Abstract:
The present invention is directed to a polypropylene composition (C) comprising: (i) 48 to 76 wt.-%, based on the weight of the polypropylene composition (C), of a random propylene copolymer (RPP) with a melt flow rate MFR2 (230 °C) measured according to ISO 1133 in the range of 0.01 to 2.0 g/lOmin; and (ii) 23 to 50 wt.-%, based on the weight of the polypropylene composition (C), of a fibre (FB); and (iii) 0.1 to 10 wt.-%, based on the weight of the polypropylene composition (C), of a modified polypropylene (PMP); wherein (a) the random propylene copolymer (RPP) comprises polypropylene (PP1), polypropylene (PP2) and polypropylene (PP3); (b) the polypropylene (PP1) has a melt flow rate MFR2 (230 °C) measured according to ISO 1133 in the range of 0.1 to 3.0 g/10min; (c) the polypropylene (PP3) has a lower melt flow rate compared to the polypropylene (PP2) and the polypropylene (PP2) has a lower melt flow rate compared to the polypropylene (PP1). The present invention also is directed to a pipe comprising the polypropylene composition (C) and the use of the polypropylene composition (C) to lower the coefficient of linear thermal extension (CLTE).
Abstract:
Polypropylene composition (PC) comprising (a) first propylene homopolymer (HPP-1) having a MFR 2 (230 ℃, 2.16 kg) measured according to ISO 1133 of at least 45 g/10min, (b) optionally second propylene homopolymer (HPP-2) having a MFR 2 (230 ℃, 2.16 kg) measured according to ISO 1133 of not more than 20 g/10min, and (c) polar modified polypropylene (PMP), wherein the composition does not comprise fibers (FB).
Abstract:
The present invention relates to a polypropylene composition comprising heterophasic propylene copolymer, propylene homopolymer, elastomeric ethylene copolymer and inorganic filler, and having dimensional stability and balanced mechanical properties.
Abstract:
Pipe comprising a polypropylene composition (PC) comprising (i) propylene homopolymer having an MFR 2 (230 ℃, 2, 16 kg) in the range of 2 to 100 g/10 min, (ii) polar modified polypropylene having an MFR 2 (190 ℃, 2, 16 kg) of at least 50 g/10 min, and (iii) fibers.
Abstract:
The present invention relates to a polypropylene composition (PC) comprising - one or more polypropylenes (P) - 0.05 to 5.0 wt. % based on the total weight of the polypropylene composition (PC) of one or more additives (A), whereby - each of the additives (A) has a melting temperature determined by DSC of 100℃ or more; and - the polypropylene composition (PC) is free from additives having a melting temperature determined by DSC below 100℃, a method for the production thereof, an article made from said composition and the use of additives having a melting temperature determined by DSC of 100℃ or more for reducing the haze of a polypropylene composition (PC) comprising one or more polypropylenes (P).
Abstract:
Disclosed is a polypropylene composition comprising: (a) a polypropylene (PP-1) having a melt flow rate MFR 2 measured according to ISO 1133 of at least 50g/10 min, (b) a propylene homopolymer (HPP-2) having a melt flow rate MFR 2 measured according to ISO 1133 of less than 38 g/10 min, (c) an elastomeric propylene ethylene copolymer (EPC), (d) an elastomeric ethylene-C 4 to C 12 a-olefin-copolymer (EEC), (e) a high density polyethylene (HDPE) having a melt flow rate MFR 2 measured according to ISO 1133 in the range of 1 to 50 g/10 min, and (f) an inorganic filler (F). An article comprising the polypropylene composition and the use of it in automotive article are also disclosed.
Abstract:
The invention relates to a polypropylene composition (PP), an article comprising said polypropylene composition (PP) as well as the use of said polypropylene composition for the preparation of a moulded article.
Abstract:
A polypropylene composition (PC) comprising: one or more polypropylenes (P) 0.05 to 5.0 wt.% based on the total weight of the polypropylene composition (PC) of one or more additives (A), whereby each of the additives (A) has a melting temperature determined by DSC of 100℃ or more; and the polypropylene composition (PC) is free from additives having a melting temperature determined by DSC below 100℃, a method for the production thereof, an article made from said composition and the use of additives having a melting temperature determined by DSC of 100℃ or more for reducing the haze of a polypropylene composition (PC) comprising one or more polypropylenes (P).
Abstract:
Polypropylene composition (C1) comprising a heterophasic propylene composition (HC) comprising a propylene homopolymer (HPP-1), a propylene homopolymer (HPP-2), an elastomeric propylene copolymer (PC-1), an elastomeric propylene copolymer (PC-2), an elastomeric ethylene copolymer (EC), and a filler (F).
Abstract:
Disclosed is a polypropylene composition (PP) having high flowability and balanced mechanical properties, an article comprising said polypropylene composition(PP) as well as the use of said polypropylene composition(PP) for the preparation of a moulded article.