METHOD FOR MANUFACTURING POSITIVE ACTIVE MATERIAL FOR RECHARGEABLE LITHIUM BATTERY AND RECHARGEABLE LITHIUM BATTERY USING SAME
    1.
    发明申请
    METHOD FOR MANUFACTURING POSITIVE ACTIVE MATERIAL FOR RECHARGEABLE LITHIUM BATTERY AND RECHARGEABLE LITHIUM BATTERY USING SAME 审中-公开
    用于制造可充电锂电池的正极活性材料和使用其的可充电锂电池的方法

    公开(公告)号:US20120264009A1

    公开(公告)日:2012-10-18

    申请号:US13435464

    申请日:2012-03-30

    摘要: A method of preparing a positive active material for a rechargeable lithium battery including a) mixing a composite metal precursor and a lithium compound; b) firing the mixture to prepare a positive active material; c) mixing the resulting positive active material, a carbon coating material, and a solvent; and d) heat-treating the resulting mixture to provide a positive active material coated with the carbon coating material, wherein the carbon coating material is used in an amount of 1 wt % to 30 wt % based on 100 wt % of the composite metal precursor, lithium compound, and carbon coating material, the firing is performed at 400 to 900° C., and the positive active material provided in d) is represented by the following Chemical Formula 1, is provided. LiaNixCoyMnzM′kO2   [Chemical Formula 1] In Chemical Formula 1, each definition is the same as in the detailed description.

    摘要翻译: 一种制备用于可再充电锂电池的正极活性材料的方法,包括:a)混合复合金属前体和锂化合物; b)烧制混合物以制备正极活性物质; c)将得到的正极活性物质,碳涂层材料和溶剂混合; 和d)对所得混合物进行热处理以提供涂覆有碳涂层材料的正极活性材料,其中所述碳涂层材料的使用量相对于所述复合金属前体的100重量%为1重量%至30重量% ,锂化合物和碳涂层材料,在400-900℃下进行焙烧,并且提供d)中提供的正极活性材料由以下化学式1表示。 LiaNixCoyMnzM'kO2 [化学式1]在化学式1中,每个定义与详细描述相同。

    POSITIVE ACTIVE MATERIAL FOR RECHARGEABLE LITHIUM BATTERY, RECHARGEABLE LITHIUM BATTERY USING THE SAME AND METHOD FOR MANUFACTURING THE SAME
    3.
    发明申请
    POSITIVE ACTIVE MATERIAL FOR RECHARGEABLE LITHIUM BATTERY, RECHARGEABLE LITHIUM BATTERY USING THE SAME AND METHOD FOR MANUFACTURING THE SAME 审中-公开
    用于可充电锂电池的正极活性材料,使用该锂电池的可充电锂电池及其制造方法

    公开(公告)号:US20110305947A1

    公开(公告)日:2011-12-15

    申请号:US13158930

    申请日:2011-06-13

    IPC分类号: H01M4/131 H01M10/056

    摘要: Disclosed are a positive active material for a lithium rechargeable battery and a lithium rechargeable battery using the same, and the positive active material is represented by the following Chemical Formula 1, and has an effective magnetic moment of about 2.4 μB/mol or greater at a temperature of more than or equal to a Curie temperature. Chemical Formula 1: LiMeO2. In Chemical Formula 1, Me is NixCOyMnzM′k, 0.45≦x≦0.65, 0.15≦y≦0.25, 0.15≦z≦0.35, 0.9≦a≦1.2, 0≦k≦0.1, x+y+z+k=1, and M′ is Al, Mg, Ti, Zr, or a combination thereof. The positive active material may have an a-axis lattice constant of the positive active material of about 2.865 Å or greater, and may have a c-axis lattice constant of the positive active material of about 14.2069 Å or greater. A mole ratio of Li to Me of Chemical Formula 1 may range from about 0.9 to about 1.2.

    摘要翻译: 公开了一种锂可再充电电池的正极活性材料和使用该锂二次电池的锂可再充电电池,正极活性材料由以下化学式1表示,并且在a的情况下具有约2.4μB/ mol以上的有效磁矩 温度大于或等于居里温度。 化学式1:LiMeO 2。 在化学式1中,Me是NixCOyMnzM'k,0.45≦̸ x和nlE; 0.65,0.15和nlE; y≦̸ 0.25,0.15≦̸ z≦̸ 0.35,0.9≦̸ a≦̸ 1.2,0≦̸ k≦̸ 0.1,x + y + z + k = 1,M'为Al,Mg,Ti,Zr或其组合。 正极活性材料可以具有约2.865或更高的正极活性材料的a轴晶格常数,并且可以具有约14.2069埃或更高的正极活性材料的c轴晶格常数。 化学式1的Li与Me的摩尔比可以在约0.9至约1.2的范围内。