Abstract:
A cast film inclucing a bimodal ethylene-based polymer having a high density fraction (HDF) from 3.0% to 10.0%, an I 10 /I 2 ratio from 5.5 to 7.0, a short chain branching distribution (SCBD) less than or equal to 10 °C, a density from 0.910 g/cc to 0.920 g/cc, and a melt index (I 2 ) from 1.0 g/10 mins to 8.0 g/10 mins.
Abstract:
Embodiments disclosed herein include multilayer cast films having a cling layer and a release layer, wherein the cling layer comprises (i) a first polyethylene composition, and (ii) ultra-low density polyethylene, very low density polyethylene, ethylene/alpha-olefin elastomer, propylene-based elastomer, or combinations thereof; and the release layer comprises a second polyethylene composition.
Abstract:
Embodiments of thermoplastic bags which yield elasticity and stiffness include a first drawtape disposed within the first channel, wherein the first drawtape comprises a linear low density polyethylene having a density of from 0.902 g/cc to 0.920 g/cc, and a second drawtape disposed within the second channel, wherein the second drawtape comprises a high density polyethylene having a density of from 0.940 g/cc to 0.965 g/cc.
Abstract:
The present disclosure relates to a multilayer stretch film comprising at least a first layer, wherein said first layer comprises a polyolefin resin. The film of this aspect of the disclosure further include at least a second layer, and a mechanochromic dye which may be in any or all layers of the film. Another aspect of the disclosure is a method of promoting optimal stretching of stretch film during a wrapping operation, which method comprises at least the following steps. A polyolefin resin is selected that has a given density. Selecting a mechanochromic dye based on its ability to agglomerate in an unstretched film made from the polyolefin resin having the given density, such that when the dye is included in the film, the unstretched film will exhibit a first color. Admixing the mechanochromic dye into a melt of the polyolefin resin. Forming a film from the admixture of the previous step. Wrapping an object using the film of the previous step, while stretching the film to a level where a change from the first color to a second color can be observed.
Abstract:
Embodiments of the present disclosure are specifically related to LLDPE compositions produced from heterogeneous procatalyst compositions and blown and cast films incorporating these LLDPE compositions.
Abstract:
The present disclosure relates to a method of promoting optimal stretching of stretch film during a wrapping operation, which method comprises at least the following steps. First a resin suitable for making stretch films is selected. Then a dispersed agent is selected, preferably one which has a refractive index similar to the selected resin such that when a film is made comprising the resin and the dispersed agent, the film will appear somewhat clear. The dispersed agent is then mixed with the resin and a film is formed from the resin containing the dispersed agent. Finally, a load is manually wrapped using such film, wherein during wrapping, the film is stretched to a level where the film becomes more opaque.
Abstract:
Provided are polyethylene compositions and cast stretch films comprising polyethylene compositions. The cast stretch films can exhibit improved tear strength and on pallet benefits while maintaining other properties. The cast stretch films can also be fully compatible with polyethylene recycling streams and can be free of polypropylene.
Abstract:
Embodiments of the present disclosure are directed to drawtapes for trash bags, wherein the drawtape comprises a multilayer polymer film having an improved stiffness.
Abstract:
The instant invention provides polyethylene compositions having reduced plate out, and films made therefrom having reduced blooming. The polyethylene composition suitable for film applications according to the present invention comprises the melt blending product of: (a) an ethylene based polymer; (b) a first antioxidant system comprising one or more antioxidants selected from the group consisting of Octadecyl-3-(3,5-di-tert.butyl-4-hydroxyphenyl)-propionate; Pentaerythritol Tetrakis(3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate); and combinations thereof; (c) a second antioxidant system comprising a liquid phosphite corresponding to the formula [4-(2-methylbutan-2-yl)phenyl]x[2,4-bis(2-methylbutan-2-yl)phenyl]3-x phosphate, wherein x = 0, 1, 2, 3, or combinations thereof; and (d) optionally one or more neutralizing agents.