Abstract:
Polypropylene composition (PC) comprising (a) first propylene homopolymer (HPP-1) having a MFR 2 (230 ℃, 2.16 kg) measured according to ISO 1133 of at least 45 g/10min, (b) optionally second propylene homopolymer (HPP-2) having a MFR 2 (230 ℃, 2.16 kg) measured according to ISO 1133 of not more than 20 g/10min, and (c) polar modified polypropylene (PMP), wherein the composition does not comprise fibers (FB).
Abstract:
The present invention relates to a polypropylene composition comprising heterophasic propylene copolymer, propylene homopolymer, elastomeric ethylene copolymer and inorganic filler, and having dimensional stability and balanced mechanical properties.
Abstract:
The present invention relates to a polypropylene composition (PC) comprising - one or more polypropylenes (P) - 0.05 to 5.0 wt. % based on the total weight of the polypropylene composition (PC) of one or more additives (A), whereby - each of the additives (A) has a melting temperature determined by DSC of 100℃ or more; and - the polypropylene composition (PC) is free from additives having a melting temperature determined by DSC below 100℃, a method for the production thereof, an article made from said composition and the use of additives having a melting temperature determined by DSC of 100℃ or more for reducing the haze of a polypropylene composition (PC) comprising one or more polypropylenes (P).
Abstract:
Disclosed is a polypropylene composition comprising: (a) a polypropylene (PP-1) having a melt flow rate MFR 2 measured according to ISO 1133 of at least 50g/10 min, (b) a propylene homopolymer (HPP-2) having a melt flow rate MFR 2 measured according to ISO 1133 of less than 38 g/10 min, (c) an elastomeric propylene ethylene copolymer (EPC), (d) an elastomeric ethylene-C 4 to C 12 a-olefin-copolymer (EEC), (e) a high density polyethylene (HDPE) having a melt flow rate MFR 2 measured according to ISO 1133 in the range of 1 to 50 g/10 min, and (f) an inorganic filler (F). An article comprising the polypropylene composition and the use of it in automotive article are also disclosed.
Abstract:
The invention relates to a polypropylene composition (PP), an article comprising said polypropylene composition (PP) as well as the use of said polypropylene composition for the preparation of a moulded article.
Abstract:
A polypropylene composition (PC) comprising: one or more polypropylenes (P) 0.05 to 5.0 wt.% based on the total weight of the polypropylene composition (PC) of one or more additives (A), whereby each of the additives (A) has a melting temperature determined by DSC of 100℃ or more; and the polypropylene composition (PC) is free from additives having a melting temperature determined by DSC below 100℃, a method for the production thereof, an article made from said composition and the use of additives having a melting temperature determined by DSC of 100℃ or more for reducing the haze of a polypropylene composition (PC) comprising one or more polypropylenes (P).
Abstract:
Fiber reinforced composite comprising polypropylene, fibers and a hindered amine light stabilizer, wherein said stabilizer is used as heat stabilizer.
Abstract:
Disclosed is a polypropylene composition (PP) having high flowability and balanced mechanical properties, an article comprising said polypropylene composition(PP) as well as the use of said polypropylene composition(PP) for the preparation of a moulded article.
Abstract:
Provided are a polypropylene composition (PP), an article comprising said polypropylene composition (PP) as well as the use of said polypropylene composition (PP) for the preparation of a moulded article and the use of said polypropylene composition (PP) for reducing tiger stripes on the surface.