摘要:
An electrostatic-image developing toner including at least a binder resin; a colorant; and a release agent, wherein an average circularity of particles having a particle diameter in a range of 0.79 times or more but less than 1.15 times as large as a most frequent diameter in a number particle size distribution of the toner is within a range of 1.010 times or more but less than 1.020 times as high as an average circularity of particles having a particle diameter of 1.15 times or more as large as the most frequent diameter.
摘要:
A toner including a binder resin and a release agent is provided. The binder resin includes an amorphous resin and a crystalline resin. In a cross-sectional image of the toner obtained by a transmission electron microscope, a longest length Lmax of the release agent is equal to or greater than 1.1 times a maximum Feret diameter Df of the toner, and the crystalline resin is dispersed in the amorphous resin forming domains having a maximum Feret diameter Cf of 0.20 μm or less.
摘要:
A toner including: binder resin; and release agent, wherein the release agent is 1% to 8% by mass to the toner, as equivalent mass of endothermic amount of the release agent determined by DSC, wherein the release agent present in region from surface of the toner to 0.3 μm depth is 0.1% to 4% by mass, as determined by FTIR-ATR, and wherein, in TEM image of torn surface of the toner, WDa
摘要:
A toner is provided. The toner includes a binder resin and a release agent. The release agent has an average aspect ratio of 31 or more, when the average aspect ratio is determined from cross-sectional images of the toner observed with a transmission electron microscope (TEM).
摘要:
A toner is provided. The toner includes a binder resin and a release agent. The toner satisfies the following inequation: 0.45≦(S1/S2)≦1.00 wherein S1 and S2 represent areas of quadrangles circumscribing the release agent and the toner, respectively, in a cross-sectional image of the toner obtained by a transmission electron microscope (TEM).
摘要:
Provided is a toner including at least: a binder resin; and a release agent, wherein in a transmission electron microscopic (TEM) image of a torn cross-section of the toner, the release agent has an acicular or filiform shape and an average aspect ratio of 31 or greater, and wherein a displacement amount of the toner when 250 micronewtons is applied to the toner in a microcompression test is 700 nm or less.
摘要:
A toner is provided. The toner includes a binder resin and a release agent. The binder resin includes a polyester resin. The toner has a single exothermic peak measured by a differential scanning calorimetry (DSC) descending in a temperature range of from 150° C. to 0° C., wherein the exothermic peak is in a temperature range of from 40° C. to 60° C. and has a half bandwidth of at most 10° C. The release agent disperse to network form in the cross-sectional images of the toner observed with a transmission electron microscope (TEM).
摘要:
A toner is provided. The toner includes a binder resin, a colorant, a release agent and an external additive. The toner has an average circularity of from 0.965 to less than 0.985. The toner has BET specific surface area of less than 1.20 m2/g after liberation treatment of external additive.
摘要:
A particulate material production method is provided. The particulate material production method includes ejecting a particulate material composition liquid, which includes an organic solvent and a particulate material composition including at least a resin and dissolved or dispersed in the organic solvent, from at least one nozzle to form droplets of the particulate material composition liquid in a gas phase; and solidifying the droplets of the particulate material composition liquid to prepare particles of the particulate material composition. The droplet solidifying step includes contacting the droplets with a poor solvent for the particulate material composition.
摘要:
A particulate material production method is provided. The particulate material production method includes ejecting a particulate material composition liquid, which includes an organic solvent and a particulate material composition including at least a resin and dissolved or dispersed in the organic solvent, from at least one nozzle to form droplets of the particulate material composition liquid in a gas phase; and solidifying the droplets of the particulate material composition liquid to prepare particles of the particulate material composition. The droplet solidifying step includes contacting the droplets with a poor solvent for the particulate material composition.