Abstract:
An aqueous dispersion of multistage polymer particles comprising a specific oligomer prepared from polymerization of monomers comprising an alkoxylated (meth) acrylate providing aqueous coating compositions with both good flow-and-leveling property and extended open time.
Abstract:
An antimicrobial coating composition comprises (i) a binder dispersion of (co)polymer particles and (ii) from 50ppm to 2000ppm, by dry weight based on total dry weight of the coating composition, a silver; wherein the binder dispersion comprises, as polymerized units, by dry weight based on total dry weight of the binder dispersion, (a) from 40% to 99.9% ethylenically unsaturated nonionic monomers and (b) from 0.1% to 60% phosphate group-containing (meth)acrylate monomers.
Abstract:
An aqueous coating composition comprising by dry weight based on total dry weight of the coating composition, from 2% to 16% a small-particle-size polymeric dispersion of (co)polymeric particles having an average particle size of from 30 to 90nm, and from 25% to 70% of titanium dioxide particles; from 50% to 100% of the titanium dioxide particles are encapsulated by a polymer shell of (co)polymeric particles.
Abstract:
It is provided an aqueous paint composition comprising by dry weight based on total dry weight of the pigment composition, from 11% to 35% of a polymeric duller of (co) polymeric particles having an average diameter of from 1 to 20μm, and from 25%to 70%of titanium dioxide particles; wherein from 50%to 100%of the titanium dioxide particles are encapsulated by polymer shell of (co) polymeric particles.
Abstract:
A water-based coating composition containing two parts (Parts A and B), (A) binder component containing a waterborne epoxy dispersion and dispersed inorganic particles with a polymeric dispersant and (B) hardener component. The polymeric dispersant contains anti-agglomerating functional groups that are unreactive with oxirane groups of the epoxy dispersion.
Abstract:
Provided are spray-dried composite particles comprising by dry weight based on total dry weight of the spray-dried composite particles, from 60%to 90%of inorganic extenders, from 5%to 25%of inorganic pigments, and from 1%to 10%of water-insoluble polymer particles. The spray-dried composite particles have a particle size of from 1 to 100μm. A spray-drying process for preparation of the spray-dried composite particles and a paint formulation comprising the spray-dried composite particles are also provided.
Abstract:
A new paper composition comprising, a) from 15 wt.% to 70 wt.% a hiding composite comprising based on the total weight of the hiding composite, from 30 wt.% to 7 wt.% pigment particles and from 25 wt.% to 70 wt.% a thermoplastic polymer. The pigment particles are hydrophobically treated with the surface tension of the pigment particles being from 0.1 to 50 mN/m, and the surface tension difference between the pigment particles and the thermoplastic polymer being less than 40 mN/m; and b) from 30 wt.% to 85 wt.% a paper pulp. Process of making such a new paper composition.
Abstract translation:一种新的纸组合物,其包含a)15重量%至70重量%的隐藏复合物,其基于所述隐藏复合物的总重量,30重量%至7重量%的颜料颗粒和25重量% 至70重量%的热塑性聚合物。 颜料颗粒被疏水处理,颜料颗粒的表面张力为0.1-50mN / m,颜料颗粒和热塑性聚合物之间的表面张力差小于40mN / m; 和b)30重量%至85重量%的纸浆。 制作这样一种新的纸张组合的过程。
Abstract:
Toughened polyamide composition including: (a) at least one polyamide; (b) at least one toughener component; and (c) at least one siloxane-based component having a viscosity of 1 mm 2/s—100,000 mm 2/s providing toughened polyamide composition with good impact strength; process for producing the toughened polyamide composition; and articles made from the toughened polyamide composition.