Method for preparing pyrochlore-type oxide and method for producing electrocatalyst for fuel cell
    1.
    发明授权
    Method for preparing pyrochlore-type oxide and method for producing electrocatalyst for fuel cell 有权
    制备烧绿石型氧化物的方法及燃料电池用电催化剂的制备方法

    公开(公告)号:US08409543B2

    公开(公告)日:2013-04-02

    申请号:US13220981

    申请日:2011-08-30

    IPC分类号: C01G55/00

    CPC分类号: H01M4/9025 H01M2008/1095

    摘要: A pyrochlore-type oxide represented by a general formula A2B2O7-Z is prepared by precipitate formation, where A and B each represent a metal element, where Z represents a number of at least 0 and at most 1, where A contains at least one element selected from a group consisting of Pb, Sn, and Zn, and where B contains at least one element selected from a group consisting of Ru, W, Mo, Ir, Rh, Mn, Cr, and Re. Impurities are then sufficiently removed through washing and drying processes, and the pyrochlore-type oxide is calcined under controlled conditions. This allows the crystallinity of the pyrochlore-type oxide, which contained amorphous parts immediately after the production of the precipitate, to be increased so that the resistance to acid can be improved while preventing particle aggregation.

    摘要翻译: 通过沉淀形成制备由通式A2B2O7-Z表示的烧绿石型氧化物,其中A和B各自表示金属元素,其中Z表示至少为0且至多为1的数,其中A包含至少一个元素 选自由Pb,Sn和Zn组成的组,并且其中B含有选自由Ru,W,Mo,Ir,Rh,Mn,Cr和Re组成的组中的至少一种元素。 然后通过洗涤和干燥过程充分除去杂质,并且在受控条件下煅烧烧绿石型氧化物。 这使得在生成沉淀物之后立即含有非晶形部分的烧绿石型氧化物的结晶度增加,从而可以改善耐酸性,同时防止颗粒聚集。

    METHOD FOR PREPARING PYROCHLORE-TYPE OXIDE AND METHOD FOR PRODUCING ELECTROCATALYST FOR FUEL CELL
    2.
    发明申请
    METHOD FOR PREPARING PYROCHLORE-TYPE OXIDE AND METHOD FOR PRODUCING ELECTROCATALYST FOR FUEL CELL 有权
    制备二氧化氯型氧化物的方法及生产燃料电池的方法

    公开(公告)号:US20120053045A1

    公开(公告)日:2012-03-01

    申请号:US13220981

    申请日:2011-08-30

    CPC分类号: H01M4/9025 H01M2008/1095

    摘要: A pyrochlore-type oxide represented by a general formula A2B2O7-Z is prepared by precipitate formation, where A and B each represent a metal element, where Z represents a number of at least 0 and at most 1, where A contains at least one element selected from a group consisting of Pb, Sn, and Zn, and where B contains at least one element selected from a group consisting of Ru, W, Mo, Ir, Rh, Mn, Cr, and Re. Impurities are then sufficiently removed through washing and drying processes, and the pyrochlore-type oxide is calcined under controlled conditions. This allows the crystallinity of the pyrochlore-type oxide, which contained amorphous parts immediately after the production of the precipitate, to be increased so that the resistance to acid can be improved while preventing particle aggregation.

    摘要翻译: 通过沉淀形成制备由通式A2B2O7-Z表示的烧绿石型氧化物,其中A和B各自表示金属元素,其中Z表示至少为0且至多为1的数,其中A包含至少一个元素 选自由Pb,Sn和Zn组成的组,并且其中B含有选自由Ru,W,Mo,Ir,Rh,Mn,Cr和Re组成的组中的至少一种元素。 然后通过洗涤和干燥过程充分除去杂质,并且在受控条件下煅烧烧绿石型氧化物。 这使得在生成沉淀物之后立即含有非晶形部分的烧绿石型氧化物的结晶度增加,从而可以改善耐酸性,同时防止颗粒聚集。