ca: 0.0005-0.01 wt % and Se: 0.0005-0.025 wt %, and the balance being Fe and inevitable impurities.

    摘要翻译: PCT No.PCT / JP95 / 01341 Sec。 371日期1996年2月28日 102(e)日期1996年2月28日PCT提交1995年7月5日PCT公布。 第WO96 / 01335号公报 日期1996年5月18日具有优异的压制成型性,特别是深冲成形性和耐二次加工脆性的铬钢板。 该结构是C:不大于0.03重量%,Si:1.0重量%以下,Mn:1.0重量%以下,P:0.05重量%以下S:不大于0.015的铬钢板 重量%,Al:0.10重量%以下,N:0.02重量%以下,Cr:5-60重量%,Ti:4(C + N)-0.5重量%,Nb:0.003-0.020重量% B:0.0002-0.005重量%,如果需要,选自Mo:0.01-5.0重量%,Ca:0.0005-0.01重量%和Se:0.0005-0.025重量%中的一种或多种,​​余量为Fe和不可避免的杂质 。

    Ferritic stainless steel plate
    3.
    发明授权
    Ferritic stainless steel plate 有权
    铁素体不锈钢板

    公开(公告)号:US06458221B1

    公开(公告)日:2002-10-01

    申请号:US09700779

    申请日:2000-11-20

    IPC分类号: C22C3818

    摘要: The present invention provides a ferritic stainless steel sheet having excellent formability and excellent surface quality after forming. In specific means, the steel sheet contains, by mass %, 0.02 to 0.06% of C, 1.0% or less of Si, 1.0% or less of Mn, 0.05% or less of P, 0.01% or less of S, 0.005% or less of Al, 0.005% or less of Ti, 11 to 30% of Cr, 0.7% or less of Ni, the balance composed of Fe, and inevitable impurities, wherein N is contained to satisfy the relation to the C content represented by 0.06≦(C+N)≦0.12, and 1≦N/C, and V is contained to satisfy the relation to the N content represented by 1.5×10−3≦(V×N)≦1.5×10−2 (wherein C, N and V: the contents (mass %) of the elements).

    摘要翻译: 本发明提供一种成形性优异且成形后表面质量优异的铁素体系不锈钢板。 具体地说,钢板以质量%计含有C:0.02〜0.06%,Si:1.0%以下,Mn:1.0%以下,P:0.05%以下,S:0.01%以下,S:0.005% 或更少的Al,0.005%以下的Ti,11〜30%的Cr,0.7%以下的Ni,余量由Fe和不可避免的杂质组成,其中N包含以满足与C 0.06 <=(C + N)<= 0.12,1 <= N / C,并且包含V以满足与1.5×10 -3 <=(VxN)<= 1.5×10 -2 其中C,N和V:元素的含量(质量%))。

    Ferritic stainless steel plate excellent in deep drawability and
anti-ridging property and production method thereof
    4.
    发明授权
    Ferritic stainless steel plate excellent in deep drawability and anti-ridging property and production method thereof 失效
    铁素体不锈钢板具有优异的深冲性和抗皱性能及其制造方法

    公开(公告)号:US6113710A

    公开(公告)日:2000-09-05

    申请号:US269295

    申请日:1999-03-29

    摘要: The present invention provides a ferritic stainless steel plate improved in the deep drawability and the anti-ridging property at deep drawing work and the production technique thereof. The practical construction of the present invention is a ferritic stainless steel plate containing from 0.001 to 0.015 wt. % C, not more than 1.0 wt. % Si, not more than 1.0 wt. % Mn, not more than 0.05 wt. % P, not more than 0.010 wt. % S, from 8 to 30 wt. % Cr, not more than 0.08 wt. % Al, from 0.005 to 0.015 wt. % N, not more than 0.0080 wt. % O, not more than 0.25 wt. % Ti with Ti/N.gtoreq.12, and from 0.05 to 0.10 wt. % (Nb+V) with V/Nb being from 2 to 5, and, if necessary, further containing one or more kinds selected from not more than 2.0 wt. % Mo, not more than 1.0 wt. % Ni, and not more than 1.0 wt. % Cu together with one or more kinds selected from from 0.0005 to 0.0030 wt. % B, from 0.0007 to 0.0030 wt. % Ca and from 0.0005 to 0.0030 wt. % Mg. Furthermore, in the production method of the present invention, the above-described ferritic stainless steel plate is produced by heating the steel slab made up of the above-described components to a temperature range of 1170.degree. C. or lower, finishing rough hot rolling of the slab at a temperature range of 950.degree. C. or higher, and then carrying out hot finish-rolling.

    摘要翻译: PCT No.PCT / JP98 / 03469 Sec。 371 1999年3月29日第 102(e)1999年3月29日PCT PCT 1998年8月4日PCT公布。 公开号WO99 /​​ 07909 日期1999年2月18日本发明提供了一种改进深冲性和深冲压加工抗皱性能的铁素体不锈钢板及其制造方法。 本发明的实际构造是含有0.001〜0.015重量%的铁素体不锈钢板。 %C,不大于1.0wt。 %Si,不大于1.0wt。 %Mn,不大于0.05wt。 %P,不大于0.010重量% %S,8〜30wt。 %Cr,不大于0.08wt。 %Al,0.005〜0.015wt。 %N,不大于0.0080wt。 %O,不大于0.25wt。 %Ti,Ti / N> / = 12,和0.05〜0.10wt。 %(Nb + V),V / Nb为2〜5,如果需要,还含有选自不超过2.0重量%的一种或多种。 %Mo,不大于1.0wt。 %Ni,不大于1.0wt。 %Cu与选自0.0005至0.0030重量%的一种或多种。 %B,0.0007-0.0030wt。 %Ca和0.0005〜0.0030wt。 %Mg。 此外,在本发明的制造方法中,上述铁素体系不锈钢板是将由上述构成的钢坯加热至1170℃以下的温度范围, 在950℃以上的温度范围内进行热精轧。

    Ferritic stainless steel plate
    6.
    发明授权

    公开(公告)号:US06383309B1

    公开(公告)日:2002-05-07

    申请号:US09725624

    申请日:2000-11-29

    IPC分类号: C22C3818

    摘要: A ferritic stainless steel plate of excellent ridging resistance and formability, as well as a manufacturing method thereof are proposed. Specifically, the rolling is conducted at a rolling reduction of 30% or more in at least 1 pass and at a temperature difference between the center of the plate thickness and the surface of 200° C. or lower in a pass for the maximum rolling reduction to cause the area ratio of a {111} orientation colony to be present by 30% or more in the regions of ⅛ to ⅜ and ⅝ to ⅞ of the plate thickness. The {111} orientation colony is an assembly of adjacent crystals in which the angle of orientation vector for each of the crystals relative to the direction vector vertical to the rolling surface is within 15°.

    Ferritic Cr-containing steel sheet having excellent ductility, formability, and anti-ridging properties
    7.
    发明授权
    Ferritic Cr-containing steel sheet having excellent ductility, formability, and anti-ridging properties 有权
    具有优异的延展性,成形性和抗皱纹性的铁素体含Cr钢板

    公开(公告)号:US06500280B2

    公开(公告)日:2002-12-31

    申请号:US09946243

    申请日:2001-09-05

    IPC分类号: C21D804

    摘要: Producing a ferritic Cr-containing steel sheet having excellent ductility, formability, and anti-ridging properties, and exhibiting excellent surface quality after forming, wherein a ferritic Cr-containing steel sheet contains, by mass %, about 0.001 to 0.12% of C, about 0.001 to 0.12% of N, and about 9 to 32% of Cr, and has a crystal grain structure in which in a section of a hot-rolled annealed steel sheet in the thickness direction parallel to the rolling direction, an elongation index of crystal grains is 5 or less at any position, and in a section of a cold-rolled annealed steel sheet in the thickness direction parallel to the rolling direction, any colony of coarse grains oriented in the rolling direction has an aspect ratio of 5 or less. The production method includes hot rolling, pre-rolling by cold or warm rolling with a rolling reduction of about 2 to 15%, hot-rolled sheet annealing, cold rolling, and finish annealing; preferably the FDT of hot rolling is 850° C., and 0.0002 to 0.0030% of B is added.

    摘要翻译: 制造具有优异的延展性,成形性和抗皱性的铁素体系Cr系钢板,成形后表现出优异的表面质量,其中铁素体含Cr钢板以质量%计含有C:0.001〜0.12% 约0.001〜0.12%的N和约9〜32%的Cr,并且具有在热轧退火钢板的厚度方向平行于轧制方向的截面中的延伸率指数 在任何位置的晶粒为5以下,在与轧制方向平行的厚度方向的冷轧退火钢板的截面中,在轧制方向取向的粗晶粒的任意集合都具有5以下的纵横比 。 制造方法包括热轧,冷轧或暖轧预压,轧制压下率为2〜15%左右,热轧板退火,冷轧,成品退火; 优选热轧的FDT为850℃,添加0.0002〜0.0030%的B。

    Method of producing ferritic Cr-containing steel sheet having excellent ductility, formability, and anti-ridging properties
    8.
    发明授权
    Method of producing ferritic Cr-containing steel sheet having excellent ductility, formability, and anti-ridging properties 有权
    具有优异的延展性,成形性和抗皱纹性的铁素体系Cr系钢板的制造方法

    公开(公告)号:US06413332B1

    公开(公告)日:2002-07-02

    申请号:US09650052

    申请日:2000-08-29

    IPC分类号: C21D802

    摘要: Producing a ferritic Cr-containing steel sheet having excellent ductility, formability, and anti-ridging properties, and exhibiting excellent surface quality after forming, wherein a ferritic Cr-containing steel sheet contains, by mass %, about 0.001 to 0.12% of C, about 0.001 to 0.12% of N, and about 9 to 32% of Cr, and has a crystal grain structure in which in a section of a hot-rolled annealed steel sheet in the thickness direction parallel to the rolling direction, an elongation index of crystal grains is 5 or less at any position, and in a section of a cold-rolled annealed steel sheet in the thickness direction parallel to the rolling direction, any colony of coarse grains oriented in the rolling direction has an aspect ratio of 5 or less. The production method includes hot rolling, pre-rolling by cold or warm rolling with a rolling reduction of about 2 to 15%, hot-rolled sheet annealing, cold rolling, and finish annealing; preferably the FDT of hot rolling is 850° C., and 0.0002 to 0.0030% of B is added.

    摘要翻译: 制造具有优异的延展性,成形性和抗皱性的铁素体系Cr系钢板,成形后表现出优异的表面质量,其中铁素体含Cr钢板以质量%计含有C:0.001〜0.12% 约0.001〜0.12%的N和约9〜32%的Cr,并且具有在热轧退火钢板的厚度方向平行于轧制方向的截面中的延伸率指数 在任何位置的晶粒为5以下,在与轧制方向平行的厚度方向的冷轧退火钢板的截面中,在轧制方向取向的粗晶粒的任意集合都具有5以下的纵横比 。 制造方法包括热轧,冷轧或暖轧预压,轧制压下率为2〜15%左右,热轧板退火,冷轧,成品退火; 优选热轧的FDT为850℃,添加0.0002〜0.0030%的B。

    Method for producing chromium-containing hot rolled steel strip
    9.
    发明授权
    Method for producing chromium-containing hot rolled steel strip 失效
    生产含铬热轧钢带的方法

    公开(公告)号:US06217679B1

    公开(公告)日:2001-04-17

    申请号:US09194129

    申请日:1998-11-23

    IPC分类号: C21D802

    摘要: The invention provides hot-rolled steel strips which, after having been acid-pickled, can be directly used. The strips have no Cr-decreasing layer and no shot blasted marks on their surface and have good corrosion resistance. The invention also provides a technique of efficiently producing the hot-rolled steel strips. A steel slab having a Cr content of from 6.0 to 25.0 wt. % is hot-rolled, then coiled at a temperature not higher than 700° C., then optionally quenched in water immediately after the coiling, then annealing in a reducing atmosphere, and thereafter acid-pickled in a solution of nitric acid/hydrochloric acid.

    摘要翻译: 本发明提供了可以直接使用酸洗后的热轧钢带。 带材没有减薄层,表面没有喷丸痕迹,具有良好的耐腐蚀性。 本发明还提供了一种有效地生产热轧钢带的技术。 Cr含量为6.0〜25.0重量%的钢坯 %热轧,然后在不高于700℃的温度下卷绕,然后在卷取后立即在水中骤冷,然后在还原气氛中退火,然后在硝酸/盐酸溶液中酸洗 。