耐水蒸気腐食性多層皮膜、およびその製造方法
    93.
    发明申请
    耐水蒸気腐食性多層皮膜、およびその製造方法 审中-公开
    蒸汽耐腐蚀多层薄膜及其制造方法

    公开(公告)号:WO2016052114A1

    公开(公告)日:2016-04-07

    申请号:PCT/JP2015/075605

    申请日:2015-09-09

    CPC classification number: B32B9/00 C04B41/87 C04B41/89 F01D5/28

    Abstract:  炭化ケイ素複合材料を含む基材上に形成される耐水蒸気腐食性多層皮膜であって、粒界ガラス相を内在させずに形成した、複数の金属酸化物の共晶構造体を含む共晶構造層と、該共晶構造層と前記基材との間に形成され、前記金属酸化物と金属炭化物とを含み、前記基材に近づくほど前記金属炭化物の含有割合が高められた組成傾斜層と、を備えたことを特徴とする。

    Abstract translation: 一种形成在含有碳化硅复合材料的基体材料上的耐蒸汽耐腐蚀多层膜,所述防蒸汽耐腐蚀多层膜的特征在于包括:含有多个金属氧化物的共晶结构的共晶结构层, 晶界玻璃相存在于其中; 以及介于共晶结构层和含有金属氧化物和金属碳化物的基体材料之间的梯度组成层,其中金属碳化物的组成比向衬底材料梯度增加。

    BOND COAT
    97.
    发明申请
    BOND COAT 审中-公开

    公开(公告)号:WO2015181549A1

    公开(公告)日:2015-12-03

    申请号:PCT/GB2015/051549

    申请日:2015-05-28

    Abstract: The present invention relates to a platinum group metal-diffused bond coat with single gamma-prime phase of a nickel-based single crystal superalloy, which is suitable for use in thermal barrier coatings to protect components (e.g. turbine blades, augmentors, and exhaust and combustion chamber components) that are exposed to exceptionally high temperatures. The present invention also relates to methods of forming the platinum group metal-diffused gamma prime bond coat and to the use of this bond coat in thermal barrier coatings.

    Abstract translation: 本发明涉及一种适用于热障涂层以保护部件(例如涡轮叶片,增压器和排气管等)的镍基单晶超级合金的单一γ-原相的铂族金属扩散粘结涂层 燃烧室组件)暴露于特别高的温度。 本发明还涉及形成铂族金属扩散的γ键合涂层的方法以及这种粘合涂层在热障涂层中的用途。

    ARTICLE FOR USE IN HIGH STRESS ENVIRONMENTS HAVING MULTIPLE GRAIN STRUCTURES
    98.
    发明申请
    ARTICLE FOR USE IN HIGH STRESS ENVIRONMENTS HAVING MULTIPLE GRAIN STRUCTURES 审中-公开
    用于具有多种颗粒结构的高应力环境中的文章

    公开(公告)号:WO2015148994A3

    公开(公告)日:2015-11-26

    申请号:PCT/US2015023125

    申请日:2015-03-27

    Applicant: GEN ELECTRIC

    Abstract: A method of forming an article can comprise heating a metal to form a molten metal having a metal temperature; heating a mold to a mold temperature greater than or equal to the metal temperature; introducing the molten metal to the mold; cooling a first portion of the molten metal while maintaining a second portion of the molten metal at the metal temperature, wherein the first portion has a first side and a second side, wherein the second side is opposite the first side and adjacent to the second portion, and wherein the cooling comprises progressively cooling the first portion from the first side to the second side such that a solidification interface progresses from the first side to the second side; and cooling the remainder of the molten metal from multiple directions after the first portion is cooled to less than or equal to a crystallization temperature.

    Abstract translation: 形成制品的方法可以包括加热金属以形成具有金属温度的熔融金属; 将模具加热到大于或等于金属温度的模具温度; 将熔融金属引入模具中; 冷却熔融金属的第一部分,同时保持熔融金属的第二部分处于金属温度,其中第一部分具有第一侧和第二侧,其中第二侧与第一侧相对并且与第二部分相邻 并且其中所述冷却包括从所述第一侧向所述第二侧逐渐冷却所述第一部分,使得凝固界面从所述第一侧向所述第二侧延伸; 在将第一部分冷却至小于或等于结晶温度之后,从多个方向冷却剩余的熔融金属。