EPOXIDISED NATURAL RUBBER-BASED BLEND WITH REVERSIBLE ELECTRICAL BEHAVIOUR
    1.
    发明申请
    EPOXIDISED NATURAL RUBBER-BASED BLEND WITH REVERSIBLE ELECTRICAL BEHAVIOUR 审中-公开
    具有可逆电气行为的环氧自然基橡胶基混合物

    公开(公告)号:US20170009029A1

    公开(公告)日:2017-01-12

    申请号:US15272431

    申请日:2016-09-22

    Applicant: Yong KOK CHONG

    Inventor: Yong KOK CHONG

    Abstract: Epoxidised natural rubber [ENR] based vulcanised-blends with two different types of electrical conductive filler (i.e. conductive grade-carbon black and intrinsically electrical conductive polymer) may be produced respectively by using either internal mechanical mixing method or open milling method or the combination of the two methods. All these ENR based vulcanised-blends show high consistent reversible electrical behaviour under the tensile straining process. They also exhibit useful mechanical properties with tensile strengths up to 28.0 MPa, elongations at break up to 800.0% and Dunlop rebound resiliencies up to 55.0%. The lower the rebound resilience, the better the damping property and shock absorption ability for the ENR based vulcanised-blends. As a result, these ENR based vulcanised-blends are ideal to be used for manufacturing flexible sensors that may correspond to the tensile straining process.

    Abstract translation: 可以通过使用内部机械混合法或开放式研磨法或两种不同类型的导电填料(即导电级 - 炭黑和本体导电聚合物)的环氧化天然橡胶[ENR]基硫化 - 共混物 两种方法。 所有这些基于ENR的硫化共混物在拉伸应变过程下显示出高度一致的可逆电性能。 它们还具有有效的机械性能,拉伸强度高达28.0MPa,断裂伸长率达到800.0%,Dunlop回弹韧性高达55.0%。 回弹性越低,ENR型硫化混合物的阻尼性能和冲击吸收能力越好。 因此,这些基于ENR的硫化共混物非常适用于制造可对应于拉伸应变过程的柔性传感器。

    EPOXIDISED NATURAL RUBBER BASED BLEND FOR ANTISTATIC FOOTWEAR APPLICATION
    2.
    发明申请
    EPOXIDISED NATURAL RUBBER BASED BLEND FOR ANTISTATIC FOOTWEAR APPLICATION 审中-公开
    用于防静电鞋材的环氧橡胶基橡胶

    公开(公告)号:US20170006957A1

    公开(公告)日:2017-01-12

    申请号:US15272423

    申请日:2016-09-21

    Abstract: Electrically conductive vulcanised epoxidised natural rubber [ENR]-carbon black blends can be produced by using either internal mechanical mixing method or open milling method. These two methods are commercially friendly due to their practicability and high production rate. The addition of vulcanisation system, either sulfur or peroxide type does not affect the electrical properties of the vulcanised blends. All vulcanized blends prepared in this innovation show useful electrical properties with electrical volume resistances as low as the order of 101 ohms. All these vulcanised blends also exhibit good mechanical properties with tensile strengths up to 26.0 MPa and Dunlop rebound resiliencies of 14.0% (i.e. high damping property). The black colour level of all these vulcanised blends is adjustable. As a result of good electrical and mechanical properties (especially high damping property), they have good potential to be used for antistatic footwear manufacturing and application.

    Abstract translation: 导电硫化环氧化天然橡胶[ENR] - 碳黑混合物可以通过内部机械混合法或开放式研磨法生产。 这两种方法由于其实用性和高生产率而在商业上是友好的。 硫化或硫化过程中硫化体系的添加不影响硫化混合物的电性能。 在本创新中制备的所有硫化混合物显示出低至101欧姆数量级的电容量电阻的有用电学性能。 所有这些硫化共混物也表现出良好的机械性能,拉伸强度高达26.0MPa,Dunlop回弹韧性为14.0%(即高阻尼性能)。 所有这些硫化混合物的黑色水平是可调节的。 由于具有良好的电气和机械性能(特别是较高的阻尼性能),它们具有很好的用于抗静电鞋类制造和应用的潜力。