Abstract:
A method for making a phosphorated composite is provided. First, a mixture is obtained by mixing a source material with red phosphorus. The weight ratio of the source material to the red phosphorus ranges from about 1:10 to about 5:1. Second, the mixture is dried in an inert atmosphere or vacuum. Third, the mixture is heated in a reacting room filled with an inert atmosphere so that the red phosphorus sublimes. Finally, the reacting room is cooled down.
Abstract:
VINYL CHLORIDE AND VINYLIDENE CHLORIDE POLYMERS CAN BE CROSS-LINKED OR OTHERWISE MODIFIED BY REACTION WITH A POLY (DIAZO) COMPOUND SELECTED FROM THE GROUP OF
R-(O-CO-CN2-R'')X AND A-(CN2-R'')X
WHERE X IS AN INTEGER GREATER THAN 1, R IS AN ORGANIC RADICAL INERT TO MODIFICATION REACTIONS, A IS AN AROMATIC RADICAL INERT TO MODIFICATION REACTIONS, AND R'' IS A HYDROGEN, ARYL OR -COOZ RADICAL WHERE Z IS AN ALKYL OR ARYL RADICAL. THE REACTION BETWEEN THE POLY (DIAZO) COMPOUND AND POLYMER CAN BE INITIATED EITHER BY HEATING OR BY EXPOSING TO ULTRAVIOLET RADIATION.
Abstract:
A phosphorated composite capable of electrochemical reversible lithium storage includes a conductive matrix and a red phosphorus. The conductive matrix includes a material being selected from the group consisting of conductive polymer and conductive carbonaceous material. A weight percentage of the conductive matrix in the phosphorated composite ranges from about 10% to about 85%. A weight percentage of the red phosphorus in the phosphorated composite ranges from about 15% to about 90%. A method for making the phosphorated composite and a lithium-ion battery using the phosphorated composite is also provided.
Abstract:
Process for the preparation of a vinylidene chloride polymer composite comprising a solid particulate encapsulated in the vinylidene chloride polymer. The process comprises providing a dispersion of a solid particulate material in a liquid phase, said dispersion comprising a RAFT/MADIX agent; providing vinylidene chloride and optionally one or more ethylenically unsaturated monomer copolymerizable therewith to said dispersion; and polymerizing vinylidene chloride and said optionally present one or more ethylenically unsaturated monomer under the control of said RAFT/MADIX agent to form polymer at the surface of said solid particulate material.
Abstract:
A method for making the phosphorated composite e is provided. First, a mixture is obtained by mixing a source material with red phosphorus. The weight ratio of the source material to the red phosphorus ranges from about 1:10 to about 5:1. Second, the mixture is dried in an inert atmosphere or vacuum. Third, the mixture is heated in a reacting room filled with an inert atmosphere so that the red phosphorus sublimes. Finally, the reacting room is cooled down.
Abstract:
Process for the preparation of a vinylidene chloride polymer composite comprising a solid particulate encapsulated in the vinylidene chloride polymer. The process comprises providing a dispersion of a solid particulate material in a liquid phase, said dispersion comprising a RAFT/MADIX agent; providing vinylidene chloride and optionally one or more ethylenically unsaturated monomer copolymerisable therewith to said dispersion; and polymerising vinylidene chloride and said optionally present one or more ethylenically unsaturated monomer under the control of said RAFT/MADIX agent to form polymer at the surface of said solid particulate material.
Abstract:
A phosphorated composite capable of electrochemical reversible lithium storage includes a conductive matrix and red phosphorus. The conductive matrix includes a material being selected from the group consisting of conductive polymer and conductive carbonaceous material. A weight percentage of the conductive matrix in the phosphorated composite ranges from about 10% to about 85%. A weight percentage of the red phosphorus in the phosphorated composite ranges from about 15% to about 90%. An anode using the phosphorated composite is also provided.
Abstract:
A phosphorated composite capable of electrochemical reversible lithium storage includes a conductive matrix and red phosphorus. The conductive matrix includes a material being selected from the group consisting of conductive polymer and conductive carbonaceous material. A weight percentage of the conductive matrix in the phosphorated composite ranges from about 10% to about 85%. A weight percentage of the red phosphorus in the phosphorated composite ranges from about 15% to about 90%. An anode using the phosphorated composite is also provided.
Abstract:
A lithium-ion battery includes an anode, a cathode, and an electrolyte. The anode includes a phosphorated composite including a conductive matrix and a red phosphorus. The conductive matrix includes a material being selected from the group consisting of conductive polymer and conductive carbonaceous material. A weight percentage of the conductive matrix in the phosphorated composite ranges from about 10% to about 85%. A weight percentage of the red phosphorus in the phosphorated composite ranges from about 15% to about 90%.